journal article·2017-05

Investigation on Conductive Layer, Delamination, and Recast Layer Characteristics of Electro-discharge Machined Holes in TBCs

Li Wang, Yongfeng Guo, Guowei Zhang

Publisher page

Abstract

In this study, electrical discharge machining (EDM) is used to directly drill normal effusion cooling holes in thermal-barrier-coated nickel-based superalloys (TBCs) via the assisting electrode method. The formation of the conductive layer was studied using scanning electron microscopy and energy-dispersive spectroscopy. The effects of the EDM process parameters including peak current, pulse duration, and duty cycle on delamination and recast layer characteristics were investigated. The analysis results indicate that the conductive layer possesses a feature of bilayer structure for the EDM of TBCs. The bottom layer is generated first due to the deposition of carbon-based products and molten brass debris, and its composition primarily contains C, Cu, Zr, and Zn; the surface layer is the result of the overlying of subsequently molten superalloy debris and carbon-based products, and its composition primarily consists of Ni, C, Cr, Nb, Co, Al, Fe, Cu, and Zr. The microcracks of the superalloy substrate only reside in the recast layer during the EDM of TBCs. The thickness of recast layer sharply increases with increasing peak current, pulse duration, and duty cycle, respectively. The delamination occurs at the ceramic coating/bond coating interface for the EDM of drilling normal holes in TBCs, and it can be eliminated by the selection of low discharge energy and appropriate duty cycle. Additionally, the length of delamination increases with increasing peak current, pulse duration, and duty cycle, respectively. The spalling of ceramic coating appears at the entrance of the hole due to the thermal-shock brittle fracture if excessive peak current, pulse duration, or duty cycle is selected.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced machining processes and optimization · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. A. Corcoran, L. Sexton, B. Seaman, P. Ryan, and G. Byrne, The Laser Drilling of Multi-layer Aerospace Material System, J. Mater. Process. Technol., 2002, 123(1), p 100–10610.1016/S0924-0136(01)01123-2 ↗
2. S.K. Mishra, N. Jagdeesh, and L.C. Pathak, Fabrication of Nanosized Lanthanum Zirconate Powder and Deposition of Thermal Barrier Coating by Plasma Spray Process, J. Mater. Eng. Perform., 2016, 25(7), p 2570–257510.1007/s11665-016-2122-4 ↗
3. M. Azadi, G.H. Farrahi, and A. Moridi, Optimization of Air Plasma Sprayed Thermal Barrier Coating Parameters in Diesel Engine Applications, J. Mater. Eng. Perform., 2013, 22(11), p 3530–353810.1007/s11665-013-0629-5 ↗
4. Q. Feng, Y.N. Picard, H. Liu, S.M. Yalisove, G. Mourou, and T.M. Pollock, Femtosecond Laser Micromachining of a Single-Crystal Superalloy, Scr. Mater., 2005, 53(5), p 511–51610.1016/j.scriptamat.2005.05.006 ↗
5. C.A. McNally, J. Folkes, and I.R. Pashby, Laser Drilling of Cooling Holes in Aeroengines: State of the Art and Future Challenges, Mach. Sci. Technol., 2004, 20(7), p 805–813
6. J. Kamalua, P. Byrdb, and A. Pitmana, Variable Angle Laser Drilling of Thermal Barrier Coated Nimonic, J. Mater. Process. Technol., 2002, 122(2–3), p 355–36210.1016/S0924-0136(02)00044-4 ↗
7. H.K. Sezer, L. Li, M. Schmidt, A.J. Pinkerton, B. Anderson, and P. Williams, Effect of Beam Angle on HAZ, Recast and Oxide Layer Characteristics in Laser Drilling of TBC Nickel Superalloys, Int. J. Mach. Tools Manuf., 2006, 46(15), p 1972–198210.1016/j.ijmachtools.2006.01.010 ↗
