Microstructure Evolution and Corrosion Mechanisms of Q370qD Steel Following Different Heat Treatments
Source abstract
Abstract
Bridge steel, frequently employed in cross-sea bridge construction, exhibits excellent weldability, superior strength, and toughness. The service life and stability of steel structures are influenced by the presence of corrosive ions within marine environments, necessitating an in-depth examination of the corrosion mechanisms affecting bridge steel. In this study, Q370qD bridge steel was subjected to heat treatment to evaluate the influence of microstructural variations on its corrosion behavior. The microstructure of untreated steel (alloy F) predominantly consists of granular ferrite. Subsequent high-temperature heat treatment induces a partial transformation in the steel microstructure (alloy A), yielding lath carbide-free bainite. Post-immersion tests show both alloy surfaces densely covered with γ-FeOOH, α-FeOOH, and a mixture of Fe3O4 and Fe2O3. Over time, γ-FeOOH undergoes partial conversion into the more stable α-FeOOH form, enhancing the protective barrier against the matrix for both alloys. Alloy F exhibits a significant reduction in corrosion rate compared to alloy A. The proportion of α-FeOOH in alloy A initially decreases then increases with prolonged exposure, while in alloy F, it consistently rises. The corrosion resistance of alloy A surpasses that of alloy F, which is attributed to the lath-shaped carbide-free bainite’s effectiveness in obstructing Cl− penetration and thereby improving corrosion resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Changsha Univ. of Science and Technology
Heriot-Watt Univ.
References (32)
Show source-provided references
1. 10.1016/j.jreng.2023.01.00310.1016/j.jreng.2023.01.003 ↗
2. 10.1016/j.msea.2019.03.02710.1016/j.msea.2019.03.027 ↗
3. 10.1016/j.corsci.2014.12.00210.1016/j.corsci.2014.12.002 ↗
4. 10.1016/j.msea.2022.14400210.1016/j.msea.2022.144002 ↗
5. 10.1016/j.scriptamat.2019.04.01910.1016/j.scriptamat.2019.04.019 ↗
6. 10.1061/(ASCE)MT.1943-5533.000304010.1061/(ASCE)MT.1943-5533.0003040 ↗
7. 10.1016/j.conbuildmat.2018.12.13010.1016/j.conbuildmat.2018.12.130 ↗
8. Jiao, S. F., Y. Z. Yin, J. L. Liang, Z. F. Shi, and C. X. Cai. 2013. “Simulation study on steel corrosion in marine environment.” [In Chinese] Technol. Dev. Chem. Ind. 42(8): 48–50. https://doi.org/10.3969/j.issn.1671-9905.2013.08.015.
9. 10.1016/j.matlet.2022.13334410.1016/j.matlet.2022.133344 ↗
10. Li, S. P., J.. Guo, S. W. Yang, and X. L. He. 2008. “Effect of carbon content and microstructure on the corrosion resistance of low alloy steels.” [In Chinese] J. Vac. Sci. Technol., B 30 (1): 16–20. https://doi.org/10.13374/j.issn1001-053x.2008.01.017.
11. 10.1016/j.conbuildmat.2019.11756610.1016/j.conbuildmat.2019.117566 ↗
12. Liu, X. H., and J. R. Zhang. 2019. “Experimental study on effect of corrosion on flexural load-carrying capacity of Q550E high-performance steel girder [In Chinese] China J. Highway Transp. 32(11): 184–191. https://doi.org/10.19721/j.cnki.1001-7372.2019.11.018.
13. 10.1016/j.jmrt.2023.07.22710.1016/j.jmrt.2023.07.227 ↗
14. 10.3390/met1308140210.3390/met13081402 ↗
15. 10.1016/j.conbuildmat.2017.06.16910.1016/j.conbuildmat.2017.06.169 ↗
16. Peng, J. X., Y. Chai, and J. R. Zhang. 2023. “Summarization of reliability theory for condition assessment of bridge structures.” [In Chinese.] J. China Foreign Highway 43(4): 1–7. https://doi.org/10.14048/j.issn.1671-2579.2023.04.001.
17. 10.1016/j.jmst.2020.12.01410.1016/j.jmst.2020.12.014 ↗
18. Tian, X., X. Liu, F. Pei, L. L. Jia, C. F. Li, C. X. Deng, and Z. M. Li. 2020. “Study on initial corrosion behavior of galvanized steel in simulated atmospheric corrosion environment.” [In Chinese] Appl. Chem. Ind. 49(02): 406–409. https://doi.org/10.16581/j.cnki.issn1671-3206.20191111.027.
19. 10.1016/j.matdes.2015.06.10910.1016/j.matdes.2015.06.109 ↗
20. Wang, Z. F., P. H. Li, Y. Guan, and Q. F. Chen. 2008. Corrosion resistance of weather-resisting steel 09CuPCrNi and ultra low carbon bainitic steel (ULCB). [In Chinese] Spec. Steel 29 (2): 31–33. https://doi.org/10.3969/j.issn.1003-8620.2008.02.012.
21. 10.5006/183710.5006/1837 ↗
22. 10.1016/j.conbuildmat.2023.13234210.1016/j.conbuildmat.2023.132342 ↗
23. 10.1016/j.corsci.2021.10935310.1016/j.corsci.2021.109353 ↗
24. Wu, Y. J., S. B. Zhou, and K. M. Wu. 2019. “Low temperature transformation microstructure and properties of high carbon bainitic steel.” [In Chinese] J. Iron Steel Res. 31 (12): 1058–1064. https://doi.org/10.13228/j.boyuan.issn1001-0963.20190099.
25. 10.1007/s13296-014-1214-y10.1007/s13296-014-1214-y ↗
26. 10.1177/136943321876089110.1177/1369433218760891 ↗
27. 10.1016/j.corsci.2012.07.01810.1016/j.corsci.2012.07.018 ↗
28. Zhang, D. D., Z. Y. Wang, C. Y. Zhao, and G. W. Cao. 2015a. “Atmospheric corrosion behavior of Q345 steel in a simulated acidic marine aerosols environment.” [In Chinese] J. Chin. Soc. Corros. Prot. 35 (4): 326–332. https://doi.org/10.11902/1005.4537.2014.16.
29. 10.1016/j.corsci.2018.04.04110.1016/j.corsci.2018.04.041 ↗
30. 10.1016/j.jallcom.2014.10.17710.1016/j.jallcom.2014.10.177 ↗
31. 10.1016/S1003-6326(16)64232-210.1016/S1003-6326(16)64232-2 ↗
32. 10.1016/j.msea.2017.09.07810.1016/j.msea.2017.09.078 ↗