journal article·2026-06Open access

Kinetics of the Dissolution of Tungsten Carbides Induced by Advanced GMAW Hardfacing Processes to Produce MMC Coatings

Wilhelm Gerald

Abstract

Abstract GMAW hardfacing with consumables containing tungsten carbides is limited by the dissolution of the carbide particles in the droplet and subsequently in the weld pool. This study investigates the dissolution behavior of unmodified, commercially used eutectoid WC/W 2 C carbides (WSC) and carburized variants (cWSC) featuring a stabilizing WC surface layer under an energy-reduced, controlled short-circuit GMAW hardfacing process. Thermal exposure is considered as two consecutive stages involving dissolution in the molten droplet and diffusion-dominated dissolution during weld-pool residence. Transient electrical process data and weld-pool surface temperature measurements are used to determine the specific droplet enthalpy and the relevant temperature–time regimes. An analytical model based on the shrinking-core concept is developed to quantify carbide dissolution as a function of particle size and cooling time and is validated experimentally by statistical particle-size analysis and particle-counting methods. The results reveal a pronounced size dependence of dissolution, with particles smaller than approximately 80 µm undergoing extensive degradation largely independent of heat input. Carburized carbides exhibit significantly reduced dissolution compared to conventional eutectoid carbides, retaining an intact WC surface layer throughout processing. Furthermore, dissolution is markedly enhanced in iron-based melts compared to iron-nickel systems, indicating that Fe-Ni matrices in combination with carburized carbides are preferable for minimizing carbide degradation in GMAW hardfacing applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Welding Techniques and Residual Stresses · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. A. Petsch, Tribosystemangepasste Verschleißuntersuchungen von Wolframschmelzkarbidhaltigen Pseudolegierungen für den Einsatz im Bergbau (Tribosystem-Specific Wear Investigations of Tungsten Fused Carbide-Containing Pseudoalloys for Mining Applications), AMS ONLINE Adv. Min. Solut., 2010, 04, p 32–41. ((in German))
2. K. Richter and J. Wiedemeier, Abrasion-Erosion: Volkswirtschaftliche Bedeutung, Kosten und Aspekte zur Kostensenkung (Abrasion-Erosion: Economic Impact, Costs, and Aspects of Cost Reduction), Expert Verlag, Renningen, 1989.
3. W. Theisen, Metal Matrix Composites widerstehen dem Verschleiß: Walzen aus Pulver (Metal Matrix Composites resist wear: Rolls made from powder), Rubin Sonderheft, Bd. (2004), p. 90–95, Ruhr-Universität Bochum (in German)
4. N.N., Department of Education and Science, Lubrication (Tribology), Education and Research: A Report on Present Position and Industry Needs, Her Majesty’s Stationery Office (London, 1966) (in English)
5. N.N., Tribologie (Tribology), Forschungsbericht BMFT: FB—T 76–38, Bundesministerium für Forschung und Technologie (München, 1976) (in German)
6. N.N., Damit Rost und Verschleiß Nicht Milliarden Fressen (Avoiding Billions Lost Due to Rust and Wear), Der Bundesminister für Forschung und Technologie, Öffentlichkeitsarbeit, BMFT-Report Fortschritt durch Forschung (Bonn, 1984) (in German)
7. N.N.: Statistisches Bundesamt (2008)
8. N.N., Reibungsverluste ab der Ersten Begegnung: Das Material Verzeiht Nichts (Friction Losses from the Very First Contact: The Material Shows no Mercy), Karlsruher Institut für Technologie, Presseinformation 096/2018, https://www.kit.edu/kit/pi_2018_096_reibungsverluste-ab-der-ersten-begegnung-das-material-verzeiht-nichts Accessed 16 July 2025
