journal article·2026-01-12Open access

Ambient-cured alkali-activated geopolymer mortars: influence of activator molarity and fly ash replacement on microstructure and mechanical performance

Kenan Toklu, Buğra Aydın, İlhami Demir, Şükrü Demir, Gazi Günel, Özer Sevim

Abstract

Abstract This study investigates the mechanical and microstructural behavior of ambient-cured geopolymer mortars synthesized with ground granulated blast furnace slag (GBFS) and Class F fly ash (FA) as binder materials. Sodium hydroxide (NaOH) solutions at molarities of 4 M, 6 M, and 8 M were used as alkali activators, while GBFS was partially replaced with FA at ratios ranging from 0% to 25% by weight. The fresh and hardened properties of the mortars were evaluated through flow table tests, flexural and compressive strength measurements, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX), and mercury intrusion porosimetry (MIP). Results indicated that higher activator molarity significantly enhanced both the flexural and compressive strengths, while increased FA content improved workability but adversely affected strength. Microstructural analyses revealed that greater FA replacement led to more microcracks and higher porosity, contributing to reduced mechanical performance. The formation of C-A-S-H and N-A-S-H gels was observed to be critical for strength development. The findings suggest that optimizing activator molarity and binder composition is essential for achieving durable, environmentally friendly geopolymer mortars under ambient curing conditions. Unlike most existing studies relying on elevated-temperature curing, this study offers a detailed analysis of ambient-cured systems using only industrial by-products, thus providing a novel framework for low-energy geopolymer mortar production suitable for real-world applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Microbial Applications in Construction Materials · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Rahmani Z, Ahmadi J. The impact of human activities on climate change. Sprin J Arts Humanit Social Sci. 2024;3(6):24–7.
2. Liu X, Yang L, Du J, Zhang H, Hu J, Chen A, Lv W. Carbon and air pollutant emissions forecast of China’s cement industry from 2021 to 2035. Volume 204. Resources, Conservation and Recycling; 2024. p. 107498.10.1016/j.resconrec.2024.107498 ↗
3. Emma L. Sustainable construction practices. Incorporating Green Materials and Technologies in Civil Engineering Projects; 2024.
4. Derrouiche Y, Achoura D, Saliba J, Cassagnabère F. (2025). Natural Pozzolan as a sustainable cement replacement in high-performance concrete: effects on mechanical properties, durability, and microstructural development. Sci Afr, 27, e02574.10.1016/j.sciaf.2025.e02574 ↗
5. Zhang B. (2024). Durability of sustainable geopolymer concrete: A critical review. Sustainable Mater Technol, e00882.10.1016/j.susmat.2024.e00882 ↗
6. Panda S, Panigrahi SK. Production of sustainable GGBFS-based Self-Compacting geopolymer concrete containing E-waste aggregates under ambient temperature curing. Constr Build Mater. 2024;440:137373.10.1016/j.conbuildmat.2024.137373 ↗
7. Vázquez-Rodríguez FJ, López-Yépez LG, Elizondo-Villarreal N, Guzmán-Hernández AM, Gómez-Zamorano LY, Rodríguez-Castellanos EA. The effect of µ-Limestone additions on the Mechano-Chemical and microstructural properties of slag and binary slag/Ground fly Ash Alkaline-Activated binders. Materials. 2024;17(23):5940.10.3390/ma17235940 ↗
8. Vázquez-Rodríguez F, Elizondo N, Montes-González M, Gómez-Rodríguez C, González-Carranza Y, Guzmán AM, Rodríguez EA. Microstructural and mechanical characteristics of alkali-activated binders composed of milled fly Ash and granulated blast furnace slag with µ-limestone addition. Materials. 2023;16(10):3818.10.3390/ma16103818 ↗
9. Coppola L, Bellezze T, Belli A, Bignozzi MC, Bolzoni F, Brenna A, Yang F. Binders alternative to Portland cement and waste management for sustainable construction—Part 1. J Appl Biomater Funct Mater. 2018;16(3):186–202.
