Abstract

This paper investigates the microstructure and autogenous shrinkage of calcined kaolinitic clay-limestone (LC) blended cement paste composites up to 200 days. The calcined clay-limestone content ranged between 20% and 65%. The microstructural parameters were studied using X-ray diffraction (XRD), thermogravimetric analysis (TGA), nitrogen adsorption (NAD), and Fourier transform infrared (FTIR) spectroscopy. The results showed that calcined kaolinitic clay-limestone blends developed higher autogenous shrinkage, faster hydration, and finer pore structure compared to the reference cement mixture. Autogenous shrinkage was the highest at 27% cement replacement and then decreased with further increases in replacement level. Both hydration and pore size distribution led to the development of high autogenous shrinkage for all calcined kaolinitic clay-limestone (LC) blends.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Grouting, Rheology, and Soil Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Ph.D. Candidate, Centre for Infrastructure Engineering and Safety, School of Civil and Environmental Engineering, Univ. of New South Wales (UNSW), Sydney, NSW 2052, Australia.

Senior Lecturer, Centre for Infrastructure Engineering and Safety, School of Civil and Environmental Engineering, Univ. of New South Wales (UNSW), Sydney, NSW 2052, Australia (corresponding author). ORCID: .

Professor, School of Civil and Environmental Engineering, Univ. of Technology Sydney (UTS), Sydney, NSW 2007, Australia.

References (100+)

