article·2024-07-25

Effect of process parameters on the texture evolution of Fe-6.5 wt% Si soft magnetic alloys manufactured via laser powder bed fusion

Hansol Lee, Youngsin Choi, Jonghyuk Ahn, Kwiyoung Lee, Yerim Kim, Yerim Kim, Joonphil Choi, Haksung Lee, Jongryoul Kim

Publisher page

Abstract

Numerous attempts have been made to manufacture high-Si steels using a laser powder bed fusion process. It has been established that controlling texture is critical to enhancing their magnetic properties. In this study, a comprehensive analysis was conducted to ascertain the texture evolution in Fe-Si alloys under various laser powers ( P) and scanning speeds ( V). The analysis revealed that texture formation in the fusion process is primarily influenced by two factors: P / V , the line energy density, and P / V , associated with enthalpy. Both the melt-pool sizes and the threshold value for the transition in melting mode were effectively characterized by the P / V term, while the P / V term proved essential for texture development under the same melting mode. In keyhole mode, an increase in P / V led to a transition from the {001}<100> to the {111}<1−10> texture. In conduction mode, an increase in P / V led to a transition from the {001}<100> to the {001}<110> texture, along with the development of a strong θ-fiber texture at intermediate P / V values. Furthermore, by examining the mechanisms behind the development of these textures, potential conditions for the development of a strong Goss texture were identified. Finally, significant improvements in magnetic properties were achieved through texture optimization.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.