9. N.N., Damit Rost und Verschleiß nicht Milliarden Fressen (Avoiding Billions Lost Due to Rust and Wear), Der Bundesminister für Forschung und Technologie, Öffentlichkeitsarbeit, BMFT-Report Fortschritt durch Forschung, (Bonn, 1983) (in German)
10. H. Czichos and K.-H. Habig, Tribologie–Handbuch: Tribometrie, Tribo-materialien. Tribotechnik (Tribology Handbook—Tribometry, Tribo-Materials. Tribotechnology), 3. Aufl. Vieweg + Teubner, Wiesbaden, 2010.10.1007/978-3-8348-9660-5 ↗
11. J.R. Davis, Surface Engineering for Corrosion and Wear Resistance, ASM International, Materials Park, 2001.10.31399/asm.tb.secwr.9781627083157 ↗
12. B. Nedeljkovic, V. Lazic, S. Aleksandrovic, Influence of the Carbide Type on Tribological Properties of the Hard Faced Layers, Metallurgical & Materials Engineering, vol. 16, no. 2, p. 77–90, Association of Metallurgical Engineers of Serbia (2010)
13. T.S. Eyre, Wear Characteristics of Metals, Tribol. Int., 1976 https://doi.org/10.1016/0301-679X(76)90077-310.1016/0301-679X(76)90077-3 ↗
14. K. Röhrig, Abrasionsbeständige Eisengußwerkstoffe (Abrasion-resistant cast iron materials), VDI-Z, Bd. 124, 1982, Nr. 5, p. 11–24
15. O. Penning, Auftragschweißen von Schienenköpfen im DB-Gleissystem mit selbstschützenden Fülldrahtelektroden (Hardfacing of Rail Heads in the DB Track System Using Self-Shielded Flux-Cored Wire Electrodes), 6. Fachtagung Verschleißschutz von Bauteilen Durch Auftragschweißen (Halle (Saale), 2008) (in German)
16. EN 14700: 2006, Welding Consumables: Covered Electrodes for Manual Metal Arc Welding of Stainless and Heat-Resisting Steels, Beuth Verlag (Berlin, 2006)
17. Durum Verschleißschutz GmbH, Wolframschmelz-karbidhaltige WSC-Produkte. DURMAT Verschleißschutz, https://durmat.com/de/produkte/wolframschmelz-karbidhaltige-wsc-produkte/Accessed 16 July (2025)
18. V. Wesling, Einfluss der Hartphasenmorphologie auf das Verschleißverhalten von Eisenbasishartlegierungen (Impact of Hard Phase Morphology on the Wear Behavior of Iron-Based Hardfacing Alloys), 32. Assistentenseminar Schweiß- und Fügetechnik, DVS-Berichte 2012, vol. 284, p. 41–48, Verlag für Schweißen und verwandte Verfahren DVS-Verlag GmbH (Düsseldorf, 2012) (in German)
19. V. Wesling, Einsatz von Fülldrahtelektroden in Kombination mit Geregelten Kurzlichtbogenprozessen zur Herstellung von Panzerungen zum Schutz vor abrasiven Beanspruchungen (Use of Flux-Cored Wire Electrodes in Combination with Controlled Short Arc Welding Processes for Producing Armouring Against Abrasive Wear), Schweißen und Schneiden–DVS-Berichte, 2012, 286, p 244–248. ((in German))
20. M. Hecht, Qualifizierung und Technisch-Wirtschaftliche Bewertung von Hochleistungsverschleißschutzsystemen zum Einsatz Unter Feinabrasiv-Erosiver Beanspruchung (Qualification and Techno-Economic Evaluation of High-Performance Wear Protection Systems for Use Under Fine-Abrasive and Erosive Conditions), Dissertation, TU (Clausthal, 2018) (in German)
21. H. Okamoto, C–W (Carbon–Tungsten), J. Phase Equilib. Diffus., 2008, 29(6), p 543–544.10.1007/s11669-008-9396-7 ↗
22. B. Wielage, A. Wank, J. Wilden, Herstellung von Verbundwerkstoffen bzw. Werkstoffverbunden Durch Thermische Beschichtungsverfahren. Metallische Verbundwerkstoffe, WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim, S. 124–159 (2003)10.1002/3527602062.ch5 ↗
23. V. Wesling, R. Reiter, L. Lau, C. Gerk, M. Hengerer, Einsatz und Nutzen Eines Randzonenaufgekohlten Wolframschmelzkarbids zum Verschleißschutz. In: Schweißen und Schneiden: DVS-Berichte 304, Düsseldorf, DVS-Media, S. 315–321 (2014)
24. D. Fister, R. Mainzinger, Verfahren zur Herstellung von Wolfram-Schmelzkarbid und Dessen Verwendung (Method for Producing Tungsten Fused Carbide and Its Use), Patent DE 3626031A1, Germany, filed August 1 (1986) (in German).
