Abstract
Sequential deposition of Pd/AuGe/Ag/Au and rapid thermal annealing at 450 to 550 °C were employed to form a shallow ohmic contact to n–Alx Ga1−x As. Contact resistivity was in the range of (0.7–1) × 10−5 at x = 0.3 to (2–4) × 10−5 ohm-cm2 at x = 0.55. Limited interfacial reaction was verified by ion backscattering and x-ray diffraction techniques and attributed to the stability of Au–Ag solid solutions against underlying substrates. Contacts form at 450 to 500 °C, possibly via solid-state reaction, whereas liquid phase reaction may take place at 550 °C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Molecular Junctions and Nanostructures · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. 10.1557/JMR.1988.091410.1557/JMR.1988.0914 ↗
2. 10.1016/0038-1101(72)90037-810.1016/0038-1101(72)90037-8 ↗
3. Hansen · 195810.1149/1.2428700 ↗
4. Nagata · IEEE Trans. Electron Devices ED-35 · 1988 · 2
5. 10.1557/JMR.1987.026210.1557/JMR.1987.0262 ↗
6. Zheng · Appl. Phys. Lett. · 1992 · 60
7. Chen · J. Vac. Sci. Technol. · 1987 · B5
8. 10.1016/0040-6090(82)90517-X10.1016/0040-6090(82)90517-X ↗
9. 10.1016/0038-1101(86)90037-710.1016/0038-1101(86)90037-7 ↗
10. 10.1016/0040-6090(86)90113-610.1016/0040-6090(86)90113-6 ↗
11. 10.1063/1.33433010.1063/1.334330 ↗
12. 10.1063/1.35091210.1063/1.350912 ↗
13. 10.1063/1.33741310.1063/1.337413 ↗
14. Langer · J. Vac. Sci. Technol. · 1987 · B5
15. Tiwari · IEEE Electron Device Lett. EDL-8 · 1987 · 417
16. 10.1016/0304-3991(84)90118-910.1016/0304-3991(84)90118-9 ↗
17. 10.1063/1.10087210.1063/1.100872 ↗
18. 10.1063/1.33608510.1063/1.336085 ↗
19. 10.1063/1.33970510.1063/1.339705 ↗
20. Borzone · Metall. Trans. · 1989 · 20A