article·2006-02-20

Abrasive wear resistance of boronized carbon and low-alloy steels

M.A. Béjar, Eduardo Araya Moreno

Publisher page

Abstract

Abstract In this study, the abrasive wear resistance of previously boronized 1020, 1045, 4140 and 4340 steels were determined. The boronizing treatments were performed in a mixture of dried borax and SiC at temperatures of 1223, 1273 and 1323 K, during 2, 4 and 8 h. On the surface of each steel, a monophase layer of Fe 2 B was obtained. The abrasive wear tests were performed by using a rubber-wheel apparatus (ASTM-G65 standard) operating with quartz sand and a force between wheel and specimen of 130 N. As a result, boronized 1020 steel exhibited the greatest abrasive wear resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.