journal article·2016-05

Combined treatment for conversion of fast-growing poplar wood to magnetic wood with high dimensional stability

Youming Dong, Yutao Yan, Yang Zhang, Shifeng Zhang, Jianzhang Li

Wood Science and Technology· Volume 50· Issue 3
Publisher page

Abstract

Magnetic wood with high performance was prepared from fast-growing poplar wood via a novel two-step combined treatment. The poplar wood was first magnetized via coprecipitation of ferric and ferrous ions and then polymerized in situ by impregnation with a furfuryl alcohol solution. The resulting products were characterized by Fourier transform infrared spectroscopy, X-ray diffractometry, and vibrating sample magnetometry. The properties and morphology were also evaluated. The results showed that: (1) Fe₃O₄ nanoparticles were successfully synthesized in poplar wood, and the average size was 16 nm; (2) the magnetic properties of the composites were remarkable, and the magnetic stability and acid resistance of the modified wood were improved by the furfurylation; (3) after furfurylation, the magnetic wood recovered from the severe collapse induced by the magnetic treatment and exhibited high dimensional stability and water resistance.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Cellulose Research Studies · Wood Treatment and Properties · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Ayrilmis N, Kaymakci A (2013) Fast growing biomass as reinforcing filler in thermoplastic composites: Paulownia elongata wood. Ind Crop Prod 43:457–46410.1016/j.indcrop.2012.07.050 ↗
2. Bhuiyan MTR, Hirai N, Sobue N (2000) Changes of crystallinity in wood cellulose by heat treatment under dried and moist conditions. J Wood Sci 46:431–43610.1007/BF00765800 ↗
3. Buchelt B, Dietrich T, Wagenführ A (2012) Macroscopic and microscopic monitoring of swelling of beech wood after impregnation with furfuryl alcohol. Eur J Wood Prod 70:865–86910.1007/s00107-012-0631-x ↗
4. Cave I (1997) Theory of X-ray measurement of microfibril angle in wood. Wood Sci Technol 31:225–23410.1007/BF00702610 ↗
5. Chang HT, Chang ST (2006) Modification of wood with isopropyl glycidyl ether and its effects on decay resistance and light stability. Bioresour Technol 97:1265–127110.1016/j.biortech.2005.06.001 ↗
6. Chen H, Lang Q, Bi Z, Miao X, Li Y, Pu J (2014) Impregnation of poplar wood (Populus euramericana) with methylolurea and sodium silicate sol and induction of in situ gel polymerization by heating. Holzforschung 68:45–5210.1515/hf-2013-0028 ↗
7. Cornell RM, Schwertmann U (2006) The iron oxides: structure, properties, reactions, occurrences and uses. Wiley, NewYork
8. Deka H, Misra M, Mohanty A (2013) Renewable resource based “all green composites” from kenaf biofiber and poly(furfuryl alcohol) bioresin. Ind Crop Prod 41:94–10110.1016/j.indcrop.2012.03.037 ↗
9. Dong Y, Yan Y, Zhang S, Li J (2014) Wood/polymer nanocomposites prepared by impregnation with furfuryl alcohol and nano-SiO2. BioResources 9:6028–6040
10. Gao H, Zhang G, Wu G, Guan H (2011) In-situ preparation and magnetic properties of Fe3O4/wood composite. In: Advanced materials and processing 2010—proceedings of the 6th international conference on Icamp. World Scientific, Singapore, pp 147–15210.1142/9789814322799_0035 ↗
11. Hazarika A, Maji TK (2014) Strain sensing behavior and dynamic mechanical properties of carbon nanotubes/nanoclay reinforced wood polymer nanocomposite. Chem Eng J 247:33–4110.1016/j.cej.2014.02.069 ↗
12. Herold N, Pfriem A (2013) Impregnation of veneer with furfuryl alcohol for an improved plasticization and moulding. Eur J Wood Prod 71:281–28210.1007/s00107-013-0677-4 ↗
13. Herold N, Pfriem A (2014) Shape retention of furfurylated and moulded wood veneer. BioResources 9:545–55310.15376/biores.9.3.4756-4763 ↗
14. Herold N, Dietrich T, Grigsby WJ, Franich RA, Winkler A, Buchelt B, Pfriem A (2013) Effect of maleic anhydride content and ethanol dilution on the polymerization of furfuryl alcohol in wood veneer studied by differential scanning calorimetry. BioResources 8:1064–107510.15376/biores.8.1.1064-1075 ↗
15. Iida H, Takayanagi K, Nakanishi T, Osaka T (2007) Synthesis of Fe3O4 nanoparticles with various sizes and magnetic properties by controlled hydrolysis. J Colloid Inter Sci 314:274–28010.1016/j.jcis.2007.05.047 ↗
16. Kielmann BC, Adamopoulos S, Militz H, Koch G, Mai C (2013) Modification of three hardwoods with an N-methylol melamine compound and a metal-complex dye. Wood Sci Technol 48:123–13610.1007/s00226-013-0595-y ↗
