Abstract

Compared to conventional hot-applied asphalt sealant, the new cold-applied crack seal bands have outstanding advantages such as high installation efficiency, fewer secondary failures, and more environmentally friendly. However, some new failure modes happen during field application. Based on field investigation and laboratory testing, the short-term and long-term failure modes of seal bands were identified in this study. The laboratory testing methods were then developed to evaluate the short-term or premature failures and explore the causes of the short-term failures of installation failure or bending, unevenness, and stripping. The strategies to prevent and reduce the short-term failures of crack sealing bands were recommended regarding material selection and construction control.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Asphalt Pavement Performance Evaluation · Infrastructure Maintenance and Monitoring · Transport Systems and Technology

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Associate Professor, Key Laboratory of Road Structure and Material, Research Institute of Highway, Ministry of Transport, Beijing 100088, China.

Professor, Key Laboratory of Road and Traffic Engineering of the Ministry of Education, Tongji Univ., Shanghai 201804, China; and Research Scientist, Dept. Civil and Environmental Engineering, University of California Pavement Research Center, Univ. of California Davis, 1 Shields Ave., Davis, CA 95616 (corresponding author).

References (24)

Show source-provided references
1. Development of a viscosity specification for hot-poured bituminous sealants10.1520/JTE100260 ↗
2. Al-Qadi I. L. Loulizi A. Aref S. Masson J. F. and MeGhee K. M. (2005). “Modification of bending beam rheometer specimen for low-temperature evaluation of bituminous crack sealants.” Transportation Research Record 1933 Transportation Research Board Washington DC 97–106.10.1177/0361198105193300111 ↗
3. ASTM. (1995). “Standard specification for crack filler hot-applied for asphalt concrete and Portland cement concrete pavements.” ASTM D5078-95 West Conshohocken PA.
4. ASTM. (2002a). “Standard test methods for cone penetration of lubricating grease.” ASTM D217-02 West Conshohocken PA.
5. ASTM. (2002b). “Standard test methods for vulcanized rubber and thermoplastic elastomers—Tension.” ASTM D412-98a West Conshohocken PA.
6. ASTM. (2004). “Standard test method for flexibility determination of hot-melt adhesives by Mandrel bend test method.” ASTM D3111-2004 West Conshohocken PA.
7. ASTM. (2006). “Standard test method for softening point of bitumen (ring-and-ball apparatus).” ASTM D36-06 West Conshohocken PA.
8. ASTM. (2007). “Standard test method for thickness of textile materials.” ASTM D1777-96 West Conshohocken PA.
9. ASTM. (2009). “Standard test methods for sealants and fillers hot-applied for joints and cracks in asphaltic and Portland cement concrete pavements.” ASTM D5329-09 West Conshohocken PA.
10. ASTM. (2012). “Standard specification for joint and crack sealants hot-applied for concrete and asphalt pavements.” ASTM D6690-12 West Conshohocken PA.
11. China Ministry of Transport of China. (2011). “Standard test methods of bitumen and bituminous mixtures for highway engineering.” China Communications Press Beijing.
12. China National Development and Reform Commission of China. (2005). “Modified bituminous waterproofing for road and bridge.” China Communications Press Beijing.
13. Crafco I. (2009). “Product data sheet of Paveprep.” Chandler AZ.
14. Crafco I. (2010). “Product data sheet and installation instructions of Qwikseal.” Chandler AZ.
15. 10.1061/(ASCE)MT.1943-5533.000022210.1061/(ASCE)MT.1943-5533.0000222 ↗
16. Galehouse L. King H. Leach D. R. Moulthrop J. and Bill B. (2005). “Preventive maintenance treatment performance at 14 years.” 92nd Annual Meeting Compendium Transportation Research Board Washington DC.
17. General Administration of Quality Supervision and China. (2007). “Test methods building sheets for waterproofing.” China Standard Press Inspection and Quarantine of China Standardization Administration of China Beijing.
18. General Administration of Quality Supervision and China. (2008). “Paints and varnishes—Standard panels for testing.” China Standard Press Inspection and Quarantine of China Standardization Administration of China Beijing.
19. A new laboratory evaluation method for the adhesive performance of crack sealants
20. Low-temperature stress relaxation evaluation index of asphalt pavement crack sealants
21. 10.1520/JTE2013019610.1520/JTE20130196 ↗
22. Peshkin D. Smith K. L. Wolters A. Moulthrop J. and Alvarado C. (2011). “Guidelines for the preservation of high-traffic-volume roadways.” Transportation Research Board Washington DC.10.17226/14487 ↗
23. 10.1061/(ASCE)0899-1561(2009)21:11(688)10.1061/(ASCE)0899-1561(2009)21:11(688) ↗
24. 10.1061/(ASCE)0899-1561(2008)20:7(470)10.1061/(ASCE)0899-1561(2008)20:7(470) ↗