journal article·2011-10

Effect of Disodium Hydrogen Phosphate on Hydration and Hardening of Magnesium Potassium Phosphate Cement

Chun-xiang Qian, Jian-Ming Yang

Publisher page

Abstract

Magnesium potassium phosphate cement (MKPC) is usually produced by using dead burned MgO and potassium dihydrogen phosphate. A new MKPC was prepared by using combination of potassium dihydrogen phosphate (KH2PO4) and disodium hydrogen phosphate (Na2HPO4·12H2O) in certain ratios instead of potassium dihydrogen phosphate alone. To investigate the effect of disodium hydrogen phosphate on hydration and hardening of MKPC, pH value, hydration temperature, setting times, and strength development were measured. The results indicated that disodium hydrogen phosphate increased the pH value of MKPC paste, resulted in endothermic reactions, and cooled MKPC paste. Thus, it retarded early hydration, improved the fluidity, and increased setting times of MKPC paste. Although the early compressive strength of hardened MKPC made with a combination of the two phosphates was slightly lower than that of hardened MKPC prepared with single potassium dihydrogen phosphate, its strength development is sustaining and was higher than that of hardened MKPC with single potassium dihydrogen phosphate at 60 days because of better crystallization and more stable hydration products.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Oxide Properties and Applications · Multiferroics and related materials · Electromagnetic wave absorption materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Southeast Univ., Nanjing, 211189, China; and Jiangsu Key Lab of Construction Material, Nanjing, 211189, China (corresponding author).

School of Materials Science and Engineering, Southeast Univ., Nanjing, 211189, China; and Civil Engineering School, Yancheng Institute of Technology, Yancheng, 224051, China.

References (25)

Show source-provided references
1. 10.1016/0008-8846(88)90075-010.1016/0008-8846(88)90075-0 ↗
2. 10.1016/0008-8846(88)90075-010.1016/0008-8846(88)90075-0 ↗
3. Allan W. (1996). “Method of slowing the setting rate of magnesium phosphate cements.” WO 96/35647 Nov. 14 18.
4. The chemistry of struvite crystallization
5. 10.1016/j.jhazmat.2009.04.09110.1016/j.jhazmat.2009.04.091 ↗
6. 10.1016/j.cemconcomp.2004.03.00310.1016/j.cemconcomp.2004.03.003 ↗
7. High-early-strength magnesium phosphate cement with fly ash
8. 10.1080/0959333280861889910.1080/09593332808618899 ↗
9. Investigation of the hydrating and hardening mechanisms of phosphate cement for repair with super rapid hardening
10. Investigation of MPB with super early strength for repair of concrete
11. Study on magnesium phosphate cement
12. Research on water resistance of magnesium phosphate cement
13. Effect of the particle sizes of raw materials on hydration and hardening process of calcium phosphate bone cement
14. 10.1016/j.cemconres.2003.09.01710.1016/j.cemconres.2003.09.017 ↗
15. 10.1016/0008-8846(93)90090-V10.1016/0008-8846(93)90090-V ↗
16. 10.1016/S0008-8846(99)00254-910.1016/S0008-8846(99)00254-9 ↗
17. 10.1016/S0008-8846(01)00647-010.1016/S0008-8846(01)00647-0 ↗
18. Wagh A. Jeong S. Y. and Singh D. (1997). “High strength phosphate cement using industrial by-product ashes.” Proc. 1st Int. Conf. ASCE Kona HI 542–533.
19. Studied for epikote-sodium dihydrogen phosphate complex material of phase change energy storage
20. 10.1007/s11595-010-0055-610.1007/s11595-010-0055-6 ↗
21. 10.1016/S0008-8846(98)00230-010.1016/S0008-8846(98)00230-0 ↗
22. 10.1016/S0008-8846(00)00419-110.1016/S0008-8846(00)00419-1 ↗
23. 10.1007/BF0247933210.1007/BF02479332 ↗
24. 10.1016/S0008-8846(01)00651-210.1016/S0008-8846(01)00651-2 ↗
25. Zhao F. · 2007