25. R. Kiefer and F. Benesovsky, Hartstoffe (Hard Materials), Springer Verlag, Vienna, 1963. ((in German))10.1007/978-3-7091-7151-6 ↗
26. R. Hähn, E. Lüderitz, H.-J. Retelsdorf, S. Sattelberger, Verfahren zur Herstellung von Wolframschmelzkarbid (Method for Producing Tungsten Fused Carbide), Patent DE 3608693 C2, Germany, filed March 15 (1986) (in German)
27. E. Findeisen, K. Frank, W. Becker, F. Müller, Verfahren zur Herstellung von Wolfram-Schmelzcarbid-Kugeln (Method for Producing Tungsten Fused Carbide Spheres), Patent DE 3835124 A1, Germany, filed October 15 (1988) (in German)
28. K.P. Wieters, W. Schatt, Pulvermetallurgie, Technologien und Werkstoffe (Powder Metallurgy, Technologies and Materials) (Springer, Berlin, Heidelberg, New York, 2007) (in German)
29. P. Brunet, F. Esnault, G. Maybon, R. Pierrer de la Bathie, Verfahren und Vorrichtung zur Herstellung hitzebeständiger Materialien Durch Induktion (Method and Device for Producing Heat-Resistant Materials by Induction), Patent AT 66171 E (translation document), Europe, filed March 10 (1987) (in German)
30. B. Predel, Heterogene Gleichgewichte (Heterogeneous Equilibria), Steinkopff-Verlag, Darmstadt, 1992. ((in German))
31. A. Hübner, Untersuchung des Einflusses der Morphologie der Eigenschaften von Verschleißschichten am Beispiel des Plasmapulver-auftragschweißens (Study of Morphology-Related Effects on the Properties of Wear-Resistant Coatings Exemplified by Plasma Powder Welding). Abschlussbericht, Forschungsvorhaben AiF-Nr.: 15.232B, September (2009) (in German)
32. F. Schreiber, Wolframschmelzkarbid im Verschleißschutz: Besonderheiten bei der schweißtechnischen Verarbeitung und Qualitätssicherung (Tungsten Eutectoid Carbide in Wear Protection: Specific Aspects of Welding Processing and Quality Assurance), 3rd Conference on Wear Protection of Components by Hardfacing, Halle (Saale), 2000, p 20–27 (in German)
33. C. Just, E. Badisch, and J. Wosik, Influence of Welding Current on Carbide/Matrix Interface Properties in MMCs, J. Mater. Process. Technol., 2010, 210, p 408–414.10.1016/j.jmatprotec.2009.10.001 ↗
34. I. Barin, Thermochemical Data of Pure Substances, Vol Vols. 1 & 2, 3rd ed., VCH, Weinheim, 1995.10.1002/9783527619825 ↗
35. J. Luthin, Untersuchungen zur Chemischen Wechselwirkung bei der Bildung von Kohlenstoff-Mischsystemen (Investigations on the Chemical Interaction in the Formation of Carbon Mixed Systems), Dissertation, Universität Bayreuth (2001) (in German)
36. L. Zulai, Y.E. Yehua, Y.E. Xiaomei, and R. Zhou, Dissolution of Tungsten Carbide Particulates (WC) in the Matrix of Reinforced Grey Cast Iron Matrix Composite, Acta Mater. Compos. Sin., 2007, 24(2), p 13–17.
37. Q. Shan, L. Zulai, J. Yehua, Z. Rong, and S. Yudong, Decomposition of Two Phases WC and W2C in Casting Tungsten Carbide Particles in Steel/Iron Substrate, Appl. Mech. Mater., 2011, 109, p 120–124.10.4028/www.scientific.net/AMM.109.120 ↗
38. S.T. Oyama, The Chemistry of Transition Metal Carbides and Nitrides, Springer, Netherlands, 2012.
39. L. Choi, M. Wolfe, M. Yarmurch, A. Gerlich, Effect of Welding Parameters on Tungsten Carbide Metal-Matrix Composites Produced by GMAW, Proceedings of Canadian Welding Association Conference (Alberta, Canada, 2011)
40. Z. Izdinska, A. Nasher, and K. Izdinsky, The Structure and Properties of Composite Laser Clad Coatings with Ni-Based Matrix with WC Particles, Mater. Eng., 2010, 17, p 1–5.
