journal article·2023-07Open access

Research status and development prospect of Fe–Mn–C–Al system low-density steels

Shao-bin Bai, Yong-an Chen, Xin Liu, Hui-hu Lu, Pei-kang Bai, Da-zhao Li, Zhi-quan Huang, Jing-yang Li

Abstract

The rapid development of automotive industry results in a series of increasingly serious problems such as energy consumption and environmental pollution, so that developing the automotive steels with high-strength and low-density is of great significance for energy conservation and emission reduction. Recently, Fe–Mn–C–Al system steel is favored by numerous researchers because of its low density and excellent combination of strength and ductility. However, too much Al addition inevitably triggers various changes of microstructure, deformation mechanism, and mechanical properties. In this paper, the composition design, production process, strengthening and strain hardening mechanism, and microstructure evolution are systematically expounded. The discussion mainly focuses on various strengthening (solid solution strengthening, grain refinement strengthening and precipitation strengthening) and strain hardening mechanisms (phase transformation-induced-plasticity (TRIP), twinning-induced-plasticity (TWIP), microband-induced-plasticity (MBIP), shear-band-induced-plasticity (SIP) and dynamic slip band refinement (DSBR), etc.). Also, the existing problems and future challenges in Fe–Mn–Al–C low-density steels are pointed out via analyzing the service performance (cryogenic performance, impact toughness, fatigue performance, hydrogen embrittlement, wear performance, and tensile properties). Finally, we look forward to the future development direction of Fe–Mn–Al–C low-density steels and provide the valuable ideas.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Korter · Eisenhuettenw · 1933 · 7 · 365
2. Ham · Prod Eng · 1958 · 52–59
3. The study of work hardening in Fe-Mn-Al-C alloys10.1007/BF01174510 ↗
4. Evidence of strain-induced martensitic transformation in Fe-Mn-Al austenitic alloy steels at room temperature10.1016/0956-716X(91)90096-J ↗
5. Composition and temperature dependence of tensile properties of austenitic Fe-Mn-Al-C alloys10.1016/0921-5093(89)90844-7 ↗
6. Physical and mechanical properties of irpn-aluminium-(Mn, Si) lightweight steels10.1051/metal:2000110 ↗
7. Alloy design, combinatorial synthesis, and microstructure–property relations for low-density Fe-Mn-Al-C austenitic steels10.1007/s11837-014-1032-x ↗
8. Microstructure and tensile behavior of duplex low-density steel containing 5 mass% aluminum10.1016/j.scriptamat.2012.09.030 ↗
9. Rapid alloy prototyping: compositional and thermo-mechanical high throughput bulk combinatorial design of structural materials based on the example of 30Mn-1.2C-xAl triplex steel10.1016/j.actamat.2012.05.017 ↗
10. Strain rate effects on tensile deformation behaviors for Fe-22Mn-0.6C-(1.5Al) twinning-induced plasticity steel10.1016/j.msea.2018.06.037 ↗
11. Mechanical properties of an Fe-30Mn-4Si-2Al alloy after rolling at different temperatures ranging from 298–1073 K
12. The effects of age hardening on tribological behavior of lightweight Fe-Mn-Al-C steel10.1007/s11665-021-05767-4 ↗
13. An atom probe study of kappa carbide precipitation and the effect of silicon addition10.1007/s11661-014-2187-3 ↗
14. Influence of silicon in low density Fe-Mn-Al-C steel10.1007/s11661-012-1149-x ↗
15. Crystallographic texture evolution and martensite transformation in the strain hardening process of a ferrite-based low density steel10.1016/j.jmst.2020.11.034 ↗