8. S. Bandyopadhyay, J.K.S. Sundar, G. Sundararajan, and S.V. Joshi, Geometrical Features and Metallurgical Characteristics of Nd:YAG Laser Drilled Holes in ThickIN718 and Ti–6Al–4V Sheets, J. Mater. Process. Technol., 2002, 127(1), p p83–p9510.1016/S0924-0136(02)00270-4 ↗
9. J. Lv, X. Dong, K.D. Wang, W.Q. Duan, Z.J. Fan, and X.S. Mei, Study on Process and Mechanism of Laser Drilling in Water and Air, Int. J. Adv. Manuf. Technol., 2016, 86(5), p p1443–p145110.1007/s00170-015-8279-4 ↗
10. M.N. Zervas and C.A. Codemard, High Power Fiber Lasers: A Review, IEEE J. Sel. Top. Quantum Electron., 2014, 20(5), p 090412310.1109/JSTQE.2014.2321279 ↗
11. C.A. Biffi and B. Previtali, Spatter Reduction in Nanosecond Fibre Laser Drilling Using an Innovative Nozzle, Int. J. Adv. Manuf. Technol., 2013, 66(9), p 1231–124510.1007/s00170-012-4402-y ↗
12. B. Shiner, Fiber Lasers Poised to Impact Aerospace Component Drilling, Laser Focus World, 2013, 49(8), p 53–55
13. B. Adelmann and R. Hellmann, Rapid Micro Hole Laser Drilling in Ceramic Substrates Using Single Mode Fiber Laser, J. Mater. Process. Technol., 2015, 221, p 80–8610.1016/j.jmatprotec.2015.02.014 ↗
14. J.D. Lin, D. Lu, and Y.T. Dai, A Review on Fiber Lasers, China Commun., 2012, 9(8), p 1–1510.3724/SP.J.1016.2012.00001 ↗
15. M. Nguyen, C. Loumena, A. Bussière, R. Kling, C. Delor, and E. Freysz, Can Fiber Laser Improve High Speed Multi-pulse Drilling of Aeronautic Alloy?, Proc. SPIE, 2016, 9741, p 97410710.1117/12.2211834 ↗
16. U. Gupta, A.K. Nath, and P.P. Bandyopadhyay, Laser Micro-hole Drilling in Thermal Barrier Coated Nickel Based Superalloy, IOP Conf. Ser. Mater. Sci. Eng., 2016, 149, p 01207610.1088/1757-899X/149/1/012076 ↗
17. D.K. Das and T.M. Pollock, Femtosecond Laser Machining of Cooling Holes in Thermal Barrier Coated CMSX4 Superalloy, J. Mater. Process. Technol., 2009, 209(15–16), p 5661–566810.1016/j.jmatprotec.2009.05.031 ↗
18. J. Girardot, M. Schneider, L. Berthe, and V. Favier, Investigation of Delamination Mechanisms During a Laser Drilling on a Cobalt-BASE Superalloy, J. Mater. Process. Technol., 2013, 213(10), p 1682–169110.1016/j.jmatprotec.2013.04.003 ↗
19. Z.J. Fan, X. Dong, K.D. Wang, W.Q. Duan, R.J. Wang, X.S. Mei, W.J. Wang, J.L. Cui, X. Yuan, and C.Y. Xu, Effect of Drilling Allowance on TBC Delamination, Spatter and Re-melted Cracks Characteristics in Laser Drilling of TBC Coated Superalloys, Int. J. Mach. Tools Manuf., 2016, 106, p 1–1010.1016/j.ijmachtools.2016.03.008 ↗
20. H.K. Sezer and L. Li, Mechanisms of Acute Angle Laser Drilling Induced Thermal Barrier Coating Delamination, J. Manuf. Sci. Eng.-Trans. ASME, 2009, 131(5), p 611–62310.1115/1.4000102 ↗
21. D.K. Das, J.P. McDonald, S.M. Yalisove, and T.M. Pollock, Depth-Profiling Study of a Thermal Barrier Coated Superalloy Using Femtosecond Laser-Induced Breakdown Spectroscopy, Spectrochim. Acta B At. Spectrosc., 2008, 63(1), p 27–3610.1016/j.sab.2007.10.048 ↗
22. M. Antar, D. Chantzis, S. Marimuthu, and P. Hayward, High Speed EDM and Laser Drilling of Aerospace Alloys, Procedia CIRP, 2016, 42, p 526–53110.1016/j.procir.2016.02.245 ↗
23. F. Klocke, A. Klink, D. Veselovac, D.K. Aspinwall, S.L. Soo, M. Schmidt, J. Schilp, G. Levy, and J.P. Kruth, Turbomachinery Component Manufacture by Application of Electrochemical, Electro-physical and Photonic Processes, CIRP Ann. Manuf. Technol., 2014, 63(2), p 703–72610.1016/j.cirp.2014.05.004 ↗