10. Singh NB, Middendorf B. Geopolymers as an alternative to Portland cement: an overview. Constr Build Mater. 2020;237:117455.10.1016/j.conbuildmat.2019.117455 ↗
11. Habert G, D’Espinose de Lacaillerie JB, Lanta E, Roussel N. (2010, June). Environmental evaluation for cement substitution with geopolymers. In Proceedings of the 2nd international conference on sustainable construction materials and technologies (pp. 1607–1615).
12. Kaya AK, Onur Mİ. Optimization of physical, mechanical and thermal properties of two-part geopolymer mortar by Taguchi method. Constr Build Mater. 2025;476:141208.10.1016/j.conbuildmat.2025.141208 ↗
13. Madirisha MM, Dada OR, Ikotun BD. Chemical fundamentals of geopolymers in sustainable construction. Mater Today Sustain. 2024;82:100842.
14. Ikotun JO, Aderinto GE, Madirisha MM, Katte VY. Geopolymer cement in pavement applications: bridging sustainability and performance. Sustainability. 2024;16(13):5417.10.3390/su16135417 ↗
15. Deevasan KK, Ranganath RV. Geopolymer concrete using industrial byproducts. Proc Institution Civil Engineers-Construction Mater. 2011;164(1):43–50.10.1680/coma.900034 ↗
16. Kubba Z, Huseien GF, Sam ARM, Shah KW, Asaad MA, Ismail M, Mirza J. Impact of curing temperatures and alkaline activators on compressive strength and porosity of ternary blended geopolymer mortars. Case Stud Constr Mater. 2018;9:e00205.
17. Shekhovtsova J, Kovtun M, Kearsley EP. Evaluation of short-and long-term properties of heat-cured alkali-activated fly Ash concrete. Magazine Concrete Res. 2015;67(16):897–905.10.1680/macr.14.00377 ↗
18. Khaleel F, Atiş C, Durak U, İlkentapar S, Karahan O. The effect of microwave curing on the strength development of Class-F fly ash-based geopolymer mortar. Erciyes Üniversitesi Fen Bilimleri Enstitüsü Fen Bilimleri Dergisi. 2021;37(1):118–29.
19. Siciliano UC, Zhao J, Trindade ACC, Liebscher M, Mechtcherine V, de Andrade Silva F. Influence of curing temperature and pressure on the mechanical and microstructural development of metakaolin-based geopolymers. Constr Build Mater. 2024;424:135852.10.1016/j.conbuildmat.2024.135852 ↗
20. Singh GB, Subramaniam KV. Influence of processing temperature on the reaction product and strength gain in alkali-activated fly Ash. Cem Concr Compos. 2019;95:10–8.10.1016/j.cemconcomp.2018.10.010 ↗
21. Ling Y, Wang K, Wang X, Hua S. Effects of mix design parameters on heat of geopolymerization, set time, and compressive strength of high calcium fly Ash geopolymer. Constr Build Mater. 2019;228:116763.10.1016/j.conbuildmat.2019.116763 ↗
22. Nagral MR, Ostwal T, Chitawadagi MV. Effect of curing temperature and curing hours on the properties of geo-polymer concrete. Int J Comput Eng Res. 2014;4(9):1–11.
23. Sajan P, Jiang T, Lau C, Tan G, Ng K. Combined effect of curing temperature, curing period and alkaline concentration on the mechanical properties of fly ash-based geopolymer. Clean Mater. 2021;1:100002.10.1016/j.clema.2021.100002 ↗
24. Duxson P, Provis JL, Lukey GC, Van Deventer JS. The role of inorganic polymer technology in the development of ‘green concrete’. Cem Concr Res. 2007;37(12):1590–7.10.1016/j.cemconres.2007.08.018 ↗
25. TS EN 196-1. Methods of testing cement - Part 1: determination of strength. Ankara: Turkish Standards Institution; 2016.
