Microstructures and Mechanical Properties of Laser Welding Joint of a CLAM Steel with Revised Chemical Compositions
Source abstract
Abstract
To suppress the tendency to form delta ferrite in weld metal (WM) of China low activation martensitic (CLAM) steel joint, a CLAM steel with revised chemical compositions was designed. Laser welding of the CLAM steel was investigated. The microstructures of the WM and heat-affected zone were analyzed. The impact toughness of the WM was evaluated by a Charpy impact test method with three V notches. The influence of temper temperature on mechanical properties was analyzed. It was found that the delta ferrite was eliminated almost completely in laser WM of CLAM steel with revised chemical compositions which has lower tendency to form delta ferrite than original chemical compositions. The joint has higher tensile strength than the parent metal. With increasing the heat input, the impact toughness of the joint is approximatively equal with that of parent metal first and then decreases obviously. Temper treatment could effectively improve mechanical property of the joint. When the temper temperature exceeds 600 °C, the impact toughness of the joint is higher than that of the parent metal.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Metal Alloys Wear and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. B. van der Schaaf, D.S. Gelles, S. Jitsukawa, S. Jitsukawa, A. Kimura, R.L. Klueh, A. Moèslang, and G.R. Odette, Progress and Critical Issues of Reduced Activation Ferritic/Martensitic Steel Development, J. Nucl. Mater., 2000, 283-287, p 52–5910.1016/S0022-3115(00)00220-8 ↗
2. J. Yu, Q. Huang, and F. Wan, Research and Development on the China Low Activation Martensitic Steel (CLAM), J. Nucl. Mater., 2007, 367-370, p 97–10110.1016/j.jnucmat.2007.03.236 ↗
3. Y. Li, Q. Huang, Y. Wu, T. Nagasaka, and T. Muroga, Mechanical Properties and Microstructures of China Low Activation Martensitic Steel Compared with JLF-1, J. Nucl. Mater., 2007, 117-121, p 367–370
4. H. Tanigawa, T. Hirose, K. Shiba, R. Kasada, E. Wakai, H. Serizawa, Y. Kawahito, S. Jitsukawa, A. Kimura, Y. Kohno, A. Kohyama, S. Katayama, H. Mori, K. Nishimoto, R.L. Klueh, M.A. Sokolov, R.E. Stoller, and S.J. Zinkle, Technical Issues of Reduced Activation Ferritic/Martensitic Steels for Fabrication of ITER Test Blanket Modules, Fusion Eng. Des., 2008, 83, p 1471–147610.1016/j.fusengdes.2008.07.024 ↗
5. A. Cardella, E. Rigal, L. Bedel, P. Bucci, J. Fiek, L. Forest, and L.V. Boccaccini, The Manufacturing Technologies of the European Breeding Blankets, J. Nucl. Mater., 2004, 329-333, p 133–14010.1016/j.jnucmat.2004.04.014 ↗
6. Q.Y. Huang, C.J. Li, Y.F. Li, S.J. Li, Y.C. Wu, J.G. Li, F.R. Wan, X. Ju, Y.Y. Shan, J.N. Yu, S.Y. Zhu, P.Y. Zhang, J.F. Yang, F.S. Han, M.G. Kong, H.Q. Li, T. Muroga, and T. Nagasaka, R&D Status of China Low Activation Martensitic Steel, Chin. J. Nucl. Sci. Eng., 2007, 27(1), p 41–50 (in Chinese)
7. X.Z. Chen, Y.M. Huang, B. Madigan, and J.Z. Zhou, An Overview of the Welding Technologies of CLAM Steels for Fusion Application, Fusion Eng. Des., 2012, 87, p 1639–164610.1016/j.fusengdes.2012.06.009 ↗
