Effects of Heat Treatment on Corrosion and Wear Behaviors of Mg-6Gd-2Zn-0.4Zr Alloy in Simulated Body Fluid
Source abstract
Abstract
Mg-6Gd-2Zn-0.4Zr (wt.%, GZ62K) alloy was processed by solution treatment under different temperatures. The microstructure, hardness, corrosion and wear behaviors in simulated body fluid (SBF) have been studied. The results indicate that the (Mg, Zn)3Gd phase decreases, the precipitated phases gradually increase, and the long-period stacking ordered structure disappears with the increase of solution temperature. The alloy has better corrosion resistance after solution treatment, and that solution treated at 490 °C for 12 h shows the best corrosion resistance. The friction coefficient of the alloy under dry sliding condition decreases slightly, but the mass loss increases with increasing the solution temperature. The alloy solution treated at 460 °C for 12 h exhibits the lowest friction coefficient and mass loss in SBF, and it also has the best wear resistance under dry sliding condition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Q.Z. Chen and G.A. Thouas, Metallic Implant Biomaterials, Mater. Sci. Eng., R, 2015, 87, p 1–5710.1016/j.mser.2014.10.001 ↗
2. M.P. Staiger, A.M. Pietak, J. Huadamai, and G. Dias, Magnesium and it Alloys As Orthopedic Biomaterials: A Review, Biomaterials, 2006, 27, p 1728–173410.1016/j.biomaterials.2005.10.003 ↗
3. Y.J. Chen, Z.G. Xu, C. Smith, and J. Sankar, Recent Advances on the Development of Magnesium Alloys for Biodegradable Implants, Acta Biomater., 2014, 10, p 4561–457310.1016/j.actbio.2014.07.005 ↗
4. H. Tang, T.Z. Xin, Y. Luo, and F.P. Wang, In Vitro Degradation of AZ31 Magnesium Alloy Coated with Hydroxyapatite by Sol–Gel Method, Mater. Sci. Technol., 2013, 29, p 547–55210.1179/1743284712Y.0000000180 ↗
5. W.J. Zhang, M.H. Li, Q. Chen, W.Y. Hu, W.M. Zhang, and W. Xin, Effects of Sr and Sn on Microstructure and Corrosion Resistance of Mg–Zr–Ca Magnesium Alloy for Biomedical Applications, Mater. Des., 2012, 39, p 379–38310.1016/j.matdes.2012.03.006 ↗
6. D.W. Zhao, F. Witte, F.Q. Lu, J.L. Wang, J.L. Li, and L. Qin, Current Status on Clinical Applications of Magnesium-Based Orthopaedic Implants: A Review from Clinical Translational Perspective, Biomaterials, 2017, 112, p 287–30210.1016/j.biomaterials.2016.10.017 ↗
7. D. Bose, H. Eggebrecht, M. Haude, A. Schmermund, and R. Erbel, First Absorbable Metal Stent Implantation in Human Coronary Arteries, Am. Heart Hosp. J., 2006, 4, p 128–13010.1111/j.1527-5299.2006.04668.x ↗
8. H.R. Bakhsheshi-Rad, E. Hamzah, H.Y. Tok, M. Kasiri-Asgarani, S. Jabbarzare, and M. Medraj, Microstructure, In Vitro Corrosion Behavior and Cytotoxicity of Biodegradable Mg-Ca-Zn and Mg-Ca-Zn-Bi Alloys, J. Mater. Eng. Perform., 2017, 26, p 653–66610.1007/s11665-016-2499-0 ↗