26. TS EN 1015-3. Methods of test for mortar for masonry- part 3: determination of consistence of fresh mortar (by flow table). Ankara: Turkish Standards Institution; 2000.
27. Pundienė I, Pranckevičienė J, Zhu C, Kligys M. The role of temperature and activator solution molarity on the viscosity and hard structure formation of geopolymer pastes. Constr Build Mater. 2021;272:121661.10.1016/j.conbuildmat.2020.121661 ↗
28. Han AL, Ekaputri JJ. (2018). The influence of molarity variations to the mechanical behavior of geopolymer concrete. In MATEC web of conferences (Vol. 195, p. 01010). EDP Sciences.10.1051/matecconf/201819501010 ↗
29. Tayeh BA, Zeyad AM, Agwa IS, Amin M. (2021). Effect of elevated temperatures on mechanical properties of lightweight geopolymer concrete. Case Stud Constr Mater, 15, e00673.10.1016/j.cscm.2021.e00673 ↗
30. Mahmoud HA, Tawfik TA, Abd El-razik MM, Faried AS. Mechanical and acoustic absorption properties of lightweight fly ash/slag-based geopolymer concrete with various aggregates. Ceram Int. 2023;49(13):21142–54.10.1016/j.ceramint.2023.03.244 ↗
31. Hardjito D, Wallah SE, Sumajouw DMJ, Rangan BV. On the development of fly ash-based geopolymer concrete. ACI Mater J. 2004;101(6):467–72.
32. Ergeshov Z, Örklemez E, Ketema AF, Kwami MIA, Ilkentapar S, Durak U, Atis CD. (2025). Influence of silica fume on the mechanical and microstructural properties and life cycle assessment of fly Ash-Based geopolymer mortar. Arab J Sci Eng, 1–18.10.1007/s13369-025-10142-9 ↗
33. Aslan S, Erkan İH. The effects of fly ash, blast furnace slag, and limestone powder on the physical and mechanical properties of geopolymer mortar. Appl Sci. 2024;14(2):553.10.3390/app14020553 ↗
34. Kamath M, Prashant S, Ralegaonkar R. Microstructure properties of popular alkali-activated pastes cured in ambient temperature. Buildings. 2023;13(4):858.10.3390/buildings13040858 ↗
35. García-Lodeiro I, Palomo A, Fernández-Jiménez A, Macphee DE. Compatibility studies between NASH and CASH gels. Study in the ternary diagram Na2O–CaO–Al2O3–SiO2–H2O. Cem Concr Res. 2011;41(9):923–31.10.1016/j.cemconres.2011.05.006 ↗
36. Chindaprasirt P, Jaturapitakkul C, Chalee W, Rattanasak U. Comparative study on the characteristics of fly Ash and bottom Ash geopolymers. Waste Manag. 2009;29(2):539–43.10.1016/j.wasman.2008.06.023 ↗
37. Görhan G, Kürklü G. The influence of the NaOH solution on the properties of the fly ash-based geopolymer mortar cured at different temperatures. Compos Part B: Eng. 2014;58:371–7.10.1016/j.compositesb.2013.10.082 ↗
38. Somna K, Jaturapitakkul C, Kajitvichyanukul P, Chindaprasirt P. NaOH-activated ground fly Ash geopolymer cured at ambient temperature. Fuel. 2011;90(6):2118–24.10.1016/j.fuel.2011.01.018 ↗
39. Hanjitsuwan S, Hunpratub S, Thongbai P, Maensiri S, Sata V, Chindaprasirt P. Effects of NaOH concentrations on physical and electrical properties of high calcium fly Ash geopolymer paste. Cem Concr Compos. 2014;45:9–14.10.1016/j.cemconcomp.2013.09.012 ↗
40. Castillo H, Collado H, Droguett T, Sánchez S, Vesely M, Garrido P, Palma S. Factors affecting the compressive strength of geopolymers: A review. Minerals. 2021;11(12):1317.10.3390/min11121317 ↗
