Erosive Wear Behavior of High-Alloy Cast Iron and Duplex Stainless Steel under Mining Conditions
Source abstract
Abstract
Centrifugal pumps used in the lignite mines encounter erosive wear problems, leading to a disastrous failure of the pump casings. This paper attempts to evaluate the erosive wear resistance of Ni-Hard 4, high-chromium iron, and Cast CD4MCu duplex stainless steel (DSS), for mining conditions. The prepared test coupons were subjected to an erosion test by varying the impingement velocity and the angle of impingement, under two different pH conditions of 3 and 7, which pertained to the mining conditions. XRD analysis was carried out to confirm the phases present in the alloy. The eroded surface was subjected to SEM analysis to identify the erosion mechanisms. The surface degradation of Ni-Hard 4 and high-chromium iron came from a low-angle abrasion with a grooving and plowing mechanism at a low angle of impingement. At normal impingement, deep indentations resulted in lips and crater formations, leading to degradation of the surface in a brittle manner. A combined extrusion-forging mechanism is observed in the CD4MCu DSS surface at all the impingement angles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Metal Alloys Wear and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. J.R. Davis, Alloying Understanding the Basics, ASM International, Materials Park, OH, 2001, p 13.10.31399/asm.tb.aub.9781627082976 ↗
2. K. Rohrig, Ni-Hard Material Data and Applications, Nickel Development Institute, Technology & Engineering, Canada, 1996, p 1–28.
3. T.A. Adler and O.N. Dogan, Erosive Wear and Impact Damage of High-Chromium White Cast Irons, Wear, 1999, 225–229, p 174–18010.1016/S0043-1648(99)00010-1 ↗
4. K.P. Sampathkumaran and S. Seetharamu, Erosion and Abrasion Characteristics of High Manganese Chromium Irons, Wear, 2005, 259, p 70–7710.1016/j.wear.2005.03.001 ↗
5. S.H.M. Anijdan, A. Bahrami, N. Varahram, and P. Davami, Effects of Tungsten on Erosion-Corrosion Behavior of High Chromium White Cast Iron, Material Science and Engineering A, 2007, 454–455, p 623–62810.1016/j.msea.2006.11.128 ↗
6. M.A. Al-Bukhaiti, S.M. Ahmed, F.M.F. Badran, and K.M. Emara, Effect of Impingement Angle on Slurry Erosion Behaviour and Mechanisms of 1017 Steel and High-Chromium White Cast Iron, Wear, 2007, 262, p 1187–119810.1016/j.wear.2006.11.018 ↗
7. H.H. Tian, G.R. Addie, and R.J. Visintainer, Erosion-Corrosion Performance of High-Cr Cast Iron Alloys in Flowing Liquid-Solid Slurries, Wear, 2009, 267, p 2039–204710.1016/j.wear.2009.08.007 ↗
8. R.J. Llewellyn, S.K. Yick, and K.F. Dolman, Scouring Erosion Resistance of Metallic Materials used in Slurry Pump Service, Wear, 2004, 256, p 592–59910.1016/j.wear.2003.10.002 ↗
9. X.H. Tang, R. Chung, D.Y. Li, B. Hinckley, and K. Dolman, Variations in Microstructure of High Chromium Cast Irons and Resultant Changes in Resistance to Wear, Corrosion and Corrosive Wear, Wear, 2009, 267, p 116–12110.1016/j.wear.2008.11.025 ↗
10. R.J. Chung, X. Tang, D.Y. Li, B. Hinckley, and K. Dolman, Abnormal Erosion-Slurry Velocity Relationship of High Chromium Cast Iron with High Carbon Concentrations, Wear, 2011, 271, p 1454–146110.1016/j.wear.2011.01.087 ↗
