Influence of Antifoaming Admixture Type on Several Properties of High-Performance Self-Compacting Concrete
Source abstract
Abstract
EN 934-2 “Admixtures for concrete, mortar and grout Concrete admixtures. Definitions, requirements, conformity, marking and labelling” requires that any increase in the air content shall not be more than 2% by volume over that obtained from the reference mix, and most types of superplasticizers (SPs) easily meet this requirement. Some types may even reduce the level of air, and this can result in a less cohesive mix, which may be more prone to bleed and segregation or may leave the mix feeling harsh and difficult to handle. Unfortunately, some types of superplasticizers increase the level of air. Too high a volume of air has been overcome using an antifoaming agent. The influence of new-generation type superplasticizer and antifoaming admixture (AFA) on the air content and workability of high performance self-compacting concrete (HPSCC) is analyzed in this paper. The purpose of this study was to examine the influence of the admixture type on pore size distribution, compressive strength and frost resistance of HPSCC at constant water to cement ratio, type and volume of aggregate, and volume of cement paste. The parameters of the open pores and air voids of hardened HPSCC are also investigated. The results presented in this paper show that admixtures significantly influence the investigated properties of HPSCC.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Concrete and Cement Materials Research · Innovations in Concrete and Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Civil Engineering, Dept. of Building Materials and Processes Engineering, Silesian Technical Univ., Akademicka 5 St., 44-100, Gliwice, Poland.
References (53)
Show source-provided references
1. ACI. (2008). “Guide to durable concrete.” ACI 201.2R.
2. Aïtcin P.-C. (1998). “The influence of the spacing factor on the freeze-thaw durability of high performance concrete.” Int. Symp. of High-Performance and Reactive Power Concretes Sherbrooke QC Canada.10.4324/9780203475034 ↗
3. ASTM. (2008). “Standard test method for resistance of concrete to rapid freezing and thawing.” C666/C666M-03 Reston VA.
4. ASTM. (2014). Standard test method for air content of freshly mixed concrete by the pressure method.” C231/C231M-14 West Conshohocken PA.
5. Austrian Standard. (2002). “Beton. Teil 1: Festlegung Herstellung Verwendung und. Konformitätsnachweis.” ÖNORM B 4710-1.
6. British Standards Institution (BSI). (2003). “Concrete—Part 1: Specification performance production and conformity.” EN 206-1 London.
7. British Standards Institution (BSI). (2008). “Admixtures for concrete mortar and grout—Test methods—Part 11: Determination of air void characteristics in hardened concrete.” EN 480-11 London.
8. British Standards Institution (BSI). (2009a). “Testing fresh concrete. Air content. Pressure methods.” EN 12350-7 London.
9. British Standards Institution (BSI). (2009b). “Testing hardened concrete. Compressive strength of test specimens.” EN 12390-3:2009 London.
10. British Standards Institution (BSI). (2010). “Testing fresh concrete—Part 8: Self-compacting concrete—Slump-flow test.” EN 12350-8 London.
11. British Standards Institution (BSI). (2012). “Admixtures for concrete mortar and grout. Concrete admixtures. Definitions requirements conformity marking and labelling.” EN 934-2:2009+A1:2012 London.
12. Danish Standard. (2004). “Concrete Materials—Rules for application.” DS 2426 Denmark.
13. Fagerlund G. · 1999
14. Relationship between compressive strength and air-void structure of foamed cement-fly ash concrete
15. Federal Ministry of Transport. (2001). “Additional technical terms of contract and guidelines for the construction of pavements.” German Federal Ministry of Communications ZTV Beton-StB 01 FSGV Cologne.