41. Ariyadasa PW, Manalo AC, Lokuge W, Aravinthan V, Gerdes A, Kaltenbach J, Galvan BA. Macro and microstructural evolution of low-calcium fly ash-based geopolymer mortar exposed to sulphuric acid corrosion. Cem Concr Res. 2024;178:107436.10.1016/j.cemconres.2024.107436 ↗
42. Lingyu T, Dongpo H, Jianing Z, Hongguang W. Durability of geopolymers and geopolymer concretes: A review. Reviews Adv Mater Sci. 2021;60(1):1–14.10.1515/rams-2021-0002 ↗
43. Wang L, Yu Z, Liu B, Zhao F, Tang S, Jin M. Effects of fly Ash dosage on shrinkage, crack resistance and fractal characteristics of face slab concrete. Fractal Fract. 2022;6(6):335.10.3390/fractalfract6060335 ↗
44. Cheng Y, Shen H, Zhang J. Understanding the effect of high-volume fly Ash on micro-structure and mechanical properties of cemented coal gangue paste backfill. Constr Build Mater. 2023;378:131202.10.1016/j.conbuildmat.2023.131202 ↗
45. Zhang D, Zhu T, Yang Q, Vandeginste V, Li J. Influence of ground granulated blast furnace slag on recycled concrete powder-based geopolymer cured at ambient temperature: Rheology, mechanical properties, reaction kinetics and air-void characteristics. Constr Build Mater. 2024;438:137190.10.1016/j.conbuildmat.2024.137190 ↗
46. Chiranjeevi K, Abraham M, Rath B, Praveenkumar TR. Enhancing the properties of geopolymer concrete using nano-silica and microstructure assessment: a sustainable approach. Sci Rep. 2023;13(1):17302.10.1038/s41598-023-44491-y ↗
47. Jeong Y, Park H, Jun Y, Jeong JH, Oh JE. Influence of slag characteristics on strength development and reaction products in a CaO-activated slag system. Cem Concr Compos. 2016;72:155–67.10.1016/j.cemconcomp.2016.06.005 ↗
48. Gök SG, Kılınç K. Mechanical properties of fly Ash and blast furnace slag based alkali activated concrete. Kırklareli Üniversitesi Mühendislik Ve Fen Bilimleri Dergisi. 2017;3(2):123–31.
49. He P, Wang M, Fu S, Jia D, Yan S, Yuan J, Zhou Y. Effects of Si/Al ratio on the structure and properties of Metakaolin based geopolymer. Ceram Int. 2016;42(13):14416–22.10.1016/j.ceramint.2016.06.033 ↗
50. Liu J, Li X, Lu Y, Bai X. Effects of Na/Al ratio on mechanical properties and microstructure of red mud-coal Metakaolin geopolymer. Constr Build Mater. 2020;263:120653.10.1016/j.conbuildmat.2020.120653 ↗
51. Provis JL, van Deventer JSJ. Geopolymers: Structure, processing, properties and industrial applications. Woodhead Publishing; 2009.10.1533/9781845696382 ↗
52. Xu Z, Yue J, Pang G, Li R, Zhang P, Xu S. Influence of the activator concentration and Solid/Liquid ratio on the strength and shrinkage characteristics of Alkali-Activated slag geopolymer pastes. Adv Civil Eng. 2021;20211:6631316.10.1155/2021/6631316 ↗
53. Fernández-Jiménez A, Palomo A. Composition and microstructure of alkali activated fly Ash binder: effect of the activator. Cem Concr Res. 2005;35(10):1984–92.10.1016/j.cemconres.2005.03.003 ↗
54. Chen S, Ruan S, Zeng Q, Liu Y, Zhang M, Tian Y, Yan D. Pore structure of geopolymer materials and its correlations to engineering properties: A review. Constr Build Mater. 2022;328:127064.10.1016/j.conbuildmat.2022.127064 ↗