9. Y.F. Zhang, J.K. Xu, Y.C. Ruan, M.K. Yu, M. O’Laughlin, H. Wise, D. Chen, L. Tian, D.F. Shi, J.L. Wang, S.H. Chen, J.Q. Feng, D.H.K. Chow, X.H. Xie, L.Z. Zheng, L. Huang, S. Huang, K. Leung, N. Lu, L. Zhao, H.F. Li, D.W. Zhao, X. Guo, K. Chan, F. Witte, H.C. Chan, Y.F. Zheng, and L. Qin, Implant-Derived Magnesium Induces Local Neuronal Production of CGRP to Improve Bone-Fracture Healing in Rats, Nat. Med., 2016, 22, p 1160–116910.1038/nm.4162 ↗
10. M. Haude, H. Ince, A. Abizaid, R. Toelg, P.A. Lemos, C. Birgelen, E.H. Christiansen, W. Wijns, F.J. Neumann, C. Kaiser, E. Eeckhout, S.T. Lim, J. Escaned, H.M. Garcia-Garcia, and R. Waksman, Safety and Performance of the Second-Generation Drug-Eluting Absorbable Metal Scaffold in Patients with De-Novo Coronary Artery Lesions (BIOSOLVE-II): 6 Month Results of a Prospective, Multicentre, Non-randomised, First-in-Man Trial, Lancet, 2016, 387, p 31–3910.1016/S0140-6736(15)00447-X ↗
11. J.J. Han, P. Wan, Y. Ge, X.M. Fan, L.L. Tan, J.J. Li, and K. Yang, Tailoring the Degradation and Biological Response of a Magnesium–Strontium Alloy for Potential Bone Substitute Application, Mater. Sci. Eng., C, 2016, 58, p 799–81110.1016/j.msec.2015.09.057 ↗
12. D.W. Zhao, S.B. Huang, F.Q. Lu, B.J. Wang, L. Yang, L. Qin, K. Yang, Y.D. Li, W.R. Li, W. Wang, S.M. Tian, X.Z. Zhang, W.B. Gao, Z.P. Wang, Y. Zhang, X.H. Xie, J.L. Wang, and J.L. Li, Vascularized Bone Grafting Fixed by Biodegradable Magnesium Screw for Treating Osteonecrosis of the Femoral Head, Biomaterials, 2016, 81, p 84–9210.1016/j.biomaterials.2015.11.038 ↗
13. Z.W. Xie, T. Chen, Q. Chen, Q. Yang, S. Tan, Y.J. Wang, Y.M. Luo, Z.Z. Luo, and M.Q. Hua, Tribocorrosion Behaviors of AlN/MoS2-Phenolic Resin Duplex Coatings on Nitrogen Implanted Magnesium Alloys, Surf. Coat. Technol., 2015, 266, p 64–6910.1016/j.surfcoat.2015.02.013 ↗
14. M.P. Sealy, Y.B. Guo, R.C. Caslaru, J. Sharkins, and D. Feldman, Fatigue Performance of Biodegradable Magnesium-Calcium Alloy Processed by Laser Shock Peening for Orthopedic Implants, Int. J. Fatigue, 2016, 82, p 428–43610.1016/j.ijfatigue.2015.08.024 ↗
15. C. Wan, Z.X. Hao, and S.Z. Wen, Research and Prospect on the Fretting Tribology of the Orthopedic Implants, Tribology, 2012, 32, p 102–109
16. L.J. Cao, Y.J. Wu, L.M. Peng, Q.D. Wang, and W.J. Ding, Microstructure and Tribological Behavior of Mg-Gd-Zn-Zr Alloy with LPSO Structure, Trans. Nonferrous Met. Soc. China, 2014, 24, p 3785–379110.1016/S1003-6326(14)63533-0 ↗
17. J. Zhang, X.B. Zhang, Q.H. Liu, S.J. Yang, and Z.Z. Wang, Effects of Load on Dry Sliding Wear Behavior of Mg-Gd-Zn-Zr Alloys, J. Mater. Sci. Technol., 2017, 33, p 645–65110.1016/j.jmst.2016.11.014 ↗
18. X.B. Zhang, Q.L. Ma, Z.X. Ba, Z.Z. Wang, and Q. Wang, Microstructure and Corrosion Behaviour in Simulated Body Fluid of Solution Treated Mg-Nd-Gd-Sr-Zn-Zr Alloys, Rare Met. Mater. Eng., 2017, 46, p 1156–1161