11. X.H. Tang, R. Chung, C.J. Pang, D.Y. Li, B. Hinckley, and K. Dolman, Microstructure of High (45 wt%) Chromium Cast Irons and Their Resistances to Wear and Corrosion, Wear, 2011, 271, p 1426–143110.1016/j.wear.2010.11.047 ↗
12. H.K.D.H. Bhadeshia and R.W.K. Honeycombe, Steels Microstructure and Properties, 3rd ed., Elsevier, Amsterdam, 2006
13. C.T. Kwok, H.C. Man, and L.K. Leung, Effect of Temperature, pH and Sulphide on the Cavitation Erosion Behaviour of Super Duplex Stainless Steel, Wear, 1997, 211, p 84–9310.1016/S0043-1648(97)00072-0 ↗
14. E.A.M. Hussain and M.J. Robinson, Erosion-Corrosion of 2205 Duplex Stainless Steel in Flowing Seawater Containing sand Particles, Corrosion Science, 2007, 49, p 1737–175410.1016/j.corsci.2006.08.023 ↗
15. A. Neville and T. Hodgkiess, Characterization of High-Grade Alloy Behaviour in Severe Erosion-Corrosion Conditions, Wear, 1999, 233–235, p 596–60710.1016/S0043-1648(99)00220-3 ↗
16. A. Neville and X. Hu, Mechanical and Electrochemical Interactions During Liquid-Solid Impingement on High-Alloy Stainless Steels, Wear, 2001, 251, p 1284–129410.1016/S0043-1648(01)00757-8 ↗
17. X. Hu and A. Neville, The Electrochemical Response of Stainless Steels in Liquid-Solid Impingement, Wear, 2005, 258, p 641–64810.1016/j.wear.2004.09.043 ↗
18. X. Hu and N. Anne, An Examination of the Electrochemical Characteristics of Two Stainless Steels (UNS S32654 and UNS S31603) Under Liquid-Solid Impingement, Wear, 2004, 256, p 537–54410.1016/S0043-1648(03)00563-5 ↗
19. M.M. Stack, J. Chacon-Nava, and F.H. Stott, Relationship Between the Effects of Velocity and Alloy Corrosion Resistance in Erosion-Corrosion Environments at Elevated Temperatures, Wear, 1995, 180, p 91–9410.1016/0043-1648(94)06536-5 ↗
20. R.C. Shivamurthy, M. Kamaraj, R. Nagarajan, S.M. Shariff, and G. Padmanabham, Influence of Microstructure on Slurry Erosive Wear Characteristics of Laser Surface Alloyed 13Cr-4Ni Steel, Wear, 2009, 267, p 204–21210.1016/j.wear.2008.12.027 ↗
21. O.N. Dogan and J.A. Hawk, Effect of Carbide Orientation on Abrasion of High Cr White Cast Iron, Wear, 1995, 189, p 136–14210.1016/0043-1648(95)06682-9 ↗
22. M. Divakar, V.K. Agarwal, and S.N. Singh, Effect of the Material Surface Hardness on the Erosion of AISI, 316, Wear, 2005, 259, p 110–11710.1016/j.wear.2005.02.004 ↗
23. A.K. Chauhan, D.B. Goel, and S. Prakash, Erosion Behaviour of Hydro Turbine Steels, Bulletin of Materials Science, 2008, 31(2), p 115–12010.1007/s12034-008-0020-6 ↗
24. H.S. Grewal, S. Bhandari, and H. Singh, Parametric Study of Slurry-Erosion of Hydroturbine Steels with and without Detonation Gun Spray Coatings using Taguchi Technique, Metallurgical and Materials Transactions A, 2012, 43A, p 3387–340110.1007/s11661-012-1148-y ↗
25. I. Kleis and P. Kulu, Solid Particle Erosion Occurrence, Prediction and Control, Springer, Berlin, 2008
26. T. Manisekaran, M. Kamaraj, S.M. Sharrif, and S.V. Joshi, Slurry Erosion Studies on Surface Modified 13Cr-Ni Steels: Effect of Angle of Impingement and Particle Size, Journal of materials engineering and performance, 2007, 16, p 567–57210.1007/s11665-007-9068-5 ↗