41. L. Lau, Einsatz Eines Randzonenaufgekohlten Wolframschmelzkarbids zum Schweißtechnischen Panzern Hochverschleißbeanspruchter Oberflächen (Use of a Surface Zone Carburized Tungsten Carbide for Welding Protection of Highly Wear-Exposed Surfaces), Dissertation, TU Clausthal (2015) (in German)
42. K. Günther, Werkstofftechnische Betrachtungen zum Heißdraht Unterstützten MSG-Auftragschweißen Hartstoffverstärkter Verschleißschutzlegierungen (Materials Engineering Considerations on Hot-Wire-Assisted GMAW Hardfacing of Wear-Resistant Alloys Reinforced with Hard Phases), Dissertation, TU Ilmenau (2018) (in German)
43. K. Günther, J.P. Bergmann, Understanding the Dissolution Mechanism of Fused Tungsten Carbides in Ni-Based Alloys: An Experimental Approach, Materials Letters, p. 253–256 (2013)10.1016/j.matlet.2017.11.088 ↗
44. A. Luft, A. Techel, S. Nowotny, and W. Reizenstein, Gefügebildung und Karbidauflösung Beim Laserbeschichten von Stahl mit Wolframkarbidverstärkten Ni- und Co-Hartlegierungen (Microstructure Formation and Carbide Dissolution in Laser Cladding of Steel with Tungsten Carbide Reinforced Ni- and Co-Based Hardfacing Alloys), Prakt. Metallogr., 1995, 32(5), p 235–247. ((in German))10.1515/pm-1995-320503 ↗
45. W. Theisen, R. Winkelmann, A. Pelz, B. Reichmann, Auftragschweißen mit Wolframkarbid in Fe-Basis-Legierungen (Hardfacing with Tungsten Carbide in Fe-Based Alloys), 7. Fachtagung Verschleißschutz von Bauteilen Durch Auftragschweißen, Halle (Saale), p. 65–70 (2008) (in German)
46. W. Theisen and A. Packeisen, Abrasionsverhalten hartstoffhaltiger Fe-Basis-Werkstoffe (Abrasive Wear Behavior of Hard-Particle Reinforced Fe-Based Materials), Materialwiss. Werkst., 2004, 35(10/11), p 736–740. ((in German))10.1002/mawe.200400829 ↗
47. U. Draugelates, B. Bouaifi, and B. Ouissa, Einfluss der Carbidauflösung auf die Eigenschaften hartstoffverstärkter Schutzschichten (Impact of Carbide Dissolution on the Properties of Hard-Particle Reinforced Protective Coatings), Schweis. Schneid., 2000, 1(52), p 12–17. ((in German))
48. A. Müller, A. Uleze, A. Techel, A. Luft, and S. Nowotny, Verschleißverhalten von Wolframcarbidverstärkten Laserauftragschweißungen (Wear Behavior of Tungsten Carbide Reinforced Laser Claddings), Schweis. Schneid., 1995, 47(4), p 260–267. ((in German))
49. L. Lau, Einsatz Eines Randzonenaufgekohlten Wolframschmelzkarbids zum Schweißtechnischen Panzern Hochverschleißbeanspruchter Oberflächen (Use of Carburized Tungsten Steel Carbide for Hardfacing of Heavily Wear-Loaded Surfaces by Welding), TU Clausthal, Dissertation (2015) (in German)
50. B. Bouaifi, Eigenschaftsvorhersage Hartstoffverstärkter Schutzschichten Durch Werkstoff- und Prozessbezogene Modellierung der Karbidauflösungskinetik (Property Prediction of Hard-Particle Reinforced Protective Coatings by Material- and Process-Related Modeling of Carbide Dissolution Kinetics), Habilitationsschrift, TU Clausthal (2001) (in German)
51. B. Bechtloff, Gezielte Beeinflussung der Kinetik von Fest-Flüssig-Reaktionskristallisationen, (Deliberate Influence on the Kinetics of Solid–Liquid Reaction Crystallization), Dissertation, Martin-Luther-Universität Halle-Wittenberg (2002) (in German)
52. E. Brunner, Reaktionsgeschwindigkeit in Heterogenen Systemen, (Reaction kinetics in heterogeneous systems), Z. f. Phys.Chem., 1904, 47, p 56–101. ((in German))10.1515/zpch-1904-4705 ↗