19. X.B. Zhang, Q. Wang, F.B. Chen, Y.J. Wu, Z.Z. Wang, and Q. Wang, Relation Between LPSO Structure and Biocorrosion Behavior of Biodegradable GZ51K Alloy, Mater. Lett., 2015, 138, p 212–21510.1016/j.matlet.2014.09.133 ↗
20. X.B. Zhang, G.Y. Yuan, X.X. Fang, Z.Z. Wang, and T. Zhang, Effects of Solution Treatment on Yield Ratio and Biocorrosion Behaviour of As-Extruded Mg-2.7Nd-0.2Zn-0.4Zr Alloy for Cardiovascular Stent Application, Mater. Technol., 2013, 28, p 155–15810.1179/1753555712Y.0000000048 ↗
21. K. Chen, J.W. Dai, and X.B. Zhang, Improvement of Corrosion Resistance of Magnesium Alloys for Biomedical Applications, Corros. Rev., 2015, 33, p 101–11710.1515/corrrev-2015-0007 ↗
22. X.B. Zhang, Y.J. Wu, Y.J. Xue, Z.Z. Wang, and L. Yang, Biocorrosion Behavior and Cytotoxicity of a Mg-Gd-Zn-Zr Alloy with Long Period Stacking Ordered Structure, Mater. Lett., 2012, 86, p 42–4510.1016/j.matlet.2012.07.030 ↗
23. F. Feyerabend, J. Fischer, J. Holtz, F. Witte, R. Willumeit, H. Drücker, C. Vogt, and N. Hort, Evaluation of Short-Term Effects of Rare Earth and Other Elements Used in Magnesium Alloys on Primary Cells and Cell Lines, Acta Biomater., 2010, 6, p 1834–184210.1016/j.actbio.2009.09.024 ↗
24. S.X. Zhang, X.N. Zhang, C.L. Zhao, J.N. Li, Y. Song, C.Y. Xie, H.R. Tao, Y. Zhang, Y.H. He, Y. Jiang, and Y.J. Bian, Research on an Mg-Zn Alloy as a Degradable Biomaterial, Acta Biomater., 2010, 6, p 626–64010.1016/j.actbio.2009.06.028 ↗
25. X.Y. Ye, M.F. Chen, M. Yang, J. Wei, and D.B. Liu, In Vitro Corrosion Resistance and Cytocompatibility of Nano-Hydroxyapatite Reinforced Mg-Zn-Zr Composites, J. Mater. Sci. Mater. Med., 2010, 21, p 1321–132810.1007/s10856-009-3954-3 ↗
26. X.B. Zhang, Z.X. Ba, Z.Z. Wang, and Y.J. Xue, Microstructures and Corrosion Behavior of Biodegradable Mg-6Gd-xZn-0.4Zr Alloys with and Without Long Period Stacking Ordered Structure, Corros. Sci., 2016, 105, p 68–7710.1016/j.corsci.2016.01.004 ↗
27. X.B. Zhang, Q. Wang, Z.X. Ba, Z.Z. Wang, and Y.J. Xue, Improved Corrosion Resistance of As-Extruded GZ51K Biomagnesium Alloy with High Mechanical Properties by Aging Treatment, J. Mater. Eng. Perform., 2016, 25, p 719–72510.1007/s11665-016-1941-7 ↗
28. W. Rong, Y. Zhang, Y.J. Wu, M. Sun, J. Chen, Y. Wang, J.Y. Han, L.M. Peng, and H.X. Ding, Effects of Zr and Mn Additions on Formation of LPSO Structure and Dynamic Recrystallization Behavior of Mg-15Gd-1Zn Alloy, J. Alloy. Compd., 2017, 692, p 805–81610.1016/j.jallcom.2016.09.068 ↗
29. Y.X. Du, Y.J. Wu, L.M. Peng, J. Chen, X.Q. Zeng, and W.J. Ding, Formation of Lamellar Phase with 18R-type LPSO Structure in an As-Cast Mg96Gd3Zn1 (at%) Alloy, Mater. Lett., 2016, 169, p 168–17110.1016/j.matlet.2015.12.080 ↗
30. K. Gusieva, C.H.J. Davies, J.R. Scully, and N. Birbilis, Corrosion of Magnesium Alloys: The Role of Alloying, Int. Mater. Rev., 2015, 60, p 169–19410.1179/1743280414Y.0000000046 ↗
