journal article·2009-10

High Power Diode Laser Surface Treatment to Minimize Droplet Erosion of Low Pressure Steam Turbine Moving Blades

B.S. Mann, Vivek Arya, B.K. Pant, Manish Agarwal

Publisher page

Abstract

This article deals with the high power diode laser (HPDL) surface treatment to overcome water droplet erosion of Low Pressure Steam Turbine (LPST) moving blades used in high rating conventional, critical and super critical thermal power plants. The materials generally used in these steam turbines are titanium alloy (Ti6Al4V), precipitate hardened stainless steel (17Cr-4Ni PH), X20Cr13 and X10CrNiMoV1222 steels. During incubation period as well as under prolonged testing, the HPDL surface treatment of these materials except for 17Cr-4Ni PH steel has enhanced the droplet erosion resistance significantly. This is due to increased hardness and formation of fine-grained martensitic phase due to rapid heating and cooling rates associated with laser treatment. The droplet erosion results of HPDL laser surface treatment of all these materials and their analysis form the main part of the article.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Erosion and Abrasive Machining · Coal Combustion and Slurry Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. J.R. Cheski, R. Patel, K. Rockaway, H. Osaghae, and M. Christianson, A Large Steam Turbine Retrofit Design and Operation History, Presented at 2005 Power-Gen International Conference held at Las Vegas, N.V. Dec 6–8, 2005, p 14
2. J.K. Reinker and P·B. Mason, Steam Turbines for Large Power Applications, GE Power System, GER-3646D, 1996
3. J. Krzyzanowski, The correlation Between Droplet Steam Structure and Steam Turbine Blading Erosion, Journal of engineering for power, Vol. 96, July 1974, 256–26610.1115/1.3445804 ↗
4. J. Krzyzanowski and Z. Szperngiel, The Influence of Droplet Size on the Turbine Blading Erosion Hazard, Journal of Engineering for power, Vol. 100, October 1978, 561–56510.1115/1.3446394 ↗
5. C. T. Kwok, H. C. Man, F. T. Cheng, Cavitation Erosion and Pitting Corrosion Behaviour of Laser Surface Melted Martensitic Stainless Steel UNSS 42000, Surface and coating Technology, 126, (2000), 238–25510.1016/S0257-8972(00)00533-8 ↗
6. J. Grum and R. Sturm, Residual Stresses State After the Laser Surface Remelting Process, J of Material Engineering and Performance, Vol. 10 (3) June 2001, 270–281.10.1361/105994901770344980 ↗
7. J. Kiesbauer, Control Valve for Critical Applications, Hydrocarbon Process., 2001, 80(6), p 89–100
8. S·V. Sherikar, Designing HRSG Desuperheaters for Performance Reliability, Power, 2006, 150(2), p 1–7
9. B·S. Mann and V. Arya, An Experimental Study to Correlate Water Jet Impingement Erosion Resistance and Properties of Metallic Materials and Coatings, Wear 253 (2002), 650–65110.1016/S0043-1648(02)00118-7 ↗
10. B·S. Mann and V. Arya, HVOF Coating and Surface Treatment for Enhancing Droplet Erosion Resistance for Steam Turbine Blades, Wear 254 (2003), 652–66710.1016/S0043-1648(03)00253-9 ↗
11. B. S. Mann, Vivek Arya and Pankaj Joshi, Advanced HVOF Coating and Candidate Materials for Protecting LP Steam Turbine Blades Against Droplet Erosion Journal of Materials Engineering and Performance,V 14. No 4. Aug. (2005), 487–49410.1361/105994905X56188 ↗
12. W. Storch, G. Blum, B. Brenner, and G. Wiedemann, Laserhartung von Turbinenschaufelkanten, DK 621.165/620, Mitteilungen aus dem kraftwerk sanlagen, 1988, p 16–17
13. M.B.Lesser and J.E.Field., The Impact of Compressible Liquids. Annu. Rev.Fluid mech. 15 (1983) 97–12210.1146/annurev.fl.15.010183.000525 ↗
14. W·F.Adler, The Mechanisms of Liquid Impact, in C.M. Preece (ed). Erosion, Academic Press. New York, 1979, pp 127–84
15. B. Stanisa, Z.Schauperl and K.Grilec, Erosion Behaviour of Turbine Rotor Blades Installed in the Krsko Nuclear Power Plant, Wear 254 (2003) pp 735–74110.1016/S0043-1648(03)00260-6 ↗
16. T. Manisekaran, M. Kamaraj, S. M. Sharif and S. V. Joshi, Slurry Erosion Studies on Surface Modified 13Cr-4Ni Steels: Effect of Angle of Impingement and Particle Size, Journal of Materials Engineering and Performance, Vol 16, No 5, Oct 2007, 567–57210.1007/s11665-007-9068-5 ↗
17. I·V. Rivero and C·O. Ruud, Residual Stresses and Patterns in 52100 Bearing Steel: Preliminary Analysis of Strain Hardening vs. Micro Structural Transformation by XRD Analysis, J. Soc. Tribol. Lubr. Eng., 2002, 58, p 30–40
18. J.Grum and R.Sturm, Deformation of Specimen During Laser Surface Remelting J. Mater. Eng. Perform., Volume 9(2) April 2000, 138–14610.1361/105994900770346079 ↗