Show source-provided references
1. 10.1016/j.conbuildmat.2017.12.16510.1016/j.conbuildmat.2017.12.165 ↗
2. 10.1016/j.conbuildmat.2022.12889110.1016/j.conbuildmat.2022.128891 ↗
3. 10.1016/j.conbuildmat.2022.12694910.1016/j.conbuildmat.2022.126949 ↗
4. 10.1617/s11527-023-02099-810.1617/s11527-023-02099-8 ↗
5. Aili, A., and I. Maruyama. 2020. “Review of several experimental methods for characterization of micro-and nano-scale pores in cement-based material.” Int. J. Concr. Struct. Mater. 14 (Dec): 1–18. https://doi.org/10.1186/s40069-020-00431-y.10.1186/s40069-020-00431-y ↗
6. 10.1016/j.cemconres.2004.06.01510.1016/j.cemconres.2004.06.015 ↗
7. 10.1021/ie401616f10.1021/ie401616f ↗
8. 10.1016/j.clay.2015.01.02810.1016/j.clay.2015.01.028 ↗
9. 10.1016/j.cemconres.2012.09.00610.1016/j.cemconres.2012.09.006 ↗
10. 10.1016/j.cemconres.2018.10.01110.1016/j.cemconres.2018.10.011 ↗
11. 10.1016/j.cemconres.2018.02.01610.1016/j.cemconres.2018.02.016 ↗
12. 10.1016/j.cemconres.2016.02.01510.1016/j.cemconres.2016.02.015 ↗
13. 10.1016/0021-9797(81)90395-710.1016/0021-9797(81)90395-7 ↗
14. 10.1016/j.cemconres.2009.06.00510.1016/j.cemconres.2009.06.005 ↗
15. 10.1016/j.cemconres.2015.02.01110.1016/j.cemconres.2015.02.011 ↗
16. 10.1016/S0008-8846(01)00750-510.1016/S0008-8846(01)00750-5 ↗
17. 10.1016/j.cemconres.2004.10.02010.1016/j.cemconres.2004.10.020 ↗
18. 10.1021/ja01145a12610.1021/ja01145a126 ↗
19. Bentz, D. P. 2010. “Powder additions to mitigate retardation in high-volume fly ash mixtures.” ACI Mater. J. 107 (5): 508–514. https://doi.org/10.14359/51663971.
20. 10.1016/j.conbuildmat.2014.10.04210.1016/j.conbuildmat.2014.10.042 ↗
21. 10.1016/S0958-9465(03)00045-310.1016/S0958-9465(03)00045-3 ↗
22. 10.1016/j.jclepro.2016.02.12510.1016/j.jclepro.2016.02.125 ↗
23. 10.1016/S0958-9465(03)00065-910.1016/S0958-9465(03)00065-9 ↗
24. 10.1016/S0958-9465(00)00095-010.1016/S0958-9465(00)00095-0 ↗
25. 10.1016/0021-9797(67)90243-310.1016/0021-9797(67)90243-3 ↗
26. 10.1016/j.cemconres.2013.05.02110.1016/j.cemconres.2013.05.021 ↗
27. 10.1016/j.cemconres.2007.08.00510.1016/j.cemconres.2007.08.005 ↗
28. 10.1016/j.cemconres.2010.01.01410.1016/j.cemconres.2010.01.014 ↗
29. 10.1016/0008-8846(94)00108-B10.1016/0008-8846(94)00108-B ↗
30. 10.1016/j.cemconres.2010.08.01410.1016/j.cemconres.2010.08.014 ↗
31. 10.1016/0095-8522(66)90006-710.1016/0095-8522(66)90006-7 ↗
32. 10.1016/j.conbuildmat.2017.04.13210.1016/j.conbuildmat.2017.04.132 ↗
33. 10.1016/j.cemconres.2018.02.00510.1016/j.cemconres.2018.02.005 ↗
34. 10.1016/j.cemconres.2021.10639610.1016/j.cemconres.2021.106396 ↗
35. 10.1016/j.cemconcomp.2017.08.01210.1016/j.cemconcomp.2017.08.012 ↗
36. 10.1016/j.conbuildmat.2020.12015210.1016/j.conbuildmat.2020.120152 ↗
37. 10.1016/j.conbuildmat.2010.12.05510.1016/j.conbuildmat.2010.12.055 ↗
38. 10.1016/j.cemconres.2008.03.01010.1016/j.cemconres.2008.03.010 ↗
39. 10.1007/BF0247363910.1007/BF02473639 ↗
40. Feldman, R. F., and P. J. Sereda. 1970. “A new model for hydrated Portland cement and its practical implications.” Eng. J. 53 (8–9): 53–59.
41. 10.1016/j.cemconres.2010.09.01310.1016/j.cemconres.2010.09.013 ↗
42. 10.1016/j.clay.2018.12.02110.1016/j.clay.2018.12.021 ↗
43. 10.1016/j.cemconres.2020.10631210.1016/j.cemconres.2020.106312 ↗
44. 10.1016/j.conbuildmat.2016.09.12310.1016/j.conbuildmat.2016.09.123 ↗
45. 10.1016/j.cemconcomp.2006.09.00510.1016/j.cemconcomp.2006.09.005 ↗
46. 10.1016/0021-9797(69)90132-510.1016/0021-9797(69)90132-5 ↗
47. 10.1021/ja01236a04810.1021/ja01236a048 ↗
48. 10.1016/j.conbuildmat.2013.10.01110.1016/j.conbuildmat.2013.10.011 ↗
49. 10.1016/j.cemconres.2007.10.00610.1016/j.cemconres.2007.10.006 ↗
50. 10.1016/j.conbuildmat.2014.03.02310.1016/j.conbuildmat.2014.03.023 ↗
