Effect of solution treatments on microstructure and mechanical properties of Ti–6Al–4V alloy hot rolled sheet
Source abstract
Abstract
The solution and aging treatment were carried out with the hot rolled sheet Ti–6Al–4V alloy sheet, and the effects of solution treatments on the microstructure and mechanical properties were mainly studied. In the solution treatment process, α→β→βt transformation occurred. With the increase of solution treatment temperature and time, the α phase gradually changed from long strip to equiaxed morphology, and the fraction of equiaxed α and β phases gradually increased. The bimodal microstructure of αp and βt was obtained during the solution treatments. Among them, βt is mainly composed of high-density nano-needle αs with different orientations, which has a significant contribution to the strength of Ti–6Al–4V alloy. The strength of bimodal microstructure increases with the increase of βt content, but its influence on ductility is complicated. When βt content exceeds a certain amount, it is easy to lead to brittleness. It is found that when the specimens are treated at 930 °C for 60min or 960 °C for 30min, the best strength-ductility matching can be obtained. In this case, the volume fractions of αp and βt are almost equal, and the PSE of Ti–6Al–4V alloy reaches more than 14500 MPa⋅%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Quantitative analysis on boundary sliding and its accommodation mode during superplastic deformation of two-phase Ti-6Al-4V alloy10.1007/s11661-998-0174-2 ↗
2. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
3. A review on biomedical titanium alloys: recent progress and prospect
4. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
5. Hot deformation behavior of Ti-6Al-4V alloy: effect of initial microstructure10.1016/j.jallcom.2017.05.097 ↗
6. A study of the microstructure and hardness of two titanium alloys: commercially pure and Ti-6Al4V10.1016/j.jallcom.2009.06.172 ↗
7. Recent developments in flat rolling technologies, 8th pacific rim international congress on advanced materials and processing 201310.1002/9781118792148.ch266 ↗
8. High-temperature microstructural characteristics of a novel biomedical titanium alloy[J]10.1016/j.jallcom.2010.03.052 ↗
9. Effects of hydrogen loading and type of titanium hydride on grain refinement and mechanical properties of laser formed Ti-6Al-4V10.1016/j.jallcom.2014.02.171 ↗
10. EBSD study of microstructural and textural changes of hot-rolled Ti-6Al-4V sheet after annealing at 800°C10.1007/s40195-018-0768-7 ↗
11. Microstructure and texture evolution during annealing of Ti-6Al-4V alloy[J]10.1080/02670836.2019.1706816 ↗
12. Evolution of texture and tensile properties of cold-rotary swaged Ti-6Al-4V alloy seamless tubing after annealing at different temperatures
13. High tensile strength-ductility combination in cold multiaxial plane-strain forged and rolled nanostructured Titanium10.1016/j.mtla.2020.100698 ↗
14. Ti-6Al-4V alloy strengthening via instantaneous phase transformation induced by electropulsing10.1016/j.jallcom.2021.163303 ↗
15. Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V alloy through equiaxial alpha microstructure10.1016/j.scriptamat.2017.11.021 ↗
16. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
17. Achieving bi-lamellar microstructure with both high tensile strength and large ductility in Ti-6Al-4V alloy by novel thermomechanical processing
18. The formation of bimodal multilayered grain structure and its effect on the mechanical properties of powder metallurgy pure titanium10.1016/j.matdes.2016.12.004 ↗
19. Simultaneously enhanced strength and ductility of titanium via multimodal grain structure10.1016/j.scriptamat.2010.07.010 ↗
20. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
21. Influence of laser peening on microstructure and fatigue lives of Ti-6Al-4V10.1016/S1003-6326(14)63449-X ↗
22. On the influence of mechanical surface treatments-deep rolling and laser shock peening-on the fatigue behavior of Ti-6Al-4V at ambient and elevated temperatures10.1016/S0921-5093(03)00069-8 ↗
23. Factors determining room temperature mechanical properties of bimodal microstructures in Ti-6Al-4V alloy10.1016/j.msea.2018.06.019 ↗
24. Bi-lamellar microstructure in Ti-6Al-4V: microstructure evolution and mechanical properties
25. Strength enhancement of a bi-lamellar PM Ti-6Al-4V alloy without sacrificing ductility by Al partitioning and twinning-induced ductility effect10.1016/j.msea.2021.142368 ↗
26. Breaking through the strength-ductility trade-off dilemma in powder metallurgy Ti-6Al-4V alloy10.1016/j.msea.2019.03.089 ↗
27. A novel Ti-6Al-4V alloy microstructure with very high strength and good ductility[J]10.1016/j.scriptamat.2015.05.008 ↗
28. On the strain hardening abilities of α + β titanium alloys: the roles of strain partitioning and interface length density10.1016/j.jallcom.2019.152040 ↗
29. Simultaneously enhanced strength and ductility in a metastable β-Ti alloy by stress-induced hierarchical twin structure10.1016/j.scriptamat.2020.03.039 ↗
30. High strength and toughness of Ti–6Al–4V sheets via cryorolling and short-period annealing10.1016/j.msea.2022.143766 ↗
31. Deformation mechanism of bimodal microstructure in Ti-6Al-4V alloy: the effects of intercritical annealing temperature and constituent hardness
32. Microstructural influence on low-temperature super-ductility of ultrafine-grained Ti-6Al-4V alloy10.1016/j.msea.2005.08.080 ↗
33. Effect of deformation reduction on microstructure, texture, and mechanical properties of forged Ti-6Al-4V10.1007/s11665-020-05396-3 ↗
34. Hot deformation behavior, processing map, microstructure evolution and dynamic recrystallization mechanism of Mg-5Al-0.6Sc alloy
35. Stretch-flangeability correlated with hardness distribution and strain-hardenability of constituent phases in dual- and complex-phase steels
36. Effect of the martensite distribution on the strain hardening and ductile fracture behaviors in dual-phase steel10.1016/j.msea.2014.02.058 ↗
37. Investigation of the evolution of Geometrically Necessary Dislocation (GND) tensor in a type 316 steel by using In-situ EBSD technique10.1016/j.matlet.2020.129254 ↗
38. Quantifying geometrically necessary dislocation density during hot deformation in AA6082 Al alloy10.1016/j.msea.2021.141158 ↗
39. Effects of temperature and load on fretting fatigue induced geometrically necessary dislocation distribution in titanium alloy