Effect of V addition on activation performances of TiMn1.25Cr0.25 hydrogen storage alloy
Source abstract
Abstract
Abstract Effect of V substitution for partial Mn on activation performances of TiMn1.25Cr0.25 alloy was investigated. It was found that both TiMn1.25Cr0.25 and TiMn0.95V0.3Cr0.25 alloy samples can be activated with easy at moderate activation conditions if without exposure to air before activation. After exposed to air for 30 days, TiMn0.95V0.3Cr0.25 alloy still can be fully activated through five activation cycles. However, there is hardly any hydrogen absorption for TiMn1.25Cr0.25 alloy even after 10 activation cycles. SEM results exhibit that the activation process of TiMn0.95V0.3Cr0.25 and TiMn1.25Cr0.25 alloys is closely related with alloy particle fragmentation. Improved activation characteristics of TiMn0.95V0.3Cr0.25 alloy could be resulted from the decreasing surface oxide layer, changed Ti/Mn ratio on alloy top surface and the increasing lattice parameters.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Catalysis and Hydrodesulfurization Studies · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.