24. Y. Zhang, Z.Y. Xu, D. Zhu, N.S. Qu, and Y. Zhu, Drilling of Film Cooling Holes by a EDM/ECM in Situ Combined Process Using Internal and Side Flushing of Tubular Electrode, Int. J. Adv. Manuf. Technol., 2016, 83(1–4), p 505–51710.1007/s00170-015-7575-3 ↗
25. Z.Y. Li, X.T. Wei, Y.B. Guo, and M.P. Sealy, State-of-Art, Challenges, and Outlook on Manufacturing of Cooling Holes for Turbine Blades, Mach. Sci. Technol., 2015, 19(3), p 361–39910.1080/10910344.2015.1051543 ↗
26. M. Imran, P.T. Mativeng, A. Gholinia, and P.J. Withers, Assessment of Surface Integrity of Ni Superalloy after Electrical-Discharge, Laser and Mechanical Micro-Drilling Processes, Int. J. Adv. Manuf. Technol., 2015, 79(5–8), p 1303–131110.1007/s00170-015-6909-5 ↗
27. Y. Fukuzawa, N. Mohri, and T. Tani, Machining Characteristics of Insulating Ceramics by Electrical Discharge Machine, Ind. Ceram., 2001, 21(3), p 187–189
28. N. Mohri, Y. Fukuzawa, T. Tani, T. Saito, N. Saito, and K. Furutani, Assisting Electrode Method for Machining Insulating Ceramics, CIRP Ann. Manuf. Technol., 1996, 45(1), p 201–20410.1016/S0007-8506(07)63047-9 ↗
29. Y. Fukuzawa, N. Mohri, H. Gotoh, and T. Tani, Three-Dimensional Machining of Insulating Ceramics Materials with Electrical Discharge Machining, Trans. Nonferrous Met. Soc. China, 2009, 19(1), p 150–15610.1016/S1003-6326(10)60263-4 ↗
30. D. Hanaoka, R. Ito, and Y. Fukuzawa, Electrical Discharge Machined Surface of the Insulating ZrO3 ceramics, J. Adv. Mech. Des. Syst. Manuf., 2011, 5(4), p 372–38410.1299/jamdsm.5.372 ↗
31. G. Kucukturk and C. Cogun, A New Method for Machining of Electrically Nonconductive Workpieces Using Electric Discharge Machining Technique, Mach. Sci. Technol., 2010, 14(2), p 189–20710.1080/10910344.2010.500497 ↗
32. Y.F. Guo, P.J. Hou, D.X. Shao, Z.F. Li, L. Wang, and L. Tang, High-Speed Wire Electrical Discharge Machining of Insulating Zirconia with a Novel Assisting Electrode, Mater. Manuf. Processes, 2014, 29(5), p 526–53110.1080/10426914.2014.892983 ↗
33. Y.F. Guo, G.W. Zhang, L. Wang, and Y.F. Hu, Optimization of Parameters for EDM Drilling of Thermal-Barrier-Coated Nickel Superalloys Using Gray Relational Analysis Method, Int. J. Adv. Manuf. Technol., 2016, 83(9–12), p 1595–160510.1007/s00170-015-7685-y ↗
34. B. Lauwers, J.P. Kruth, W. Liu, W. Eeraerts, B. Schacht, and P. Bleys, Investigation of Material Removal Mechanisms in EDM of Composite Ceramic Materials, J. Mater. Process. Technol., 2004, 149(1–3), p 347–35210.1016/j.jmatprotec.2004.02.013 ↗
35. K.T. Voisey and T.W. Clyne, Laser Drilling of Cooling Holes through Plasma Sprayed Thermal Barrier Coatings, Surf. Coat. Technol., 2004, 176(3), p 296–30610.1016/S0257-8972(03)00748-5 ↗
36. V. Kumar and K. Balasubramanian, Progress Update on Failure Mechanisms of Advanced Thermal Barrier Coatings: A Review, Prog. Org. Coat., 2016, 90, p 54–8210.1016/j.porgcoat.2015.09.019 ↗
37. C.S. Trueman and J. Huddleston, Material Removal by Spalling during EDM of Ceramics, J. Eur. Ceram. Soc., 2000, 20(10), p 1629–163510.1016/S0955-2219(00)00027-3 ↗
38. H.M. Zhang, Effect of Wire Electrical Discharge Machining (WEDM) Parameters on Surface Integrity of Nanocomposite Ceramics, Ceram. Int., 2014, 40(7), p 9657–966210.1016/j.ceramint.2014.02.046 ↗
39. R.A. Miller and C.E. Lowell, Failure Mechanisms of Thermal Barrier Coatings Exposed to Elevated Temperatures, Thin Solid Films, 1982, 95, p 265–27310.1016/0040-6090(82)90019-0 ↗
40. A. Bennett, Properties of Thermal Barrier Coatings, Mater. Sci. Technol., 1986, 2, p 257–26110.1179/mst.1986.2.3.257 ↗