53. W. Nernst, Theorie der Reaktionsgeschwindigkeit in heterogenen Systemen, (Theory of reaction kinetics in heterogeneous systems), Z. f. Phys.Chem. Ausg., 1904, 47, p 53–55. ((in German))
54. M. Hördler, Phasengrenzreaktionen im Fest-Flüssig-System Nickel/Zinn (Phase Boundary Reactions in the Solid–Liquid System Nickel/Tin), Dissertation, Universität Erlangen-Nürnberg (2006) (in German)
55. R. Romankov, Frolov, Stoffübertragungsprozesse der Chemischen Technologie (Systeme Mit Einer Festen Phase), (Mass Transfer Processes in Chemical Technology (Systems Involving a Solid Phase), Akademie-Verlag, Berlin, 1979. ((in German))
56. A. Böbe, Zum Einfluss der Morphologie der Wolframcarbide auf die Verschleißbeständigkeit von Plasmapulverauftragschweißungen, (On the Influence of Tungsten Carbide Morphology on the Wear Resistance of Plasma Transferred Arc Coatings), Dissertation, Otto von Guericke Universität (2011) (in German)
57. M. Hermans, Study of Short Circuiting Arc Welding, Dissertation. TU Delft (1997)
58. N.N. Rykalin, Berechnung der Wärmevorgänge beim Schweißen, (Computational Analysis of Thermal Phenomena in Welding), VEB Verlag Technik, Berlin, 1957. ((in German))
59. F. W. Morich, Beitrag zur Wärmeführung beim Schweißen mit Mechanischen Lichtbogenverfahren (Contribution to the Thermal Regime in Welding with Mechanical Arc Processes), Dissertation RWTH Aachen (1969) (in german)
60. W.W. Mullens, Theory of Thermal Grooving, J. Appl. Phys., 1957, 28(3), p 333–339.10.1063/1.1722742 ↗
61. W.M. Robertson, Grain-Boundary Grooving by Surface Diffusion for Finite Surface Slopes, J. Appl. Phys., 1971, 42(1), p 463–467.10.1063/1.1659625 ↗
62. S. Lu, H. Fujii, H. Sugiyama, Effects of the Oxygen Additions to Argon Shielding Gas on GTA Weld Shape, ISIJ International, vol. 43, no. 10, p. 1590–1595, Iron and Steel Institute of Japan (2003)10.2355/isijinternational.43.1590 ↗
63. S. Lu, H. Fujii, H. Sugiyama, K. Nogi, Marangoni Convection and Weld Shape Variations in Ar–O2 and Ar–CO2 Shielding Gas. Mater. Sci. Eng. A, vol. 380, p 290–297, Elsevier (2004)10.1016/j.msea.2004.05.057 ↗
64. S. N. Basu, V. K. Sarin, Oxidation Behavior of WC–Co. Mater. Sci. Eng. A, vol. 209, no. 1–2, p. 206–212, Elsevier (1996)10.1016/0921-5093(95)10145-4 ↗
65. B. Wang, H. Wang, F. Wang, Effect of (Ti, W) C/TaC Addition on the Early Oxidation Behavior of Cemented Carbides. Corros. Sci. vol. 174, art. 108857, Elsevier, (2020)10.1016/j.corsci.2020.108857 ↗
66. N. Eustathopoulos, Wetting by Liquid Metals: Application in Materials Processing: The Contribution of the Grenoble Group, Metals, vol. 5, no. 1, p. 350–370, MDPI (2015)10.3390/met5010350 ↗
67. W. Li, F. Zhang, W. He, et al., Sonoprocessing of Wetting of SiC by liquid Al. Ultrason. Sonochem. vol. 86, art. 106005, Elsevier (2022)
68. R. M. German, P. S. Suri, S. J. Park, Review: Liquid Phase Sintering. J. Mater. Sci. vol. 44, p. 1–39, Springer (2009)10.1007/s10853-008-3008-0 ↗
69. D.M. Jacobson, Principles of Brazing, ASM International, 2005, p 1–26810.31399/asm.tb.pb.9781627083515 ↗
70. E. Bormashenko and Elsevier, Apparent Contact Angles for Reactive Wetting of Smooth, Rough and Heterogeneous Surfaces, J. Colloid Interface Sci., 2019, 555, p 629–634.10.1016/j.jcis.2019.08.021 ↗
71. N. Popov, A. Suchkov, M. Zharkov, V. Kirillova, A. Bazhenov, I. Fedotov, I. Bajenova, A. Khvan, I. Kozlov, A. Vertkov, O. Sevryukov, and Pensoft, Interaction of Iron Melt with Tungsten and WFe Composite: Wetting and Joint Structure, Nucl. Energy Technol., 2024, 10(3), p 189–198.10.3897/nucet.10.129596 ↗