8. C.J. Li, Q.Y. Huang, Q.S. Wu, S.J. Liu, Y.C. Lei, T. Muroga, T. Nagasaka, J.X. Zhang, and J.L. Li, Welding Techniques Development of CLAM Steel for Test Blanket Module, Fusion Eng. Des., 2009, 84, p 1184–118710.1016/j.fusengdes.2008.12.039 ↗
9. Z.Z. Jiang, L.T. Ren, J.H. Huang, X. Ju, H.B. Wu, Q.Y. Huang, and Y.C. Wu, Microstructure and Mechanical Properties of the TIG Welded Joints of Fusion CLAM Steel, Fusion Eng. Des., 2010, 85, p 1903–190810.1016/j.fusengdes.2010.06.019 ↗
10. Q. Zhu, Y.C. Lei, X.Z. Chen, W.J. Ren, X. Ju, and Y.M. Ye, Microstructure and Mechanical Properties in TIG Welding of CLAM Steel, Fusion Eng. Des., 2011, 86, p 407–41110.1016/j.fusengdes.2011.03.070 ↗
11. J. Hu, Z.Z. Jiang, J.H. Huang, S.H. Chen, X.K. Zhao, and H. Zhang, Effects of Heat Treatment Processes on Microstructure and Impact Toughness of Weld Metal of Vacuum Electron Beam Welding on CLAM Steel, Trans. China Weld. Inst., 2012, 33(11), p 67–71 (in Chinese)
12. Z.Z. Jiang, J.H. Huang, S.H. Chen, and X. Ju, Microstructure Transformation and Mechanical Properties of Electron Beam Welded Joints of Fusion CLAM Steel, Trans. China Weld. Inst., 2011, 32(3), p 45–48 (in Chinese)
13. Y. Lei, M. Han, Q. Zhu, and X. Ju, Microstructure and Hardness of Laser Welded Joint of China Low Activation Martensitic Steel, Trans. China Weld. Inst., 2010, 31(1), p 5–8 (in Chinese)
14. Z.Z. Jiang, J.H. Huang, J. Hu, and S.H. Chen, Microstructure and Mechanical Properties of Laser Welded Joints of CLAM Steel Used for Fusion Reactor, Trans. China Weld. Inst., 2012, 33(2), p 5–8 (in Chinese)
15. C.A. Wang, R.L. Klueh, and B.A. Chin, The Weldability of Low Activation Cr-W Steels, J. Nucl. Mater., 1992, 191-194, p 831–83510.1016/0022-3115(92)90589-D ↗
16. J. Onoro, Weld Metal Microstructure Analysis of 9-12% Cr Steels, J. Mater. Process. Technol., 2006, 180, p 137–14210.1016/j.jmatprotec.2006.05.014 ↗
17. J. Hald, Microstructure and Long-Term Creep Properties of 9-12% Cr Steels, Int. J. Press. Vessels Pip., 2008, 85, p 30–3710.1016/j.ijpvp.2007.06.010 ↗
18. Q.S. Wu, S.H. Zheng, S.J. Liu, C.J. Li, and Q.Y. Huang, Effect of Post-weld Heat Treatment on the Mechanical Properties of Electron Beam Welded Joints for CLAM Steel, J. Nucl. Mater., 2013, 442, p 512–51710.1016/j.jnucmat.2013.07.041 ↗
19. S. Sam, C.R. Das, V. Ramasubbu, S.K. Albert, A.K. Bhaduri, T. Jayakumar, and E. Rajendra Kumar, Delta Ferrite in the Weld Metal of Reduced Activation Ferritic Martensitic Steel, J. Nucl. Mater., 2014, 455, p 343–34810.1016/j.jnucmat.2014.07.008 ↗
20. J. Moon, C.H. Lee, T.H. Lee, M.H. Jang, M.G. Park, and H.N. Han, Phase Transformation and Impact Properties in the Experimentally Simulated Weld Heat-Affected Zone of a Reduced Activation Ferritic/Martensitic Steel, J. Nucl. Mater., 2014, 455, p 81–8510.1016/j.jnucmat.2014.04.048 ↗
21. R. Rai, S.M. Kelly, R.P. Martukanitz et al., A Convective Heat-Transfer Model for Partial and Full Penetration Keyhole Mode Laser Welding of a Structural Steel, Metall. Mater. Trans. A, 2008, 39, p 98–11210.1007/s11661-007-9400-6 ↗
22. D.-W. Cho, W.-I. Cho, and S.-J. Na, Modeling and Simulation of Arc: Laser and Hybrid Welding Process, J. Manuf. Process., 2014, 16, p 26–5510.1016/j.jmapro.2013.06.012 ↗
23. R.L. Klueh and R. Harries Donald, High-Chromium Ferritic and Martensitic Steels for Nuclear Applications, ASTM, West Conshohocken, PA, 2001, p 3510.1520/MONO3-EB ↗