16. Multistage strain hardening through dislocation substructure and twinning in a high strength and ductile weight-reduced Fe-Mn-Al-C steel10.1016/j.actamat.2012.07.018 ↗
17. Ultrahigh strength-high ductility 1 GPa low density austenitic steel with ordered precipitation strengthening phase and dynamic slip band refinement10.1016/j.msea.2022.142829 ↗
18. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
19. Fe-Al-Mn-C lightweight structural alloys: a review on the microstructures and mechanical properties10.1088/1468-6996/14/1/014205 ↗
20. A literature review of age hardening Fe-Mn-Al-C alloys
21. Effect of niobium addition on microstructure and mechanical properties of Fe-7Al-0.35C low-density steel10.1007/s13632-020-00622-9 ↗
22. Strengthening and strain hardening mechanisms in a precipitation-hardened high-Mn lightweight steel10.1016/j.actamat.2017.08.049 ↗
23. Effect of alloying chemistry on the lattice constant of austenitic Fe-Mn-Al-C alloys10.1016/0956-716X(94)90611-4 ↗
24. Fe-Mn-C-Al low-density steel for structural materials: a review of alloying, heat treatment, microstructure, and mechanical properties10.1002/srin.202200191 ↗
25. Effects of Al on microstructure and tensile properties of C-bearing high Mn TWIP steel10.1016/j.actamat.2011.12.004 ↗
26. Austenite-Based Fe-Mn-Al-C ligntweight steels: research and prospective10.3390/met12101572 ↗
27. Deformation behavior of iron-rich iron-aluminum alloy at low temperatures10.1016/S1359-6454(03)00089-2 ↗
28. A remarkable improvement of low-cycle fatigue resistance of high-Mn austenitic TWIP alloys with similar tensile properties: importance of slip mode10.1016/j.actamat.2016.07.034 ↗
29. A general perspective of Fe-Mn-Al-C steels10.1007/s10853-018-2551-6 ↗
30. Strain hardening during hot compression through planar dislocation and twin-like structure in a low-density high-Mn steel10.1007/s11665-014-1168-4 ↗
31. Microstructures and mechanical properties of Fe3Al-based Fe-Al-C alloys10.1016/j.intermet.2005.01.013 ↗
32. Combined atom probe tomography and density functional theory investigation of the Al off-stoichiometry of κ-carbide in an austenitic Fe-Mn-Al-C low density steel10.1016/j.actamat.2016.01.007 ↗
33. Synergistic strengthening effect induced ultrahigh yield strength in lightweight Fe-30Mn-11Al-1.2C steel10.1016/j.msea.2019.03.006 ↗
34. Investigations of the microstructure evolution and tensile deformation behavior of austenite Fe-Mn-Al-C lightweight steels and the effect of Mo addition10.1016/j.actamat.2018.01.051 ↗
35. High strength and ductile low density austenitic Fe-Mn-Al-C steels: simplex and alloys strengthened by nanoscale ordered carbides10.1179/1743284714Y.0000000515 ↗
36. Low density steels encyclopedia of materials
37. Dynamic recrystallization mechanisms of an Fe-8% Al low density steel under hot rolling conditions10.1016/j.scriptamat.2012.07.037 ↗
38. Low density Fe-Mn-Al-C steels: phase structures, mechanisms and properties10.2355/isijinternational.ISIJINT-2020-467 ↗
39. The effect of silicon content on the dynamic fracture toughness of high manganese and aluminum steels10.1007/s11837-014-1068-y ↗
40. Phase transformations of a Fe-0.85C-17.9Mn-7.1Al austenitic steel after quenching and annealing10.1007/s11837-014-1088-7 ↗
41. Low-density low-carbon Fe-Al ferritic steels10.1016/j.scriptamat.2012.10.004 ↗
42. Direct evidence for the formation of ordered carbides in a ferrite-based low-density Fe-Mn-Al-C alloy studied by transmission electron microscopy and atom probe tomography10.1016/j.scriptamat.2012.08.013 ↗
43. Impact of short-range ordering on yield strength of high manganese austenitic steels10.1016/j.msea.2014.07.016 ↗
