Cr Related Impact Abrasive Wear Mechanism of Low Alloy Wear-Resistant Steel
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Mechanical stress and fatigue analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Z.B. Li, Q. Yuan, S.P. Xu, Y. Zhou, S. Liu, and G. Xu, In situ Observation of the Grain Growth Behavior and Martensitic Transformation of Supercooled Austenite in NM500 Wear-Resistant Steel at Different Quenching Temperatures, Materials, 2023, 16, p 3840. https://doi.org/10.3390/ma1610384010.3390/ma16103840 ↗
2. S.Y. Li, H. Yu, Y. Lu, J. Lu, W.C. Wang, and S.F. Yang, Effects of Titanium Content on the Impact Wear Properties of High-Strength Low-Alloy Steels, Wear, 2021, 474–475, p 203647. https://doi.org/10.1016/j.wear.2021.20364710.1016/j.wear.2021.203647 ↗
3. X.K. Yao, T. Jiang, S.Z. Wei, L.J. Xu, K.M. Pan, H. Yu, C. Chen, C. Zhang, X.D. Wang, and C.J. Wang, Microstructure and Abrasive Wear Performance of a Novel CALPHAD-Inspired Wear-Resistant Steel Containing Multiphase and Multiscale Carbides, Wear, 2024, 538–539, p 205182. https://doi.org/10.1016/j.wear.2023.20518210.1016/j.wear.2023.205182 ↗
4. P.W. Cleary and P. Owen, Development of Models Relating Charge Shape and Power Draw to SAG Mill Operating Parameters and Their Use in Devising Mill Operating Strategies to Account for Liner Wear, Miner. Eng., 2018, 117, p 42–62. https://doi.org/10.1016/j.mineng.2017.12.00710.1016/j.mineng.2017.12.007 ↗
5. R. Kumar, R.K. Dwivedi, and S. Ahmed, Stability of Retained Austenite in Carbide Free Bainite during the Austempering Temperature and its Influence on Sliding Wear of High Silicon Steel, SILICON, 2020, 13, p 1249–1259. https://doi.org/10.1007/s12633-020-00513-210.1007/s12633-020-00513-2 ↗
6. J.H. Wu, M. Liu, L.Y. Sun, Y.L. Li, F.Q. Dai, and G. Xu, Sliding Wear Behaviors of Low Alloy High Strength Martensite Wear-Resistant Steels, Wear, 2024, 558–559, p 205573. https://doi.org/10.1016/j.wear.2024.20557310.1016/j.wear.2024.205573 ↗
7. C. Chen, F.C. Zhang, F. Wang, H. Liu, and B.D. Yu, Effect of N+Cr Alloying on the Microstructures and Tensile Properties of Hadfield Steel, Mater. Sci. Eng., 2017, 679, p 95–103. https://doi.org/10.1016/j.msea.2016.09.10610.1016/j.msea.2016.09.106 ↗
8. X. Xu, S. van der Zwaag, and W. Xu, The Scratch and Abrasive Wear Behaviour of a Tempered Martensitic Construction Steel and its Dual Phase Variants, Wear, 2016, 358–359, p 80–88. https://doi.org/10.1016/j.wear.2016.04.00510.1016/j.wear.2016.04.005 ↗
9. D.V. Edmonds, K. He, F.C. Rizzo, B.C. De Cooman, D.K. Matlock, and J.G. Speer, Quenching and Partitioning Martensite—A Novel Steel Heat Treatment, Mater. Sci. Eng., 2006, 438–440, p 25–34. https://doi.org/10.1016/j.msea.2006.02.13310.1016/j.msea.2006.02.133 ↗
10. H. Fu, Q. Xiao, and H. Fu, Heat Treatment of Multi-Element Low Alloy Wear-Resistant Steel, Mater. Sci. Eng., 2005, 396, p 206–212. https://doi.org/10.1016/j.msea.2005.01.02310.1016/j.msea.2005.01.023 ↗
