article·2002-12-01

Brazeability of cold rolled three layer Al–7.5Si/Al–1.2Mn–2Zn–(0.04–1.0)Si/Al–7.5Si (wt.%) clad sheets

Jea-Sung Ryu, Mok‐Soon Kim, Dongsoo Jung

Publisher page

Abstract

Abstract The effect of silicon content in the core alloy on the brazeability of three layer aluminium clad sheets was investigated using the clad sheets composed of Al–7.5 wt.% Si alloy (filler, thickness: 10 μm)/Al–1.2 wt.% Mn–2 wt.% Zn based alloy containing 0.04–1.05 wt.% Si (core, 80 μm)/Al–7.5 wt.% Si alloy (filler, thickness: 10 μm). It was revealed that the clad sheets with 0.04–0.64 wt.% Si core have an excellent sagging resistance (brazeability) with a limited erosion owing to the formation of a coarsely recrystallized grain structure in the core during brazing. In contrast, if the Si content in the core increased to about 1%, the sagging resistance of the clad sheets decreased with severe erosion due to an incomplete recrystallization of the core during brazing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.