16. 10.1016/j.buildenv.2006.01.01210.1016/j.buildenv.2006.01.012 ↗
17. 10.1016/0008-8846(88)90053-110.1016/0008-8846(88)90053-1 ↗
18. European requirements for air-entrained concrete in XF class environment
19. Grodzicka A. · 2005
20. 10.1016/j.cemconres.2007.09.00610.1016/j.cemconres.2007.09.006 ↗
21. 10.1007/BF0249873810.1007/BF02498738 ↗
22. 10.1016/S0008-8846(01)00665-210.1016/S0008-8846(01)00665-2 ↗
23. 10.1016/S0958-9465(99)00031-110.1016/S0958-9465(99)00031-1 ↗
24. Air-void stability in self-consolidating concrete
25. Influence of anti-foaming admixture and polycarboxylic superplasticizer type on fresh and hardened properties of self-compacting mortar
26. 10.1016/j.conbuildmat.2011.12.10710.1016/j.conbuildmat.2011.12.107 ↗
27. 10.1016/j.conbuildmat.2012.11.03210.1016/j.conbuildmat.2012.11.032 ↗
28. 10.3846/13923730.2012.65741010.3846/13923730.2012.657410 ↗
29. 10.1016/0008-8846(86)90110-910.1016/0008-8846(86)90110-9 ↗
30. Meyer F. (1998). “Air void distribution in concrete for the great belt link West Bridge.” Nordic Concrete Research 17.
31. Origin, evolution, and effects of the air void system in concrete. Part 4—The air void system and job concrete
32. Mosquet M. · 2003 · 21
33. 10.1016/0008-8846(85)90113-910.1016/0008-8846(85)90113-9 ↗
34. Philleo R. E. · 1987 · 819
35. Pigeon M. · 1994 · 141
36. 10.1016/0950-0618(95)00067-410.1016/0950-0618(95)00067-4 ↗
37. Pinto R. C. A. and Hover K. C. (2001). “Frost and scaling resistance of high-strength concrete.” PCA Research and Development Bulletin RD122 Portland Cement Association Skokie IL 74.
38. 10.1016/0008-8846(85)90044-410.1016/0008-8846(85)90044-4 ↗
39. Rougeau P. Maillard J. L. and Mary-Dippe C. (1999). “Comparative study on properties of self-compacting and high performance concrete used in precast construction.” Proc. 1st Int. RILEM Symp. on Self-Compacting Concrete (PRO 7) 251–261.
40. 10.1016/j.cemconres.2006.08.00310.1016/j.cemconres.2006.08.003 ↗
41. Schell H. and Konecny J. (2003). “Development of an end-results specification for air void parameters of hardened concrete in Ontario’s highway structures.” 82nd Annual Meeting Transportation Research Board Washington DC.
42. Siebel E. (1989). “Air-void characteristics and freezing and thawing resistance of superplasticized air-entrained concrete with high workability.” Proc. 3rd CANMET/ACI Int. Conf. on Superplasticizers and Other Chemical Admixtures in Concrete V. M. Malhotra ed. American Concrete Institute Detroit 297–319.
43. Stark D. (1989). “Effect of length of freezing period on durability of concrete.” Research and Development Bulletin No. RD096.01 T Portland Cement Association Skokie IL 9.
44. The increase of air-content in mix under influence of carboxylate superplasticizers acting
45. The increase of air-content in SCC mixes under the influence of carboxylate superplasticizers
46. 10.3846/1392-3730.2009.15.137-14710.3846/1392-3730.2009.15.137-147 ↗
47. Taylor C. P. Kosmatka S. H. and Voigt G. F. (2006). “Integrated materials and construction practices for concrete pavement: A state-of-the-practice manual.” FHWA-HIF-07-004 Federal Highway Administration Washington DC.
48. Thomas D. A. and Wilson L. (2002). “Admixtures for use in concrete.” CD-ROM CD039 Portland Cement Association Skokie IL.
49. 10.1680/macr.2011.63.8.58310.1680/macr.2011.63.8.583 ↗
50. Wang K. Lomboy G. and Steffes R. (2009). “Investigation into freezing-thawing durability of low-permeability concrete with and without air entraining agent.” Final Rep. National Concrete Pavement Technology Center 50.
51. 10.4028/www.scientific.net/AMR.687.15510.4028/www.scientific.net/AMR.687.155 ↗
52. Whiting D. and Dziedzic D. (1992). “Effects of conventional and high-range water reducers on concrete properties.” Research and Development Bulletin RD107 Portland Cement Association Skokie IL 28.
53. 10.1007/s11595-007-3303-710.1007/s11595-007-3303-7 ↗