journal article·2019-10

Strength, Durability, and Thermal Properties of Glass Aggregate Mortars

Karla Gorospe, Emad Booya, Hossein Ghaednia, Sreekanta Das

Publisher page

Abstract

This study investigated the use of glass aggregates as a building and construction material through the assessment of strength, durability, and thermal properties of cement mortars. A combination of crushed glass and glass beads was incorporated in the mortar specimens as 30%, 50%, 70%, and 100% replacement of natural sand. Compressive strength was studied, until 365 days, using standard (20°C) and accelerated (50°C) curing conditions. A decrease in strength was observed with increasing glass aggregate amount. Nonetheless, higher strength gain was evident in glass aggregate mortars cured in standard conditions at later ages. Qualitative analysis of durability by means of plastic shrinkage cracking indicated that full replacement of natural sand with glass aggregates reduces 96% of cracks as compared to mortar containing no glass. Further, chloride permeation of glass aggregate mortars was improved with increasing glass replacement and age due to the inherently impermeable nature of glass particles. Glass aggregates also improved the overall thermal conductivity of mortar because glass itself has low thermal conductivity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycled Aggregate Concrete Performance · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

M.A.Sc. Candidate, Dept. of Civil and Environmental Engineering, Univ. of Windsor, Windsor, ON, Canada N9B 3P4 (corresponding author).

Ph.D. Candidate, Dept. of Civil and Environmental Engineering, Univ. of Windsor, Windsor, ON, Canada N9B 3P4.

Postdoctoral Fellow, Dept. of Civil and Environmental Engineering, Univ. of Windsor, Windsor, ON, Canada N9B 3P4.

Professor, Dept. of Civil and Environmental Engineering, Univ. of Windsor, Windsor, ON, Canada N9B 3P4.

References (40)

Show source-provided references
1. 10.1016/j.conbuildmat.2016.04.07210.1016/j.conbuildmat.2016.04.072 ↗
2. 10.1016/j.conbuildmat.2011.07.02010.1016/j.conbuildmat.2011.07.020 ↗
3. 10.1061/(ASCE)MT.1943-5533.000107710.1061/(ASCE)MT.1943-5533.0001077 ↗
4. 10.1111/j.1747-1567.2007.00191.x10.1111/j.1747-1567.2007.00191.x ↗
5. 10.1016/S0950-0618(00)00058-110.1016/S0950-0618(00)00058-1 ↗
6. 10.1007/BF0248313210.1007/BF02483132 ↗
7. 10.1007/BF0253358810.1007/BF02533588 ↗
8. 10.1016/j.cemconcomp.2016.10.00410.1016/j.cemconcomp.2016.10.004 ↗
9. 10.1016/j.anucene.2016.09.03510.1016/j.anucene.2016.09.035 ↗
10. 10.1016/j.cemconres.2008.03.02010.1016/j.cemconres.2008.03.020 ↗
11. 10.1016/j.jclepro.2012.09.02110.1016/j.jclepro.2012.09.021 ↗
12. 10.1155/2016/128089410.1155/2016/1280894 ↗
13. 10.1016/0958-9465(96)00017-010.1016/0958-9465(96)00017-0 ↗
14. 10.1016/j.cemconcomp.2012.08.02910.1016/j.cemconcomp.2012.08.029 ↗
15. Effect of curing temperature on cement hydration
16. 10.1016/S0008-8846(01)00471-910.1016/S0008-8846(01)00471-9 ↗
17. Foster C. W. 1970. “Use of waste glass as asphaltic concrete aggregate.” Master’s thesis Dept. of Civil Architectural and Environmental Engineering Missouri Univ. of Science and Technology.
18. 10.1016/S0958-9465(03)00068-410.1016/S0958-9465(03)00068-4 ↗
19. 10.1016/j.conbuildmat.2009.12.03010.1016/j.conbuildmat.2009.12.030 ↗
20. 10.1016/j.cemconcomp.2010.09.01310.1016/j.cemconcomp.2010.09.013 ↗
21. 10.1016/j.ijsbe.2016.05.00710.1016/j.ijsbe.2016.05.007 ↗
22. 10.1016/j.wasman.2008.08.01210.1016/j.wasman.2008.08.012 ↗
23. 10.1016/j.conbuildmat.2015.06.01010.1016/j.conbuildmat.2015.06.010 ↗
24. 10.1016/j.cemconcomp.2008.12.00210.1016/j.cemconcomp.2008.12.002 ↗
25. 10.1016/j.jclepro.2012.02.01810.1016/j.jclepro.2012.02.018 ↗
26. Use of domestic waste glass as aggregate in bituminous concrete
27. 10.1617/s11527-014-0342-310.1617/s11527-014-0342-3 ↗
28. Pore structure of concrete with mineral admixtures and its effect on self-desiccation shrinkage
29. Influence of different fibers on plastic shrinkage cracking of concrete
30. 10.1016/j.cemconres.2004.02.00610.1016/j.cemconres.2004.02.006 ↗
31. Portland Cement Association · 2001
32. Strength development of concrete made with recycled glass aggregates subjected to frost curing conditions
33. 10.1016/j.conbuildmat.2006.11.01810.1016/j.conbuildmat.2006.11.018 ↗
34. Straube J. · 2017
35. 10.1061/(ASCE)0899-1561(2009)21:12(709)10.1061/(ASCE)0899-1561(2009)21:12(709) ↗
36. 10.1016/j.cemconcomp.2012.08.02810.1016/j.cemconcomp.2012.08.028 ↗
37. 10.1016/j.cemconres.2003.07.00310.1016/j.cemconres.2003.07.003 ↗
38. USEPA. 2018. “Facts and figures about materials waste and recycling.” Accessed June 06 2018. https://www.epa.gov/facts-and-figures-about-materials-waste-and-recycling/glass-material-specific-data.
39. 10.1061/(ASCE)MT.1943-5533.000097910.1061/(ASCE)MT.1943-5533.0000979 ↗
40. Effect of surrogate aggregates on the thermal conductivity of concrete at ambient and elevated temperatures