Transitioning from AASHTO T283 to the Simple Performance Test Using Moisture Conditioning
Source abstract
Abstract
The current method of determining the moisture susceptibility of asphalt concrete mixtures is American Association of State Highway and Transportation Officials (AASHTO) T283. AASHTO T283 is based on the Marshall mix design method, however the current state of the practice for an asphalt concrete mixture design is the Superpave mix design method. There has not been a transition in test procedure from Marshall mix design to Superpave mix design in that Superpave adopted AASHTO T283 to evaluate the moisture susceptibility of asphalt concrete mixtures even though it was based on Marshall mix design. The procedures in AASHTO T283 and National Cooperative Highway Research Program (NCHRP) Report 444 consider the loss of strength due to freeze/thaw cycling and the effects of moisture existing in specimens compared to unconditioned specimens. Current research (NCHRP Project 9-34) is considering the use of a modified environmental conditioning system (ECS) with dynamic complex modulus testing. However, mixtures do not experience such a pure phenomenon. Pavements undergo cycling of environmental conditions, but when moisture is present, there is repeated hydraulic loading with development of pore pressure in mixtures. Thus, AASHTO T283 and NCHRP Report 444 do not consider the effect of pore pressure, but rather consider a single load effect on environmentally conditioned specimens. The test procedure proposed in this paper uses a retained dynamic modulus of 60% of conditioned specimens to unconditioned specimens. This initial criterion was derived as it is the same percentage of mixtures that fail the AASHTO T283 criteria (80%) of the 21 field mixes that were sampled. Comparison of mixtures performance ranked via AASHTO T283 and the proposed retained dynamic modulus criteria results in considerably different rankings. Pavements undergo cycling of environmental conditions, but when moisture is present, there is repeated hydraulic loading with the development of pore pressure in mixtures. Thus, the results of this testing can be input into the AASHTO Mechanistic-Empirical Pavement Design Guide to consider the effects of unconditioned versus conditioned dynamic modulus values and their respective impacts in pavement performance in terms of predicting pavement distresses.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Asphalt Pavement Performance Evaluation · Geotechnical Engineering and Underground Structures · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Product Development Engineer, SemMaterials, LP, 6502 South Yale Ave., Tulsa, OK 74136.
Associate Professor Dept. of Civil, Construction, and Environmental Engineering, Iowa State Univ., 494 Town Engineering, Ames, IA 50011 (corresponding author).
References (32)
Show source-provided references
1. AASHO · 2001 · T283-1–T283-8
2. Alam M. M. Tandon V. Nazarian S. and Tahmoressi M. (1998). “Identification of moisture-susceptible asphalt concrete mixes using modified environmental conditioning system.” Transportation Research Record . 1630 Transportation Research Board Washington D.C. 106–116.10.3141/1630-13 ↗
3. Al-Swailmi S. Scholz T. and Terrel R. (1992). “Development and evaluation of test system to induce and monitor moisture damage to asphalt concrete mixtures.” Transportation Research Record . 1353 Transportation Research Board Washington D.C. 39–45.
4. Evaluation of the environmental conditioning system (ECS), with AASHTO T-283
5. Evaluation of water damage of asphalt concrete mixtures using the environmental conditioning system (ECS)
6. Comparison of several moisture susceptibility tests to pavements of known field performance
7. Ayyub B. · 1997
8. Bausano J. (2006). “Development of a new test procedure to evaluate the moisture susceptibility of hot mix asphalt.” Doctoral dissertation Iowa State Univ. Ames Iwoa.
9. Choubane B. Page G. and Musselman J. (2000). “Effects of water saturation level on resistance of compacted hot-mix asphalt samples to moisture-induced damage.” Transportation Research Record . 1723 Transportation Research Board Washington D.C. 97–106.10.3141/1723-13 ↗
10. Copeland A. R. Youtcheff J. S. Jr. and Shenoy A. (2007). “Moisture sensitivity of modified asphalt binders: Factors influencing bond strength.” Proc. 86th Annual Meeting of the Transportation Research Board (CD-ROM) Transportation Researh Board Washington D.C.10.3141/1998-03 ↗
11. Coplantz J. and Newcomb D. (1988). “Water sensitivity test methods for asphalt concrete mixtures: A laboratory comparison.” Transportation Research Record . 1171 Transportation Research Board Washington D.C. 44–50.