17. La Mantia FP, Morreale M (2011) Green composites: a brief review. Compos Part A 42:579–58810.1016/j.compositesa.2011.01.017 ↗
18. Lande S, Westin M, Schneider M (2004a) Properties of furfurylated wood. Scand J For Res 19:22–3010.1080/0282758041001915 ↗
19. Lande S, Westin M, Schneider M (2004b) Eco-efficient wood protection: furfurylated wood as alternative to traditional wood preservation. Manag Environ Qual 15:529–54010.1108/14777830410553979 ↗
20. Lande S, Westin M, Schneider M (2008) Development of modified wood products based on furan chemistry. Mol Cryst Liq Cryst 484:367–37810.1080/15421400801901456 ↗
21. Li P, Zhu AM, Liu QL, Zhang QG (2008) Fe3O4/poly(N-isopropylacrylamide)/chitosan composite microspheres with multiresponsive properties. Ind Eng Chem Res 47:7700–770610.1021/ie800824q ↗
22. Li JZ, Furuno T, Zhou WR, Ren Q, Han XZ, Zhao JP (2009) Properties of acetylated wood prepared at low temperature in the presence of catalysts. J Wood Chem Technol 29:241–25010.1080/02773810903009499 ↗
23. Lin C, Ho J (2014) Structural analysis and catalytic activity of Fe3O4 nanoparticles prepared by a facile co-precipitation method in a rotating packed bed. Ceram Int 40:10275–1028210.1016/j.ceramint.2014.02.119 ↗
24. Merk V, Chanana M, Gierlinger N, Hirt AM, Burgert I (2014) Hybrid wood materials with magnetic anisotropy dictated by the hierarchical cell structure. ACS Appl Mater Interface 6:9760–976710.1021/am5021793 ↗
25. Mohammadi A, Daemi H, Barikani M (2014) Fast removal of malachite green dye using novel superparamagnetic sodium alginate-coated Fe3O4 nanoparticles. Int J Biol Macromol 69:447–45510.1016/j.ijbiomac.2014.05.042 ↗
26. Mohebby B, Kevily H, Kazemi-Najafi S (2014) Oleothermal modification of fir wood with a combination of soybean oil and maleic anhydride and its effects on physico-mechanical properties of treated wood. Wood Sci Technol 48:797–80910.1007/s00226-014-0640-5 ↗
27. Oishi SS, Rezende MC, Origo FD, Damiao AJ, Botelho EC (2013) Viscosity, pH, and moisture effect in the porosity of poly (furfuryl alcohol). J Appl Polym Sci 128:1680–168610.1002/app.38332 ↗
28. Oka H, Fujita H, Seki K (2000) Composition and heating efficiency of magnetic wood by induction heating. IEEE Trans Magn 36:3715–371710.1109/20.908950 ↗
29. Oka H, Hojo A, Seki K, Takashiba T (2002) Wood construction and magnetic characteristics of impregnated type magnetic wood. J Magn Magn Mater 239:617–61910.1016/S0304-8853(01)00684-9 ↗
30. Oka H, Hojo A, Osada H, Namizaki Y, Taniuchi H (2004) Manufacturing methods and magnetic characteristics of magnetic wood. J Magn Magn Mater 272–276:2332–233410.1016/j.jmmm.2003.12.1214 ↗
31. Oka H, Terui M, Osada H, Sekino N, Namizaki Y, Dawson F (2012) Electromagnetic wave absorption characteristics adjustment method of recycled powder-type magnetic wood for use as a building material. IEEE Trans Magn 48:3498–350010.1109/TMAG.2012.2196026 ↗
32. Pranger L, Tannenbaum R (2008) Biobased nanocomposites prepared by in situ polymerization of furfuryl alcohol with cellulose whiskers or montmorillonite clay. Macromolecules 41:8682–868710.1021/ma8020213 ↗
33. Rahman MR, Hamdan S, Ahmed AS, Islam MS, Talib ZA, Abdullah WFW, Mat MSC (2011) Thermogravimetric analysis and dynamic Young’s modulus measurement of N,N-dimethylacetamide-impregnated wood polymer composites. J Vinyl Addit Technol 17:177–18310.1002/vnl.20275 ↗
34. Rowell RM (2012) Handbook of wood chemistry and wood composites. CRC Press, Boca Raton10.1201/b12487 ↗
35. Trey SM, Olsson RT, Strom V, Berglund LA, Johansson M (2014) Controlled deposition of magnetic particles within the 3-D template of wood: making use of the natural hierarchical structure of wood. RSC Adv 4:35678–3568510.1039/C4RA04715J ↗
36. Wu S, Sun A, Zhai F, Wang J, Xu W, Zhang Q, Volinsky AA (2011) Fe3O4 magnetic nanoparticles synthesis from tailings by ultrasonic chemical co-precipitation. Mater Lett 65:1882–188410.1016/j.matlet.2011.03.065 ↗
37. Xu Z, Wang C, Yang W, Fu S (2005) Synthesis of superparamagnetic Fe3O4/SiO2 composite particles via sol-gel process based on inverse miniemulsion. J Mater Sci 40:4667–466910.1007/s10853-005-3924-1 ↗
38. Yan Y, Dong Y, Li C, Chen H, Zhang S, Li J (2014) Optimization of reaction parameters and characterization of glyoxal-treated poplar sapwood. Wood Sci Technol 49:241–25610.1007/s00226-014-0674-8 ↗
39. Yang H, Yan R, Chen H, Lee DH, Zheng C (2007) Characteristics of hemicellulose, cellulose and lignin pyrolysis. Fuel 86:1781–178810.1016/j.fuel.2006.12.013 ↗