44. A literature review of age hardening Fe-Mn-Al-C alloys
45. Ferrite effects in Fe-Mn-Al-C triplex steels10.1007/s11661-013-1990-6 ↗
46. Nano-mechanical properties of Fe-Mn-Al-C lightweight steels10.1038/s41598-018-27345-w ↗
47. Application of texture analysis for optimizing thermo-mechanical treatment of a high Mn TWIP steel10.4028/www.scientific.net/AMR.922.213 ↗
48. Designing duplex, ultrafine-grained Fe-Mn-Al-C steels by tuning phase transformation and recrystallization kinetics10.1016/j.actamat.2017.09.026 ↗
49. Ultrastrong and ductile austenitic lightweight steel via ultra-fine grains and heterogeneous B2 precipitates10.1016/j.msea.2022.144330 ↗
50. Aging hardening response and β-Mn transformation behavior of high carbon high manganese austenitic low-density Fe-30Mn-10Al-2C steel
51. Microstructural evolution and tensile properties of Fe-11Mn-10Al-1.2C medium-Mn lightweight steel10.1016/j.msea.2020.140256 ↗
52. Effect of cold rolling and subsequent heat treatment on microstructural evolution and mechanical properties of Fe-Mn-Al-C-(Ni) based austenitic low-density steels
53. Improvement of strength-ductility balance of B2-strengthened lightweight steel10.1016/j.actamat.2020.03.022 ↗
54. Effect of early stage of κ-carbides precipitation on tensile properties and deformation mechanism in high Mn-Al-C austenitic low-density steel10.1016/j.msea.2022.144132 ↗
55. A feasible route to produce 1.1 GPa ferritic-based low-Mn lightweight steels with ductility of 47%10.1016/j.jmst.2021.11.052 ↗
56. Development of oxidation resistant Fe-Mn-Al-C alloys
57. Effect of Nb on the microstructure and properties of Ti-Mo microalloyed high-strength ferritic steel10.1016/j.msea.2018.08.092 ↗
58. The effect of vanadium micro-alloying on the microstructure and the tensile behavior of TWIP steel10.1016/j.msea.2017.04.083 ↗
59. Effects of Nb and C additions on the microstructure and tensile properties of lightweight ferritic Fe-8Al-5Mn alloy10.1016/j.scriptamat.2014.06.018 ↗
60. κ-phase formation in Fe-Mn-Al-C austenitic steels10.1002/srin.201400587 ↗
61. Phase transformation of the L12 to kappa-carbide after spinodal decomposition and ordering in an Fe-C-Mn-Al austenitic steel10.1016/j.msea.2015.06.096 ↗
62. β-Mn formation and aging effect on the fracture behavior high-Mn low-density steels10.1016/j.scriptamat.2016.04.040 ↗
63. Modulated structure and magnetic properties of age-hardenable Fe-Mn-Al-C alloys10.1007/BF02656419 ↗
64. Experimental determination of phase equilibria in the Fe-Al-C system10.1016/0966-9795(95)00003-H ↗
65. High manganese and aluminum steels for the military and transportation industry10.1007/s11837-014-1068-y ↗
66. Tensile deformation of low density duplex Fe-Mn-Al-C steel10.1016/j.matdes.2015.03.043 ↗
67. Phase transformation of an Fe-0.85C-17.9Mn-7.1Al austenitic steel after quenching and annealing10.1007/s11837-014-1088-7 ↗
68. Effect of annealing treatment on microstructures and properties of austenite-based Fe-28Mn-9Al-0.8C lightweight steel with addition of Cu10.1007/s41230-021-1026-6 ↗
69. An assessment of the entire Al-Fe system including DO3 ordering10.1016/j.actamat.2009.02.046 ↗
70. Grain boundary precipitation behaviors in an Fe-9.8Al-28.6Mn-0.8Si-1.0C alloy10.1016/1359-6462(95)00485-8 ↗
71. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility
72. Strain hardening in Fe-16Mn-10Al-0.86C-5Ni high specific strength steel10.1016/j.actamat.2016.02.044 ↗
