journal article·2014-11-28

Experimental investigation on HCF strength affected by predamage from LCF of a near alpha titanium alloy

Huang Jia, Luo Yinyin, Shi Duoqi, Yang Xiaoguang, Yu Huichen, Zhao Pengtao

Journal of Materials Research· Volume 29· Issue 22
Publisher page

Abstract

The feasibility of an accelerated test method on revealing the high cycle fatigue (HCF) limit stresses of a near alpha titanium alloy was successfully verified firstly during the rotary bending tests. The stress-controlled low cycle fatigue (LCF) tests at room temperature were then carried out over a range of maximum stresses and stress ratios to reveal the basic LCF strength. Finally, the core emphasis was focused on the influences of the predamage from LCF loadings on the subsequent HCF limit stresses corresponding to the life of 106cycles. A total of eight levels of predamage from LCF with different stress levels, stress ratios, and proportions of LCF life were introduced, which resulted in obvious deterioration of the HCF stress limits (even under only 2% of expected LCF life). The fracture analysis exhibited that there were typical LCF failure characteristics in crack initiation regions of specimens under prior LCF loadings.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. 10.1007/BF0274753610.1007/BF02747536 ↗
2. 10.1007/BF0001267010.1007/BF00012670 ↗
3. A rapid method for generation of a Haigh diagram for high cycle fatigue
4. 10.1063/2.120310710.1063/2.1203107 ↗
5. 10.1016/S0142-1123(03)00116-610.1016/S0142-1123(03)00116-6 ↗
6. 10.1016/S0921-5093(01)01468-X10.1016/S0921-5093(01)01468-X ↗
7. 10.1016/S0921-5093(01)01742-710.1016/S0921-5093(01)01742-7 ↗
8. Fatigue crack propagation
9. 10.1016/S0142-1123(99)00074-210.1016/S0142-1123(99)00074-2 ↗
10. High cycle fatigue property of Ti-600 alloy at ambient temperature10.1016/j.jallcom.2010.10.144 ↗
11. 10.1016/j.ijfatigue.2005.07.03210.1016/j.ijfatigue.2005.07.032 ↗
12. Fatigue properties of titanium alloy TA11 under multiaxial loadings with tension-bending vibration
13. Effect of microstructural morphology on the mechanical properties of titanium alloys
14. 10.1016/0956-7151(92)90146-610.1016/0956-7151(92)90146-6 ↗
15. 10.1046/j.1460-2695.1999.00194.x10.1046/j.1460-2695.1999.00194.x ↗
16. 2002 · 3 · 847
17. 10.1016/j.jnucmat.2010.03.01410.1016/j.jnucmat.2010.03.014 ↗
18. 10.1016/j.msea.2009.09.01210.1016/j.msea.2009.09.012 ↗