31. L.G. Bland, N. Birbilis, and J.R. Scully, Exploring the Effects of Intermetallic Particle Size and Spacing on the Corrosion of Mg-Al Alloys Using Model Electrodes, J. Electrochem. Soc., 2016, 163, p C895–C90610.1149/2.1151614jes ↗
32. C.Q. Li, D.K. Xu, Z.R. Zeng, B.J. Wang, L.Y. Wang, X.B. Chen, and E.H. Han, Effect of Volume Fraction of LPSO Phases on Corrosion and Mechanical Properties of Mg-Zn-Y Alloys, Mater. Des., 2017, 121, p 430–44110.1016/j.matdes.2017.02.078 ↗
33. J.J. Han, P. Wan, Y. Sun, Z.Y. Liu, X.M. Fan, L.L. Tan, and K. Yang, Fabrication and Evaluation of a Bioactive Sr-Ca-P Contained Micro-arc Oxidation Coating on Magnesium Strontium Alloy for Bone Repair Application, J. Mater. Sci. Technol., 2016, 32, p 233–24410.1016/j.jmst.2015.11.012 ↗
34. X.B. Zhang, Z.X. Ba, Z.Z. Wang, Y.J. Xue, and Q. Wang, Microstructure and Biocorrosion Behaviors of Solution Treated and As-Extruded Mg-2.2Nd-xSr-0.3Zr Alloys, Trans. Nonferrous Met. Soc. China, 2014, 24, p 3793–3803
35. Z.M. Shi, M. Liu, and A. Atrens, Measurement of the Corrosion Rate of Magnesium Alloys Using Tafel Extrapolation, Corros. Sci., 2010, 52, p 579–58810.1016/j.corsci.2009.10.016 ↗
36. J.S. Zhang, D. Wang, W.B. Zhang, H.X. Pei, Z.Y. You, C.X. Xu, and W.L. Cheng, The relation Between Microstructure and Corrosion Behavior of Mg–Gd–Zn Alloy with Long Period Stacking Ordered Structure, Mater. Corros., 2015, 66, p 542–54810.1002/maco.201407696 ↗
37. X.B. Zhang, Z.X. Ba, Q. Wang, Y.J. Wu, Z.Z. Wang, and Q. Wang, Uniform Corrosion Behavior of GZ51K Alloy with Long Period Stacking Ordered Structure for Biomedical Application, Corros. Sci., 2014, 88, p 1–510.1016/j.corsci.2014.07.004 ↗
38. A. Srinivasan, Y. Huang, C.L. Mendis, C. Blawert, K.U. Kainer, and N. Hort, Investigations on Microstructures, Mechanical and Corrosion Properties of Mg–Gd–Zn Alloys, Mater. Sci. Eng., A, 2014, 595, p 224–23410.1016/j.msea.2013.12.016 ↗
39. D.B. Liu, B. Wu, X. Wang, and M.F. Chen, Corrosion and Wear Behavior of an Mg–2Zn–0.2Mn Alloy in Simulated Body Fluid, Rare Met., 2015, 34, p 553–55910.1007/s12598-013-0052-y ↗
40. H. Li, D.B. Liu, Y. Zhao, F. Jin, and M.F. Chen, The Influence of Zn Content on the Corrosion and Wear Performance of Mg-Zn-Ca Alloy in Simulated Body Fluid, J. Mater. Eng. Perform., 2016, 25, p 3890–389510.1007/s11665-016-2207-0 ↗
41. S.W. Xia, Y. Liu, D.M. Fu, B. Jin, and J. Lu, Effect of Surface Mechanical Attrition Treatment on Tribological Behavior of the AZ31 Alloy, J. Mater. Sci. Technol., 2016, 32, p 1245–125110.1016/j.jmst.2016.05.018 ↗
42. J. An, X.H. Xuan, J. Zhao, W. Sun, and C. Liang, Dry Sliding Wear Behavior and Subsurface Microstructure Evolution of Mg97Zn1Y2 Alloy in a Wide Sliding Speed Range, J. Mater. Eng. Perform., 2016, 25, p 5363–537310.1007/s11665-016-2381-0 ↗