Effect of growth ring orientations and location on moisture-induced swelling behavior of Chinese fir wood
Source abstract
Abstract
In this study, the moisture adsorption and swelling behavior of Chinese fir (Cunninghamia lanceolata) wood in different growth ring orientations and locations were investigated. Heartwood specimens were divided into α = 90°(H90°), 45°≤α<90°(H45–90°), and 0°≤α<45°(H0–45°), along with specimens obtained from transition wood (T0–45°) and sapwood (S0–45°) in the same angle of 0°≤α<45°. Approximately 70% changes in moisture adsorption content and swelling in the thickness and width were observed during the initial 4-day period, and then moisture content (MC) and swelling reached equilibrium on the 16th day, irrespective of growth ring orientations and location. In comparison with length swelling, swelling in the width and thickness directions were closely related to α angle. For heartwood specimens, the width swelling was negatively correlated with α angle, while the thickness swelling was positively correlated with α angle. For specimens with the same angle, MC and swelling followed the order of S0–45°>T0–45°>H0–45°, which was attributed to the higher holocellulose and lower extractives content. Furthermore, swelling in the width and thickness directions increased first and then decreased with increasing α angle. These findings will be helpful to understand the hygro-deformation of wood in different growth ring orientations and locations, and provide a scientific basis for the utilization of solid wood.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Bamboo properties and applications · Tree Root and Stability Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Research Institute of Wood Industry
Nanjing Forestry University
Chinese Academy of Forestry
Funding
National Natural Science Foundation of China · Fundamental Research Funds of the Chinese Academy of Forestry
References (44)
Show source-provided references
1. 10.1080/07373937.2014.92413210.1080/07373937.2014.924132 ↗
2. Azadeh, A. and Ghavami, K., 2018. The influence of heat on shrinkage and water absorption of dendrocalamus giganteus bamboo as a functionally graded material. Construction and Building Materials, 186, 145–154.10.1016/j.conbuildmat.2018.07.011 ↗
3. 10.1371/journal.pone.015077710.1371/journal.pone.0150777 ↗
4. Broushakian, V. and Mohebby, B., 2025. Moisture distribution in cross laminated timber (CLT) made from heat-treated wood. European Journal of Wood and Wood Products, 83 (2), 53.10.1007/s00107-025-02212-4 ↗
5. Cha, H., 2016, The study on visual characteristics of radial texture of wood based on modern solid wood chair. Nanjing: Nanjing Forestry University.
6. 10.3390/f912076310.3390/f9120763 ↗
7. Duong, D.V. and Matsumura, J., 2018. Transverse shrinkage variations within tree stems of Melia azedarach planted in northern Vietnam. Journal of Wood Science, 64, 720–729.10.1007/s10086-018-1756-2 ↗
8. 10.1007/s00226-012-0514-710.1007/s00226-012-0514-7 ↗
9. Follrich, J., 2010. Relationship between radial and longitudinal swelling in dependence of grain orientation. Wood Research, 55 (2), 1–6.
10. Garcia, R., Rosero-Alvarado, J., and Hernández, R., 2020. Full-field moistureinduced strains of the different tissues of tamarack and red oak woods assessed by 3D digital image correlation. Wood Science and Technology, 54 (1), 139–159.10.1007/s00226-019-01145-5 ↗
11. Gereke, T., et al., 2009. Experimental and numerical determination of the hygroscopic warping of cross-laminated solid wood panels. Holzforschung, 63 (3), 340–347.10.1515/HF.2009.061 ↗
12. Gereke, T., Hass, P., and Niemz, P., 2010. Moisture-induced stresses and distortions in spruce cross-laminates and composite laminates. Holzforschung, 64 (1), 127–133.10.1515/hf.2010.003 ↗
13. 10.1007/s10570-020-03552-510.1007/s10570-020-03552-5 ↗
14. 10.1002/app.2972510.1002/app.29725 ↗
15. Hill, C.A.S., Norton, A., and Newman, G., 2010. Analysis of the water vapour sorption behaviour of sitka spruce [picea sitchensis (bongard) carr.] based on the parallel exponential kinetics model. Holzforschung, 64 (4), 469–473.