72. S. Kuthe, M. Boström, W. Chen, B. Glaser, C. Persson, and American Chemical Society, Exploring Wettability of Liquid Iron on Refractory Oxides with the Sessile Drop Technique and Density Functional-Derived Hamaker Constants, ACS Appl. Mater. Interfaces, 2025, 17(10), p 16173–16186.10.1021/acsami.4c21877 ↗
73. V.S. Panov, M.A. Goldberg, and Springer, Interaction of Tungsten Carbide with Aluminum Nickelide Ni3Al, Powder Metall. Met. Ceram., 2009, 48, p 445–448.10.1007/s11106-009-9146-3 ↗
74. N. Sievers, Die Elektrische Widerstandsmessung zur Zerstörungsfreien Prüfung von Lötnähten am Beispiel von Hartmetall–Stahl-Verbunden, Diss., p. 1–216, TU Dortmund/Vulkan-Verlag (2017)
75. T. Iida, R. I. L. Guthrie, The Physical Properties of Liquid Metals, 2nd ed., Oxford University Press. p. 1–430 (2015)
76. S. Lu, H. Fujii, H. Sugiyama, M. Tanaka, K. Nogi, and The Iron and Steel Institute of Japan, Effects of Oxygen Additions to Argon Shielding Gas on GTA Weld Shape, ISIJ Int., 2003, 43(10), p 1590–1595.10.2355/isijinternational.43.1590 ↗
77. A. Eliasson, Liquid Phase Sintering of W–Ni–Fe Composites: Initial Melt Penetration, Agglomerate Separation and Particle Interaction, Doctoral Thesis, KTH Royal Institute of Technology. p. 1–20, KTH (2006)
78. D. Vedel, B. Bégand, T. Baron, and Elsevier, Wetting and Interfacial Behavior of Fe, Co, Ni on (Ti, Zr, Hf, Nb, Ta) C High-Entropy Ceramics, Open Ceramics, 2023, 15, 100393.10.1016/j.oceram.2023.100393 ↗
79. A. D. Kirshenbaum, J. A. Cahill, The Density of Liquid Iron from the Melting Point to 2500 K, Trans. Metall. Soc. AIME, vol. 224, p. 385–389, AIME (1962)
80. K. Mukai, T. Hibiya, J. Brillo, I. Egry, Density of Ni–Cr Alloy in Liquid and Solid–Liquid Coexistence States; Liquid Ni at the Melting Point and its Thermal Expansion. Mater. Trans. vol. 43, no. 5, p. 1153–1157, The Japan Institute of Metals and Materials (2002)10.2320/matertrans.43.1153 ↗
81. K. Assael, S. K. Polimatidou, D. G. Frangis, Viscosity of Liquid Iron, Journal of Physical and Chemical Reference Data, vol. 35, no. 1, p. 285–300, American Institute of Physics (2006)10.1063/1.2149380 ↗
82. Y. Sato, K. Sugisawa, D. Aoki, and T. Yamamura, Viscosities of Fe–Ni, Fe–Co and Ni–Co Binary Melts, Meas. Sci. Technol., 2005, 16(2), p 363–371.10.1088/0957-0233/16/2/006 ↗
83. R. SanSoucie, M. P. Green, J. J. Foley, Surface Tension and Viscosity of Liquid Nickel Under Controlled Oxygen Partial Pressures. Int. J. Thermophys. vol. 37, no. 5, p. 76–88, Springer (2016)10.1007/s10765-016-2085-6 ↗
84. H. Kobatake and J. Brillo, Density and Viscosity of Ternary Cr–Fe–Ni Liquid Alloys, J. Mater. Sci., 2013, 48, p 6818–6824.10.1007/s10853-013-7487-2 ↗
85. S. Lu, H. Fujii, and K. Nogi, Marangoni Convection and Weld Shape Variations in Ar–O2 and Ar–CO2 Shielded GTA Welding, Mater. Sci. Eng. A, 2004, 380, p 290–297.10.1016/j.msea.2004.05.057 ↗
86. J. Xu, X. Zhou, and D. Zhu, Effect of Arc Length on Oxygen Content and Mechanical Properties of Weld Metal During Pulsed GMAW, Crystals, 2022, 12(176), p 1–10.
87. X. Xiao and J. Brillo, Surface Tension of Liquid Fe–Ni, Fe–Cr, and Ni–Cr with Physics-Informed Statistical Modeling on the Influence of Oxygen Content, J. Mol. Liq., 2022 https://doi.org/10.1016/j.molliq.2022.11959910.1016/j.molliq.2022.119599 ↗
88. Y. Ogino, F.O. Borgmann, and M.G. Frohberg, On the Anomalous Change of Viscosity of Liquid Iron with Temperature, Trans. Iron Steel Inst. Jpn., 1974, 14(2), p 82–87.10.2355/isijinternational1966.14.82 ↗