Shrinkage Characteristics of Alkali-Activated Slag Cements
Source abstract
Abstract
Recent interest in creating green construction materials has sparked the development of portland cement–free binders. Alkali-activated slag (AAS) concrete has a low embodied energy and comparable or superior strengths to ordinary portland cement (OPC) concrete. However, one factor limiting AAS usage is its durability performance, specifically its susceptibility to shrinkage. Before declaring AAS a marketable product, the mechanisms behind its volumetric instability need to be understood. This paper presents a preliminary study of the shrinkage deformations of various AAS mixtures, wherein four unique AAS mortars were designed and tested for autogenous, chemical, and drying shrinkage; time of setting; and compressive strength. All results were compared to those obtained for a control OPC mortar. Alkali-activated slag mixtures with comparable strength to OPC show a higher autogenous and drying shrinkage. A lower elastic stiffness, higher degree of saturation, and potentially higher chemical shrinkage contribute to the high autogenous shrinkage of AAS. A lower elastic stiffness also leads to a large drying shrinkage, although other mechanisms, such as reduced pore size and carbonation shrinkage, are likely to also contribute to the high drying shrinkage measured for AAS.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Graduate Research Assistant, Dept. of Civil and Environmental Engineering, Pennsylvania State Univ., 3127 Research Dr., State College, PA 16802 (corresponding author).
Assistant Professor of Civil and Environmental Engineering, Pennsylvania State Univ., 231M Sackett Building, University Park, PA 16802.
Assistant Professor of Civil and Environmental Engineering, Pennsylvania State Univ., 231D Sackett Building, University Park, PA 16802.
References (39)
Show source-provided references
1. Adamson A. W. · 1997
2. Ashby M. · 2009
3. ASTM. (2007). “Standard test method for flow of hydraulic cement mortar.” ASTM C1437-07 ASTM International West Conshohocken PA.
4. ASTM. (2008). “Standard test method for time of setting of concrete mixtures by penetration resistance.” ASTM C403M-08 ASTM International West Conshohocken PA.
5. ASTM. (2009). “Standard test method for autogenous strain of cement paste and mortar.” ASTM 1698-09 ASTM International West Conshohocken PA.
6. ASTM. (2011a). “Standard test method for compressive strength of hydraulic cement mortars.” ASTM C 109M-11b ASTM International West Conshohocken PA.
7. ASTM. (2011b). “Standard practice for mechanical mixing of hydraulic cement pastes and mortars of plastic consistency.” ASTM C 305-12 ASTM International West Conshohocken PA.
8. ASTM. (2011c). “Standard specification for concrete aggregates.” ASTM C 33M-11a ASTM International West Conshohocken PA.
9. ASTM. (2012). “Standard specification for slag cement for use in concrete and mortars.” ASTM C989M-12a ASTM International West Conshohocken PA.
10. ASTM. (2013). “Standard practice for use of apparatus for the determination of length change of hardened cement paste mortar and concrete.” ASTM C642-13 ASTM International West Conshohocken PA.
11. 10.1016/S0008-8846(00)00349-510.1016/S0008-8846(00)00349-5 ↗
12. 10.1016/j.cemconres.2010.11.01610.1016/j.cemconres.2010.11.016 ↗
13. 10.1088/0965-0393/6/3/00210.1088/0965-0393/6/3/002 ↗
14. 10.1016/S0008-8846(02)00717-210.1016/S0008-8846(02)00717-2 ↗
15. 10.1016/S0008-8846(02)01096-710.1016/S0008-8846(02)01096-7 ↗
16. 10.1007/s10853-006-0873-210.1007/s10853-006-0873-2 ↗
17. Cincotto M. A. Melo A. A. and Repette W. L. (2003). “Effect of different activators type and dosages and relation to autogenous shrinkage of activated blast furnace slag cement.” Proc. 11th Int. Congress on the Chemistry of Cement G.Grieve and G.Owens eds. The Cement and Concrete Institute of South Africa Midrand South Africa 1878–1888.
18. 10.1016/S0008-8846(00)00327-610.1016/S0008-8846(00)00327-6 ↗
19. 10.1016/j.cemconres.2007.09.00810.1016/j.cemconres.2007.09.008 ↗
20. Properties and durability of alkali-activated slag concrete
21. 10.1016/0008-8846(87)90009-310.1016/0008-8846(87)90009-3 ↗
22. 10.1016/0021-9797(81)90212-510.1016/0021-9797(81)90212-5 ↗
23. Gebregziabiher B. S. and Peethamparan S. (2013). “Characterization of alkali-activated slag gel using nano-indentation.” 3rd Int. Conf. on Sustainable Construction Materials and Technologies (SCMT3) Japan Concrete Institute (JCI).
24. 10.1016/S0008-8846(01)00463-X10.1016/S0008-8846(01)00463-X ↗
25. 10.1061/(ASCE)IS.1943-555X.000021110.1061/(ASCE)IS.1943-555X.0000211 ↗
26. Lura P. (2003). “Autogenous deformation and internal curing of concrete.” Ph.D. dissertation Delft Univ. of Technology Delft the Netherlands.
27. 10.1088/0370-1301/63/1/30210.1088/0370-1301/63/1/302 ↗
28. 10.1016/j.cemconres.2007.11.00210.1016/j.cemconres.2007.11.002 ↗
29. Mindess S. · 2003
30. 10.1016/j.cemconres.2006.11.02110.1016/j.cemconres.2006.11.021 ↗
31. Powers T. C. and Brownyard T. L. (1948). Studies of the physical properties of hardened portland cement paste Bulletin 22 Research Laboratories of the Portland Cement Association Chicago.
32. 10.1007/s10853-005-1821-210.1007/s10853-005-1821-2 ↗
33. Radlińska A. Rajabipour F. Bucher B. Henkensiefken R. Sant G. and Weiss J. (2008). “Shrinkage mitigation strategies in cementitious systems: A closer look at differences in sealed and unsealed behaviour.” Transportation Research Record 2070 Transportation Research Board Washington DC 59–67.10.3141/2070-08 ↗
34. 10.1016/j.cemconcomp.2012.03.00610.1016/j.cemconcomp.2012.03.006 ↗
35. Sant G. Lura P. and Weiss J. (2006). “Measurement of volume change in cementitious materials at early ages.” Transportation Research Record 1979 Transportation Research Board Washington DC 21–29.10.1177/0361198106197900104 ↗
36. 10.4324/978020339067210.4324/9780203390672 ↗
37. 10.1007/978-3-642-17866-510.1007/978-3-642-17866-5 ↗
38. 10.1016/j.cemconres.2011.11.00310.1016/j.cemconres.2011.11.003 ↗
39. Performance of shrinkage reducing admixtures at different humidities at early ages