Effects of Deicing Salts on the Scaling Resistance of Concrete
Source abstract
Abstract
The scaling resistance of concrete with strength grades of 30 MPa (C30) and 50 MPa (C50) subjected to different types (A and B) and concentrations (3, 5, and 20%) of deicing salt solution were studied using an accelerated freezing-thawing test. Deicing Salt A was composed of about 80% sodium chloride and 20% calcium chloride, B was composed of 70% sodium chloride, 25% magnesium chloride and 5% calcium chloride. The changes in strength, mass loss and relative dynamic modulus of elasticity of concrete were examined during the testing. The results showed that the salt scaling resistance of C50 was better than that of C30. The former could pass 160 freezing-thawing cycles while the latter could pass only 95 cycles. Specimens showed the largest deterioration when subjected to 5% solution, and the smallest deterioration when subjected to 20% solution after 200 cycles. Deicing salts with a higher percentage of NaCl and CaCl2 demonstrated a more obvious deterioration effect on concrete. The incorporation of 5% silica fume (by the mass of binder) or 1% high-efficiency air entraining agent significantly improved the salt scaling resistance of the concrete, even no visible deterioration was observed after 200 cycles. The main scaling deterioration features of concrete include surface spalling and cracking. Microstructural examinations indicated that formation of Friedel’s salt resulting from chemical reaction between NaCl or CaCl2 and calcium aluminate hydrates could lead to the deterioration of concrete during salt scaling testing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Ph.D. Candidate, College of Civil Engineering, Hunan Univ., Changsha 410082, P.R. China.
Professor, College of Civil Engineering, Hunan Univ., Changsha 410082, P.R. China (corresponding author).
Professor, Dept. of Civil Engineering, Nanjing Univ. of Aeronautics and Astronautics, Nanjing 210016, P.R. China.
References (41)
Show source-provided references
1. How poor curing leads to scaling
2. 10.1016/S0008-8846(96)00162-710.1016/S0008-8846(96)00162-7 ↗
3. 10.1016/j.cemconcomp.2007.09.00310.1016/j.cemconcomp.2007.09.003 ↗
4. Chinese National Standard. (2009). “The test methods for long-term performance and durability of ordinary concrete.” GB/J 50082-2009 Beijing China.
5. 10.1016/j.conbuildmat.2010.02.01510.1016/j.conbuildmat.2010.02.015 ↗
6. 10.1016/S0958-9465(02)00052-510.1016/S0958-9465(02)00052-5 ↗
7. The international cooperative test of the critical degree of saturation method of assessing the freeze/thaw resistance of concrete
8. 10.1016/j.cemconres.2004.04.00610.1016/j.cemconres.2004.04.006 ↗
9. 10.1016/0008-8846(88)90053-110.1016/0008-8846(88)90053-1 ↗
10. Gagne R. · 1990 · 29
11. 10.1016/j.conbuildmat.2008.10.00110.1016/j.conbuildmat.2008.10.001 ↗
12. 10.1016/S0008-8846(02)00910-910.1016/S0008-8846(02)00910-9 ↗
13. 10.1016/0008-8846(84)90079-610.1016/0008-8846(84)90079-6 ↗
14. Influence of silica fume replacement of cement on physical properties and resistance to sulfate attack, freezing and thawing and alkali-silica reactivity
15. 10.1016/0008-8846(94)90186-410.1016/0008-8846(94)90186-4 ↗
16. Lee H. Cody R. D. Cody A. M. and Spry P. G. (2000). “Effects of various deicing chemicals on pavement and concrete deterioration.” Proc. Mid-Continent Transportation Symp. Center for Transportation Research and Education 151–155.
17. Cracking-corrosion interaction in concrete exposed to marine environment
18. Mehta P. K. · 2006
19. Mehta P. K. Schiessl P. and Raupach M. (1992). “Performance and durability of concrete systems.” Proc. 9th Int. Congress on the Chemistry of Cement New Delhi India 571–659.
20. 10.1016/j.conbuildmat.2010.10.00410.1016/j.conbuildmat.2010.10.004 ↗
21. 10.1016/j.cemconres.2007.09.00310.1016/j.cemconres.2007.09.003 ↗
22. A working hypothesis for further studies of frost resistance
23. Theory of volume change in hardened portland cement pastes during freezing
24. 10.1016/0008-8846(89)90036-710.1016/0008-8846(89)90036-7 ↗
25. Improving the durability of concrete to freezing and deicing salts
26. 10.1016/j.cemconcomp.2007.10.00610.1016/j.cemconcomp.2007.10.006 ↗
27. 10.1016/j.cemconcomp.2010.06.00110.1016/j.cemconcomp.2010.06.001 ↗
28. Stark J. and Stürmer S. (1997). “Investigation of compatibility of cements with several salts.” Proc. 10th Int. Congress Chemistry Cement SINTEF Trondheim Norway 4.
29. 10.1016/S0008-8846(02)00769-X10.1016/S0008-8846(02)00769-X ↗
30. 10.1016/j.cemconres.2009.09.02710.1016/j.cemconres.2009.09.027 ↗
31. 10.1016/S0008-8846(96)85010-110.1016/S0008-8846(96)85010-1 ↗
32. Tremblay M. H. Lory F. and Marchand J. (2007). “Ability of the glue spall model to account for the de-icer salt scaling deterioration of concrete.” Proc. 12th Int. Congress on the Chemistry of Cement Montreal Canada 123–132.
33. 10.1111/j.1551-2916.2006.00913.x10.1111/j.1551-2916.2006.00913.x ↗
34. 10.1016/j.cemconres.2007.03.00510.1016/j.cemconres.2007.03.005 ↗
35. 10.1016/j.cemconres.2007.03.00310.1016/j.cemconres.2007.03.003 ↗
36. Valenza J. J. · 2005 · 207
37. Verbeck G. · 1982 · 211
38. 10.1016/j.cemconcomp.2005.07.00610.1016/j.cemconcomp.2005.07.006 ↗
39. Whiting D. · 1989 · 343
40. Effects of salt and snow-thawing agent types on salt-scaling damage of concrete
41. Effects of NaCl concentration on ice-formation expansion and the solution absorption by concrete