11. A. Leiro, E. Vuorinen, K.G. Sundin, B. Prakash, T. Sourmail, V. Smanio, F.G. Caballero, C. Garcia-Mateo, and R. Elvira, Wear of Nano-Structured Carbide-Free Bainitic Steels under Dry Rolling–Sliding Conditions, Wear, 2013, 298–299, p 42–47. https://doi.org/10.1016/j.wear.2012.11.06410.1016/j.wear.2012.11.064 ↗
12. X.H. Liu, L. Xiao, C.H. Wei, X.X. Xu, M.H. Luo, and W.L. Yan, Effect of Multi-Directional Forging and Annealing on Abrasive Wear Behavior in a Medium Carbon Low Alloy Steel, Tribol. Int., 2018, 119, p 608–613. https://doi.org/10.1016/j.triboint.2017.11.04310.1016/j.triboint.2017.11.043 ↗
13. C.Y. Wang, X.D. Li, Y. Chang, S. Han, and H. Dong, Comparison of Three-Body Impact Abrasive Wear Behaviors for Quenching–Partitioning–Tempering and Quenching–Tempering 20Si2Ni3 Steels, Wear, 2016, 362–363, p 121–128. https://doi.org/10.1016/j.wear.2016.05.02610.1016/j.wear.2016.05.026 ↗
14. R. Dalai, S. Das, and K. Das, Effect of Thermo-Mechanical Processing on the Low Impact Abrasion and Low Stress Sliding Wear Resistance of Austenitic High Manganese Steels, Wear, 2019, 420–421, p 176–183. https://doi.org/10.1016/j.wear.2018.10.01310.1016/j.wear.2018.10.013 ↗
15. E. Zdravecká, J. Tkáčová, and M. Ondáč, Effect of Microstructure Factors on Abrasion Resistance of High-Strength Steels, Res. Agric. Eng., 2014, 60, p 115–120. https://doi.org/10.17221/20/2013-rae10.17221/20/2013-rae ↗
16. C.Y. Zhang, Z.R. Li, Y.Y. Li, X.M. Zhou, D. Fang, Y.S. Ye, Y.L. Yuan, and H.H. Wu, Study on Mechanical Properties and Microstructure of the Ultrastrong Low Alloy Wear‐Resistant Steel, Steel Res. Int., 2020, 1, p 92. https://doi.org/10.1002/srin.20200015510.1002/srin.202000155 ↗
17. T. Xia, Y.X. Ma, Y.S. Zhang, J.L. Li, and H. Xu, Effect of Mo and Cr on the Microstructure and Properties of Low-Alloy Wear-Resistant Steels, Materials, 2024, 17, p 2408. https://doi.org/10.3390/ma1710240810.3390/ma17102408 ↗
18. C. Su, G.H. Feng, J.G. Zhi, B. Zhao, and W. Wu, The Effect of Rare Earth Cerium on Microstructure and Properties of Low Alloy Wear-Resistant Steel, Metals, 2022, 12, p 1358. https://doi.org/10.3390/met1208135810.3390/met12081358 ↗
19. T.S. Cao, C.Q. Cheng, F. Ye, H.B. Xu, and J. Zhao, Relationship between Carbon Segregation and the Carbide Precipitation along Grain Boundary Based on the Structural Unit Model, J. Mater. Sci., 2020, 55, p 7883–7893. https://doi.org/10.1007/s10853-020-04537-210.1007/s10853-020-04537-2 ↗
20. S.-G. Park, M.-C. Kim, B.-S. Lee, and D.-M. Wee, Correlation of the Thermodynamic Calculation and the Experimental Observation of Ni-Mo-Cr Low Alloy Steel Changing Ni, Mo, and Cr Contents, J. Nucl. Mater., 2010, 407, p 126–135. https://doi.org/10.1016/j.jnucmat.2010.09.00410.1016/j.jnucmat.2010.09.004 ↗
21. T. Hu, R.M. Wu, F.J. Li, N. Na, and W. Li, Effect of Mo-Related Precipitation Behavior on the Strengthening and Thermal Stability of 4Cr5Mo2V Die Steel, J. Mater. Eng. Perform., 2022, 31, p 10213–10224. https://doi.org/10.1007/s11665-022-07029-310.1007/s11665-022-07029-3 ↗