12. DATAPAVE. (2004). LTPP DataPave Online ⟨http://www.datapave.com⟩ (August 2005).
13. Epps J. Sebaaly P. Penaranda J. Maher M. McCann M. and Hand A. (2000). “Compatibility of a test for moisture-induced damage with superpave volumetric mix design.” NCHRP 444 Transportation Research Board National Highway Research Council Washington D.C.
14. Factors affecting moisture susceptibility of asphalt concrete mixes
15. Kandhal P. (1994). “Field and laboratory investigation of stripping in asphalt pavements: State of the art report.” Transportation Research Record . 1454 Transportation Research Board Washington D.C. 36–47.
16. Kanitpong K. and Bahia H. (2006). “Evaluation of HMA moisture damage in Wisconsin as it relates to pavement performance.” Proc. 85th Annual Meeting of the Transportation Research Board (CD-ROM) TRB Washington D.C.
17. Kennedy T. McGennis R. and Roberts F. (1983). “Investigation of moisture damage to asphalt concrete and the effect on field performance—A case study.” Transportation Research Record . 911 Transportation Research Board Washington D.C. 158–165.
18. Kennedy T. and Ping W. V. (1991). “Comparison study of moisture damage test methods for evaluating antistripping treatments in asphalt mixtures.” Transportation Research Record . 1323 Transportation Research Board Washington D.C. 94–111.
19. Khosla N. P. Birdsall B. and Kawaguchi S. (2000). “Evaluation of moisture susceptibility of asphalt mixtures—Conventional and new methods.” Transportation Research Record . 1728 Transportation Research Board Washington D.C. 43–51.10.3141/1728-07 ↗
20. Lottman R. P. (1978). “National Highway Research Council Report 192: Predicting moisture-inducted damage to asphaltic concrete.” Rep to Transportation Research Board National Highway Research Council Washington D.C.
21. Lottman R. P. (1982). “National Highway Research Council Report 246: Predicting moisture-inducted damage to asphaltic concrete—Field evaluation.” Rep. to Transportation Research Board National Highway Research Council Washington D.C.
22. Lu Q. and Harvey J. T. (2007). “Inclusion of moisture effect in fatigue test for asphalt pavements.” Proc. 86th Annual Meeting of the Transportation Research Board (CD-ROM) Transportation Research Board Washington D.C.10.1061/40961(319)82 ↗
23. Roberts F. L. Kandhal P. S. Brown E. R. Lee D.-Y. and Kennedy T. W. (1996). “Hot mix asphalt materials mixture design and construction.” 2nd Ed. National Asphalt Pavement Association Research and Education Foundation Lanham Md.
24. The effect of multiple freeze-thaw cycle conditioning on the moisture damage of asphalt concrete mixtures
25. Shatnawti S. Nagarajaiah M. and Harvey J. (1995). “Moisture sensitivity evaluation of binder-aggregate mixtures.” Transportation Research Record . 1492 Transportation Research Board Washington D.C. 71–84.
26. Simple performance test for moisture damage prediction in asphalt concrete
27. Stroup-Gardiner M. and Epps J. (1992). “Laboratory tests for assessing moisture damage of asphalt concrete mixtures.” Transportation Research Record . 1353 Transportation Research Board Washington D.C. 15–23.
28. Significance of conditioning parameters affecting distinction of moisture susceptible asphalt concrete mixtures in the laboratory
29. Terrel R. and Al-Swailmi S. (1993). “Role of pessimum voids concept in understanding moisture damage to asphalt concrete mixtures.” Transportation Research Record . 1386 Transportation Research Board Washington D.C. 31–37.
30. Tunnicliff D. G. and Root R. E. (1984). “National Highway Research Council Report 274: Use of antistripping additives in asphalt concrete mixtures—Laboratory phase.” Rep. to Transportation Research Board National Highway Research Council Washington D.C.
31. Tunnicliff D. G. and Root R. E. (1995). “National Highway Research Council Report 373: Use of antistripping additives in asphalt concrete mixtures—Field evaluation.” Rep. to Transportation Research Board National Highway Research Council Washington D.C.
32. Witczak M. W. Kaloush K. Pellinen T. El-Basyouny M. and Von Quintus H. (2002). “National Highway Research Council Report 465: Simple performance test for superpave mix design.” Rep. to Transportation Research Board National Research Council Washington D.C.