Interface strengthened brazing of carbon/carbon composite and GH3044 alloy via inserting W fibers
Source abstract
Abstract
The poor joining strength at the C/C/interlayer interface is a tricky problem that results in low joint strength in C/C-to-metal joining. Aiming at this problem, an interface strengthened brazing process based on inserting high-strength tungsten (W) fibers on the joining interface was proposed to join C/C composite and GH3044 alloy. Microstructures, room-temperature (RT) shear strength and three-point bending strength of the joints were investigated, and the effects of process parameters on the joint microstructures and RT shear strength were discussed. The results show that by using BNi2 powder filler, the joints with high-strength W fibers crossing the C/C/interlayer joining interface were obtained. Cr 3C 2 compound was formed near the C/C substate, and Ni 4W+NiW mixed phases were formed around the W fibers. The interlayer was mainly consisted of two phases: Ni 3 Si compound and Ni-based solid solution. Because of the inserting of W fibers, not only the joining area was increased but also the crack propagation was effectively hindered. Therefore, the joints showed good shear strength and bending strength. Under the optimized process conditions (i.e., brazing temperature 1050 °C, holding time 30 min, fiber-inserting density 64 cm −2, and fiber-inserting depth 3.0 mm), the highest RT shear strength, 600 °C shear strength, and three-point bending strength of the joint reached 72.2 MPa, 40.6 MPa, and 34.5 MPa, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.