16. Hong, L., et al., 2016. Methods for improving the dimensional stability of solid wood panel assemblies. China Forest Products Industry, 43 (2), 34–35. + 39.
17. Jiang, Z. and Jiang, X., 2008. The correlation between wood structure and its quality characteristics. Beijing: Science Press. 119–123.
18. 10.1051/forest/200904510.1051/forest/2009045 ↗
19. 10.1515/HF.2005.10410.1515/HF.2005.104 ↗
20. 10.1163/15685540376582690010.1163/156855403765826900 ↗
21. Lao, W., et al., 2022. Development path of China wood industry under the targets of carbon dioxide emission peaking and carbon neutrality. Chinese Journal of Wood Science and Technology, 36 (1), 87–91.
22. Li, J., et al., 2025. Frontier advances in wood science towards a new departure. Forest Engineering, 41 (1), 1–39.
23. 10.1007/s10086-010-1142-110.1007/s10086-010-1142-1 ↗
24. 10.1080/17480272.2023.222167810.1080/17480272.2023.2221678 ↗
25. Mou, Q., et al., 2022. Hygroexpansion behaviors of bamboo in response to moisture absorption and desorption. Construction and Building Materials, 341, 127895.10.1016/j.conbuildmat.2022.127895 ↗
26. 10.1515/hf-2021-022210.1515/hf-2021-0222 ↗
27. 10.3390/jimaging712026310.3390/jimaging7120263 ↗
28. 10.1111/j.1365-2621.1988.tb13565.x10.1111/j.1365-2621.1988.tb13565.x ↗
29. 10.1007/s00226-019-01104-010.1007/s00226-019-01104-0 ↗
30. 10.1515/hf-2018-006710.1515/hf-2018-0067 ↗
31. Peng, H., et al., 2023. Bending responses of self-shaping wood bilayers: comparison between adsorption and desorption processes. Journal of Wood Science, 69 (1), 29.10.1186/s10086-023-02105-1 ↗
32. Podibka, T., 2020. A investigation of form of stability of variously designed furniture board made of pine wood of different constructions. Forestry, Forest, Paper and Woodworking Industry, 46, 108–120.10.36930/42204613 ↗
33. Podibka, T., 2022. Determination of the regulations of the influence of the characteristics of the rails on the form resistance of furniture panels made of beech wood of different constructions. Forestry, Forest, Paper and Woodworking Industry, 48, 40–56.10.36930/42214804 ↗
34. 10.3390/f1305072210.3390/f13050722 ↗
35. Song, K., 2012, Changes of structure and performance of cell walls during the transformation from sapwood to heartwood of Cunninghamia lanceolata. Beijing: Chinese Academy of Forestry.
36. Song, K., et al., 2014. Changes in the properties of wood cell walls during the transformation from sapwood to heartwood. Journal of Materials Science, 49 (4), 1734–1742.10.1007/s10853-013-7860-1 ↗
37. Song, R., et al., 2025. Hygromechanical deformation of wood cell walls regulated by the microfibril angle. Journal of Materials Chemistry A, 13, 1973.10.1039/D4TA07560A ↗
38. Stevens, W. and Johnston, D., 1960. Distortion caused by spiral grain. Timber Technol, 68, 217–218.
39. 10.1515/hf-2022-001310.1515/hf-2022-0013 ↗
40. Wang, E., et al., 2008. Variation in anisotropic shrinkage of plantation-grown pinus radiata wood. Maderas. Ciencia y tecnología, 10 (3), 243–249.10.4067/S0718-221X2008000300007 ↗
41. Yin, F., et al., 2024. Shrinkage and swelling behavior of different types of tissues in catalpa bungei wood. Scientia Silvae Sinicae, 60 (7), 1–14.
42. Yu, T., et al., 2025. Growth-ring effect on moisture-induced stress and damage development in glued laminated timber. Wood Science and Technology, 59 (4), 58.10.1007/s00226-025-01647-5 ↗
43. 10.1016/j.conbuildmat.2023.13047910.1016/j.conbuildmat.2023.130479 ↗
44. 10.1007/s00226-021-01321-610.1007/s00226-021-01321-6 ↗