73. Strain hardening of novel high Al low-density steel consisting of austenite matrix and B2-ordered intermetallic second phase in the perspective of non-cell forming face-cen-tered-cubic alloy with high stacking fault energy10.1016/j.scriptamat.2018.09.044 ↗
74. Effect of annealing temperature on microstructural modification and tensile properties in 0.35C-3.5Mn-5.8Al lightweight steel10.1016/j.actamat.2013.04.038 ↗
75. Novel ultra-high-strength Cu-containing medium-Mn duplex steels10.1016/j.actamat.2017.06.035 ↗
76. Solution-dislocation interactions and creep-enhanced Cu precipitation in a novel ferrite-martensitic steel10.1016/j.actamat.2020.05.054 ↗
77. Study of the influence of alloying elements on Cu precipitation in steel by non-classical nucleation theory10.1016/j.actamat.2006.05.006 ↗
78. Novel ultra-high-strength Cu-containing medium-Mn duplex lightweight steels10.1016/j.actamat.2017.06.035 ↗
79. The effect of Ti-Mo-Nb on the microstructure and tensile properties of a Fe-Mn-Al-C austenitic steel10.1016/j.msea.2020.139220 ↗
80. Control of strain hardening behavior in High-Mn-austenitic steels10.1007/s40195-014-0084-9 ↗
81. Effect of hot rolling and heat treatment on structure and properties of high carbon Fe-Al alloys10.1016/S0921-5093(00)02026-8 ↗
82. Alloy design, combinatorial synthesis and microstructure-property relations for loe-density Fe-Mn-Al-C austenitic steels10.1007/s11837-014-1032-x ↗
83. Deformation behaviour of iron-rich iron-aluminium alloys at low temperatures10.1016/S1359-6454(03)00089-2 ↗
84. Stacking fault energy and plastic deformation of fully austenitic high manganese steels: effect of Al addition10.1016/j.msea.2010.02.058 ↗
85. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIP-LEX steels10.1002/srin.200606440 ↗
86. The mechanism of mechanical twinning near grain boundaries in twinning-induced plasticity steel10.1016/j.scriptamat.2019.08.025 ↗
87. Tensile deformation of low-density Fe-Mn-AL-C austenitic steels at ambient temperature10.1016/j.scriptamat.2012.09.031 ↗
88. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel10.1016/j.actamat.2016.06.037 ↗
89. Tensile deformation of a duplex Fe-20Mn-9Al-0.6C steel having the reduced specific weight10.1016/j.msea.2011.03.045 ↗
90. Microstructure evolution and strain hardening behavior during plastic deformation of Fe-12Mn-Al-0.8C steel10.1016/j.msea.2013.07.023 ↗
91. Effects of heat treatment on microstructure and tensile properties of a Fe-27Mn-12Al-0.8C low-density steel10.1007/s11837-014-1064-2 ↗
92. Tensile deformation of a duplex Fe-20Mn-9Al-0.6C steel having the reduced specific weight10.1016/j.msea.2011.03.045 ↗
93. Research progress of new automotive steel-low-density high strength-toughness steel10.1016/j.msea.2015.07.043 ↗
94. Deformation behavior of ferrite–austenite duplex lightweight Fe-Mn-Al-C steel10.1016/j.scriptamat.2011.12.026 ↗
95. Effect of deformation speed on the microstructure and mechanical properties of AA6063 during continuous extrusion process10.1016/j.jmatprotec.2013.05.006 ↗
96. Thermal stability of retained austenite in TRIP steels studied by synchrotron X-ray diffraction during cooling10.1016/j.actamat.2005.08.017 ↗
97. Deformation-induced austenite grain rotation and transformation in TRIP-assisted steel10.1016/j.actamat.2011.11.026 ↗
98. Effects of annealing treatment prior to cold rolling on the edge cracking phenomenon of ferritic lightweight steel10.1007/s11661-014-2332-z ↗
99. The relationship between austenite morphology and continuous TRIP effects in forged 4Mn steel10.1016/j.matchar.2022.112172 ↗
100. Deformation mechanisms of a novel Mn-based 1 GPa TRIP/TWIP assisted lightweight steel with 63% ductility10.1016/j.msea.2020.140658 ↗