Effect of carbonation and foam content on CO2 foamed concrete behavior
Source abstract
Abstract
Coal and electricity integration plays an important role in ensuring national energy security, but it still faces the challenge of carbon emission reduction. The development of in-situ CO2 sequestration and utilization technology for pithead power plants is an effective way to achieve low-carbon and efficient utilization of coal power. The preparation of foam concrete for mining using CO2 is a type of carbon capture, utilization, and storage technology featuring in-situ CO2 sequestration and utilization in pithead power plants and mine filling and sequestration. The purpose of this study is to evaluate the basic performance and carbon sequestration potential of Portland cement-based CO2 foam concrete (PC-CFC) as a mining material. In this study, PC-CFC was prepared through physical foaming and the carbonation pretreatment cement process. The influence of carbonation pretreatment time and CO2 foam content on density, strength, and carbon sequestration of PC-CFC was investigated. The experimental results showed that carbonation pretreatment could enhance the stability of CO2 foam in Portland cement and improve the CO2 foaming performance. With the extension of carbonation pretreatment time, the extend of dry density reduction decreases from 16.6% to 0.8%. A 60 min–90 min of carbonation pretreatment can achieve the best treatment performance. Carbonation pretreatment and CO2 foam can promote the degree of cement hydration, optimize the PC-CFC pore structure, and improve the compressive strength of PC-CFC. However, the PC-CFC material strength owing to the extended carbonation treatment time, which leads to well-developed vesicle distribution, has an overall decreasing trend. In addition, the 7 day (d) compressive strength of PC-CFC can reach more than 60% of the 28 d compressive strength, which has evident early strength characteristics. Extending the carbonation pretreatment time and CO2 foam content increased the PC-CFC carbon sequestration that ranged from 61.0 kg/ton to 85.7 kg/ton. The dry density of the PC-CFC material was significantly and positively correlated to the 28 d compressive strength and negatively correlated to the amount of carbon sequestration. In the case in which the best carbon sequestration effects is achieved, a single filling of the working face end can store ∼3929.31 kg of CO2; in the most economical condition, it can store ∼3642.79 kg of CO2. The conducted research provides new ideas for the low-carbon and green development of coal and electricity integration.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · CO2 Sequestration and Geologic Interactions · Rock Mechanics and Modeling
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Research progress of air pollutant emission from coal-fired power plants in China
2. Study on fire prevention and extinguishing technology for mined-out area by flue gas of coal mine power plant
3. Technical route selection of carbon capture, utilization and storage in coal-fired power plants
4. Prospect of carbon neutral geological technology and its application in low carbon coal
5. Effect of CO2 foaming agent on the hydration and hardening properties of OPC-CSA-FA ternary composite filling materials
6. Study on preparation and performance of calcium carbide slag foam for coal mine disaster reduction and CO2 storage10.1016/j.colsurfa.2020.125322 ↗
7. Research progress and prospect of coal-based solid waste filling mining technology
8. Development of mortar for laying and coating with pineapple fibers10.1590/1807-1929/agriambi.v24n3p187-193 ↗
9. Recycling of mine tailings for the geopolymers production: a systematic review
10. Clay ceramic waste as pozzolan constituent in cement for structural concrete10.3390/ma14112917 ↗
11. Application of plastic wastes in construction materials: a review using the concept of life-cycle assessment in the context of recent research for future perspectives10.3390/ma14133549 ↗
12. CO2 utilization via direct aqueous carbonation of synthesized concrete fines under atmospheric pressure10.1021/acsomega.0c00985 ↗
13. A review of mineral carbonation technologies to sequester CO210.1039/C4CS00035H ↗
14. Experimental study on the preparation and properties of a novel foamed concrete based on magnesium phosphate cement10.1016/j.conbuildmat.2017.01.092 ↗
15. Tian · 2018
16. Preparation and research of new sulphoaluminate cement foam concrete
17. Hu · 2018
18. Effects of surfactant on thermo-mechanical behavior of geopolymer foam paste made with sodium perborate foaming agent10.1016/j.conbuildmat.2020.118282 ↗
19. Comparative investigation of the static and dynamic properties of CO2 foam and N2 foam10.1002/cjce.22502 ↗
20. Structural and interfacial properties of the CO2-in-water foams prepared with sodium dodecyl sulfate (SDS): a molecular dynamics simulation study10.1016/j.colsurfa.2019.123615 ↗
21. Preparation and performances of foamed hydraulic lime10.1016/j.conbuildmat.2021.123244 ↗
22. Effect of foaming agent on physical and mechanical properties of alkali-activated slag foamed concrete10.1016/j.conbuildmat.2019.07.302 ↗
23. Properties and sustainability of alkali-activated slag foamed concrete10.1016/j.jclepro.2013.12.068 ↗
24. Fundamental characteristics of alkali activated slag cement foam concrete
25. Zhao · 2013 · vol. 648 · 92
26. Liu · 2019
27. Models relating mixture composition to the density and strength of foam concrete using response surface methodology10.1016/j.cemconcomp.2006.06.001 ↗
28. Investigation of carbon-capture property of foam concrete using stainless steel AOD slag10.1016/j.jclepro.2020.125621 ↗
29. Carbon dioxide fixation via accelerated carbonation of cement-based materials: potential for construction materials applications10.1016/j.conbuildmat.2018.12.078 ↗
30. Properties and applications of foamed concrete; a review10.1016/j.conbuildmat.2015.10.112 ↗
31. Characterization of pore structure of foamed concrete and its effect on mechanical properties
32. Foaming characteristics and microstructure of aerated steel slag block prepared by accelerated carbonation10.1016/j.conbuildmat.2019.03.077 ↗
33. Vaterite crystals contain two interspersed crystal structures10.1126/science.1232139 ↗
34. Bio-friendly encapsulation of superoxide dismutase into vaterite CaCO3 crystals. Enzyme activity, release mechanism, and perspectives for ophthalmology10.1016/j.colsurfb.2019.05.077 ↗
35. Diatomite-based porous ceramics with high apparent porosity: pore structure modification using calcium carbonate10.1016/j.ceramint.2018.12.082 ↗
36. Effects of Ca(OH)2 – CaCO3 concentration distribution on the pH and pore structure in natural carbonated cover concrete: a case study10.1016/j.conbuildmat.2018.08.041 ↗
37. Yuan · 2012
38. Relation between density and compressive strength of foamed concrete10.3390/ma14112967 ↗
39. Xupeng · 2019