22. Z.S. Yao, G. Xu, Z.Y. Jiang, J.Y. Tian, Q. Yuan, and H.W. Ma, Effects of Ni and Cr on Cryogenic Impact Toughness of Bainite/Martensite Multiphase Steels, Met. Mater. Int., 2019, 25, p 1151–1160. https://doi.org/10.1007/s12540-019-00262-x10.1007/s12540-019-00262-x ↗
23. J. Trzaska, Calculation of Critical Temperatures by Empirical Formulae, Arch. Metall. Mater., 2016, 61, p 981–986. https://doi.org/10.1515/amm-2016-016710.1515/amm-2016-0167 ↗
24. X.D. Wang, Y.B. Chen, S.Z. Wei, L.L. Zuo, and F. Mao, Effect of Carbon Content on Abrasive Impact Wear Behavior of Cr-Si-Mn Low Alloy Wear Resistant Cast Steels, Front. Mater., 2019 https://doi.org/10.3389/fmats.2019.0015310.3389/fmats.2019.00153 ↗
25. L. Li and J. Tang, Synthesis of Cr7C3 and Cr3C2 by Mechanical Alloying, J. Alloys Compd., 1994, 209, p L1–L3. https://doi.org/10.1016/0925-8388(94)91060-x10.1016/0925-8388(94)91060-x ↗
26. W.M. Liu, T. Jiang, S.Z. Wei, L.J. Xu, C. Chen, H. Yu, X. Jin, H.L. Ding, C. Zhang, and K.M. Pan, A Comparative Analysis of Abrasive Wear Behaviors and Mechanisms of Pearlitic and Carbide-Free Bainitic Steels for Grinding Mill Liners under Varied Impact Loads, Wear, 2025, 566–567, p 205765. https://doi.org/10.1016/j.wear.2025.20576510.1016/j.wear.2025.205765 ↗
27. D. Music, U. Kreissig, R. Mertens, and J.M. Schneider, Electronic Structure and Mechanical Properties of Cr7C3, Phys. Lett., 2004, 326, p 473–476. https://doi.org/10.1016/j.physleta.2004.04.06810.1016/j.physleta.2004.04.068 ↗
28. B. Xiao, J.D. Xing, J. Feng, Y.F. Li, C.T. Zhou, W. Su, X.J. Xie, and Y.H. Chen, Theoretical Study on the Stability and Mechanical Property of Cr7C3, Physica Condens. Matter., 2008, 403, p 2273–2281. https://doi.org/10.1016/j.physb.2007.12.01210.1016/j.physb.2007.12.012 ↗
29. J. Zhou, D.S. Ma, H.X. Chi, Z.Z. Chen, and X.Y. Li, Microstructure and Properties of Hot Working Die Steel H13MOD, J. Iron. Steel Res. Int., 2013, 20, p 117–125. https://doi.org/10.1016/S1006-706X(13)60166-110.1016/S1006-706X(13)60166-1 ↗
30. W.H. Ding, Y.Z. Liu, J.X. Xie, L. Sun, T.W. Liu, F. Yuan, and J. Pan, Effect of Carbide Precipitation on the Evolution of Residual Stress during Tempering, Metals, 2019, 9, p 709. https://doi.org/10.3390/met906070910.3390/met9060709 ↗
31. K. Wieczerzak, P. Bala, R. Dziurka, T. Tokarski, G. Cios, T. Koziel, and L. Gondek, The Effect of Temperature on the Evolution of Eutectic Carbides and M 7 C 3 → M 23 C 6 Carbides Reaction in the Rapidly Solidified Fe-Cr-C alloy, J. Alloys Compd., 2017, 698, p 673–684. https://doi.org/10.1016/j.jallcom.2016.12.25210.1016/j.jallcom.2016.12.252 ↗
32. X.Y. Shen, M.L. Peng, H. Fu, T.T. Wei, H. Wu, X. Huang, Z.L. Li, L. Li, I. Baker, and Q. Shan, Enhanced Wear Resistance of a Die Steel via Modification of the M7C3 and M23C6 Carbides, Wear, 2025, 576–577, p 206106. https://doi.org/10.1016/j.wear.2025.20610610.1016/j.wear.2025.206106 ↗
33. H.F. Li, Q.Q. Duan, P. Zhang, X.H. Zhou, B. Wang, and Z.F. Zhang, The Quantitative Relationship between Fracture Toughness and Impact Toughness in High-Strength Steels, Eng. Fract. Mech., 2019, 211, p 362–370. https://doi.org/10.1016/j.engfracmech.2019.03.00310.1016/j.engfracmech.2019.03.003 ↗