27. M.A. Al-Bukahiti, S.M. Ahmed, F.M.F. Badran, and K.M. Emara, Effect of Impingement Angle on Slurry Erosion Behaviour and Mechanisms of 1017 Steel and High-Chromium White Cast Iron, Wear, 2007, 262, p 1187–119810.1016/j.wear.2006.11.018 ↗
28. H.M. Clark, The Influence of the Flow Field in Slurry Erosion, Wear, 1992, 152, p 223–24010.1016/0043-1648(92)90122-O ↗
29. J. Yoganandh, S. Natarajan, and S.P. Kumaresh Babu, Erosive Wear Behavior of Nickel Based High Alloy White Cast Iron Under Mining Conditions Using Orthogonal Array, Journal of Materials Engineering Performance, 2013, 22(9), p 2534–254110.1007/s11665-013-0539-6 ↗
30. B.K. Prasad, A.K. Jha, O.P. Modi, and A.H. Yegneswaran, Effect of Sand Concentration in the Medium and Travel Distance and Speed on the Slurry Wear Response of a Zinc-Based Alloy Alumina Particle Composite, Tribology Letters, 2004, 17, p 301–30910.1023/B:TRIL.0000032468.27468.2c ↗
31. A.N.J. Stevenson and I.M. Hutchings, Wear of Hardfacing White Cast Irons by Solid Particle Erosion, Wear, 1995, 186–187, p 150–15810.1016/0043-1648(95)07184-9 ↗
32. A.J. Ninham and A.V. Levy, The Erosion of Carbide-Metal Composites, Wear, 1988, 121, p 347–36110.1016/0043-1648(88)90210-4 ↗
33. I. Hussainova, J. Pirso, M. Antonov, K. Juhani, and S. Letunovits, Erosion and Abrasion of Chromium Carbide Based Cermets Produced by Different Methods, Wear, 2007, 263, p 905–91110.1016/j.wear.2006.12.027 ↗
34. I.R. Sare and B.K. Arnold, Gouging Abrasion of Wear-Resistant Alloy White Cast Irons, Wear, 1989, 131, p 15–3910.1016/0043-1648(89)90243-3 ↗
35. J.J. Coronado and A. Sinatora, Abrasive Wear Study of White Cast Iron with Different Solidification Rates, Wear, 2009, 267, p 2116–212110.1016/j.wear.2009.08.010 ↗
36. E. Albertin and A. Sinatora, Effect of Carbide Fraction and Matrix Microstructure on the Wear Cast Iron Balls Tested in a Laboratory Ball Mill, Wear, 2001, 250, p 492–50110.1016/S0043-1648(01)00664-0 ↗
37. J.C. Rawersa, J.H. Tylczaka, and D.E. Almana, Wear Evaluation of High Interstitial Stainless Steels, Tribology Transactions, 2008, 51(4), p 515–52510.1080/10402000802071285 ↗
38. M.T. Benchaita, Some Observations on Erosive-Abrasive Wear of Metallic Surfaces in Particular Geometries, Tribology Transaction, 1988, 31(1), p 133–14010.1080/10402008808981809 ↗
39. G. Sundararajan, The Solid Particle Erosion of Metallic Materials: The Rationalization of the Influence of Material Variables, Wear, 1995, 186–187, p 129–14410.1016/0043-1648(95)07172-5 ↗
40. S.S. Rajahram, T.J. Harvey, and R.J.K. Wood, Full Factorial Investigation on the Erosion-Corrosion Resistance of UNS S31603, Tribology International, 2010, 43, p 2072–208310.1016/j.triboint.2010.05.012 ↗
41. H. Imrek, M. Bagci, and O.M. Khalfan, Solid Particle Erosion as Influenced by Tensile Axial Loads, Tribology Transaction, 2011, 54(5), p 779–78310.1080/10402004.2011.603459 ↗
42. I. Finnie, Some Observations on the Erosion of Ductile Metals, Wear, 1972, 19, p 81–9010.1016/0043-1648(72)90444-9 ↗