51. 10.1016/j.cemconres.2019.05.00810.1016/j.cemconres.2019.05.008 ↗
52. 10.1016/j.conbuildmat.2017.08.09110.1016/j.conbuildmat.2017.08.091 ↗
53. 10.1680/jadcr.18.0017210.1680/jadcr.18.00172 ↗
54. 10.3141/2290-0210.3141/2290-02 ↗
55. 10.1680/adcr.2000.12.1.3510.1680/adcr.2000.12.1.35 ↗
56. 10.1016/j.cemconres.2018.03.01010.1016/j.cemconres.2018.03.010 ↗
57. 10.1016/j.conbuildmat.2019.06.12310.1016/j.conbuildmat.2019.06.123 ↗
58. 10.1016/j.conbuildmat.2017.09.16510.1016/j.conbuildmat.2017.09.165 ↗
59. 10.1016/j.conbuildmat.2010.04.01810.1016/j.conbuildmat.2010.04.018 ↗
60. 10.1016/j.conbuildmat.2013.12.01010.1016/j.conbuildmat.2013.12.010 ↗
61. 10.1016/j.cemconres.2008.01.00210.1016/j.cemconres.2008.01.002 ↗
62. 10.1016/j.cemconres.2010.12.00110.1016/j.cemconres.2010.12.001 ↗
63. 10.1016/S0008-8846(02)00890-610.1016/S0008-8846(02)00890-6 ↗
64. 10.1016/S0008-8846(01)00601-910.1016/S0008-8846(01)00601-9 ↗
65. 10.1617/s11527-022-01989-710.1617/s11527-022-01989-7 ↗
66. Malvern Mastersizer. 2023. “Malvern Mastersizer 2000.” Accessed July 7 2023. https://www.malvernpanalytical.com/en/products/category/particle-size-analyzers.
67. 10.1016/0009-2541(92)90064-C10.1016/0009-2541(92)90064-C ↗
68. Meddah, M. S., and A. Tagnit-Hamou. 2009. “Pore structure of concrete with mineral admixtures and its effect on self-desiccation shrinkage.” ACI Mater. J. 106 (3): 241–250.
69. 10.1016/j.conbuildmat.2018.06.13810.1016/j.conbuildmat.2018.06.138 ↗
70. 10.1016/j.conbuildmat.2020.11945410.1016/j.conbuildmat.2020.119454 ↗
71. 10.1016/j.cemconres.2009.10.01410.1016/j.cemconres.2009.10.014 ↗
72. 10.1016/j.cemconres.2004.09.01310.1016/j.cemconres.2004.09.013 ↗
73. 10.1016/j.jcis.2015.02.06610.1016/j.jcis.2015.02.066 ↗
74. 10.1016/j.cemconres.2011.08.00410.1016/j.cemconres.2011.08.004 ↗
75. Muller, N., and J. Harnisch. 2007. A blueprint for a climate friendly cement industry. Gland, Switzerland: WWF International.
76. 10.1016/j.cemconcomp.2019.02.01910.1016/j.cemconcomp.2019.02.019 ↗
77. 10.3390/jmse805030110.3390/jmse8050301 ↗
78. 10.1016/j.conbuildmat.2021.12572010.1016/j.conbuildmat.2021.125720 ↗
79. 10.3151/jact.16.34310.3151/jact.16.343 ↗
80. Nguyen, Q. D., M. S. H. Khan, and A. Castel. 2020b. “Chloride diffusion in limestone flash calcined clay cement concrete.” ACI Mater. J. 117 (6): 165–175. https://doi.org/10.14359/51725986.
81. 10.1016/j.cemconres.2020.10617610.1016/j.cemconres.2020.106176 ↗
82. 10.1617/s11527-015-0789-x10.1617/s11527-015-0789-x ↗
83. 10.1111/j.1151-2916.1997.tb03144.x10.1111/j.1151-2916.1997.tb03144.x ↗
84. 10.1016/j.conbuildmat.2015.08.09410.1016/j.conbuildmat.2015.08.094 ↗
85. 10.1016/j.ces.2003.09.01710.1016/j.ces.2003.09.017 ↗
86. 10.1016/j.cemconres.2011.09.01010.1016/j.cemconres.2011.09.010 ↗
87. 10.1016/j.cemconres.2019.02.00910.1016/j.cemconres.2019.02.009 ↗
88. Saje, D. 2015. “Reduction of the early autogenous shrinkage of high strength concrete.” Adv. Mater. Sci. Eng. 2015 (Jan): 310641. https://doi.org/10.1155/2015/310641.10.1155/2015/310641 ↗
89. 10.1680/adcr.14.0010410.1680/adcr.14.00104 ↗
90. 10.1680/jgrma.18.0002910.1680/jgrma.18.00029 ↗
91. 10.1016/j.cemconres.2017.08.01710.1016/j.cemconres.2017.08.017 ↗
92. 10.1201/b1907410.1201/b19074 ↗
93. 10.1016/j.powtec.2014.01.04610.1016/j.powtec.2014.01.046 ↗
94. 10.1016/j.clay.2016.07.01510.1016/j.clay.2016.07.015 ↗
95. 10.1016/j.cemconres.2018.11.00310.1016/j.cemconres.2018.11.003 ↗
96. 10.1016/j.cemconres.2016.06.00610.1016/j.cemconres.2016.06.006 ↗
97. 10.1016/j.clay.2013.12.01610.1016/j.clay.2013.12.016 ↗
98. 10.1617/s11527-018-1298-510.1617/s11527-018-1298-5 ↗
99. 10.1016/j.cemconres.2014.06.00910.1016/j.cemconres.2014.06.009 ↗
100. 10.1007/978-94-024-1207-9_7210.1007/978-94-024-1207-9_72 ↗