34. W.M. da Silva, H.L. Costa, and J.D.B. de Mello, Transitions in Abrasive Wear Mechanisms: Effect of the Superimposition of Interactions, Wear, 2011, 271, p 977–986. https://doi.org/10.1016/j.wear.2011.04.01010.1016/j.wear.2011.04.010 ↗
35. K. Wang, F. Hu, S.B. Zhou, W. Zhou, Z.C. Zhang, S. Yershov, and K.M. Wu, Effect of Microstructure Transformation Below MS Temperature in Bainitic Steels on the Impact-Abrasive Wear Behavior, Wear, 2023, 514–515, p 204589. https://doi.org/10.1016/j.wear.2022.20458910.1016/j.wear.2022.204589 ↗
36. A. Fischer, Mechanisms of High Temperature Sliding Abrasion of Metallic Materials, Wear, 1992, 152, p 151–159. https://doi.org/10.1016/0043-1648(92)90210-y10.1016/0043-1648(92)90210-y ↗
37. I. El-Mahallawi, R. Abdel-karim, and A. Naguib, Evaluation of Effect of Chromium on Wear Performance of High Manganese Steel, Mater. Sci. Technol., 2001, 17, p 1385–1390. https://doi.org/10.1179/02670830110150934010.1179/026708301101509340 ↗
38. W.Q. Leng, L.J. Xu, T. Jiang, X.D. Wang, S.Z. Wei, X.W. Shi, and M. Li, Carbide and Matrix Microstructure Evolution of High-Vanadium Wear-Resistance Cast Iron with High-Silicon Content during Austempering, Int. J. Met., 2022, 17, p 1859–1870. https://doi.org/10.1007/s40962-022-00886-710.1007/s40962-022-00886-7 ↗
39. N.Y. Du, H.H. Liu, Y.F. Cao, P.X. Fu, C. Sun, H.W. Liu, and D.Z. Li, In situ Investigation of the Fracture of Primary Carbides and its Mechanism in M50 Steel, Mater Charact, 2022, 186, p 111822. https://doi.org/10.1016/j.matchar.2022.11182210.1016/j.matchar.2022.111822 ↗
40. S.D. Bakshi, P.H. Shipway, and H.K.D.H. Bhadeshia, Three-Body Abrasive Wear of Fine Pearlite, Nanostructured Bainite and Martensite, Wear, 2013, 308, p 46–53. https://doi.org/10.1016/j.wear.2013.09.00810.1016/j.wear.2013.09.008 ↗
41. P.H. Shipway, S.J. Wood, and A.H. Dent, The Hardness and Sliding Wear Behaviour of a Bainitic Steel, Wear, 1997, 203–204, p 196–205. https://doi.org/10.1016/s0043-1648(96)07411-x10.1016/s0043-1648(96)07411-x ↗
42. S. Hernandez, A. Leiro, M.R. Ripoll, E. Vuorinen, K.-G. Sundin, and B. Prakash, High Temperature Three-Body Abrasive Wear of 0.25C 1.42Si Steel with Carbide Free Bainitic (CFB) and Martensitic Microstructures, Wear, 2016, 360–361, p 21–28. https://doi.org/10.1016/j.wear.2016.04.01210.1016/j.wear.2016.04.012 ↗
43. A.S. Rajput and S. Das, Abrasive Wear Behaviour of Continuously Cooled Carbide-Free Bainitic Steel, Wear, 2025, 570, p 205951. https://doi.org/10.1016/j.wear.2025.20595110.1016/j.wear.2025.205951 ↗
44. K. Cao, Z.G. Wang, P.F. Liu, and A.M. Zhao, Effect of Austenitizing Temperature and Cooling Rate on Ms Temperature of Fe-Ni-Cr cast iron, J. Mater. Res. Technol., 2023, 26, p 796–806. https://doi.org/10.1016/j.jmrt.2023.07.20810.1016/j.jmrt.2023.07.208 ↗
45. Y. Wang and Z. Wang, Analysis and Calculation of Three-Body Abrasive Wear, J. Shanghai Jiaotong Univ., 1986, 20, p 40–51. https://doi.org/10.16183/j.cnki.jsjtu.1986.03.00510.16183/j.cnki.jsjtu.1986.03.005 ↗