Fe nanoparticles modified pure Ti alloy on microstructure evolution and fine crystallization mechanism fabricated by additive manufacturing

Caibao Guo, Guoqing Dai, Jingzhe Niu, Yanhua Guo, Zhonggang Sun, Hui Chang, Qitu Zhang

Abstract

It has been confirmed that micro-alloying is the effective way to refine the grain size and elevate the properties of pure Ti alloy produced via additive manufacturing. The pure Ti, Ti-2Fe (wt.%) and Ti-4Fe (wt.%) alloys created via Laser Melting Deposition (LMD) are compared based on their grain size, orientation relationship, and mechanical properties. Ti-4Fe displays a significantly lower average grain size of 220 μm in comparison to pure Ti and Ti-2Fe alloys, with average size of 442.3 and 319.6 μm. The superior constitutional supercooling of the former is responsible for the decrease in grain size. The orientation of the α phase is found to be influenced by the solid solution of Fe, with greater Fe content resulting in a preference towards the (0 0 0 1) direction for growth. Furthermore, the inclusion of Fe led to a noteworthy increase in both the yields strength, peaking at 798 MPa, and tensile strength, reaching 880 MPa. This enhancement is attributed to both the fine grain strengthening (54.4%) and the solid solution strengthening of Fe atoms (45.6%).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. The mechanism of grain refinement of titanium by silicon10.1016/j.scriptamat.2008.01.041 ↗
2. Status of the titanium production, research, and applications in the CIS10.1007/s11003-008-9079-x ↗
3. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
4. Cost-affordable, biomedical Ti-5Fe alloy developed using elemental powders and laser in-situ alloying additive manufacturing10.1016/j.matchar.2021.111526 ↗
5. Yang · 2022
6. Hao · 2016 · vol. 35
7. New beta-type Ti-Fe-Sn-Nb alloys with superior mechanical strength
8. Structure and mechanical properties of Ti–5Cr based alloy with Mo addition10.1016/j.msec.2010.04.006 ↗
9. Porous titanium implants: a review10.1002/adem.201700648 ↗
10. Liu · 2019 · 164
11. Review on manufacture by selective laser melting and properties of titanium based materials for biomedical applications10.1179/1753555715Y.0000000076 ↗
12. Additive manufacturing of metallic components–process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
13. Additive manufacturing of ultrafine-grained high-strength titanium alloys
14. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing
15. In-situ ultrafine three-dimensional quasi-continuous network microstructural TiB reinforced titanium matrix composites fabrication using laser engineered net shaping
16. Grain refinement and columnar-to-equiaxed transition of Ti6Al4V during additive manufacturing via different laser oscillations10.1016/j.ijmachtools.2023.104031 ↗
17. A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles10.1016/S1359-6454(00)00368-2 ↗
18. Improved mechanical, bio-corrosion properties and in vitro cell responses of Ti-Fe alloys as candidate dental implants
19. Microstructure evolution and grain refinement behavior during hot deformation of Fe micro-alloyed Ti-6Al-4V
20. Lütjering · 2007
21. Fujii · 2014 · vol. 106
22. Fe element promotes the transformation from columnar to equiaxed grains and the formation of ultrafine microstructure of Ti-6Al-4V alloy by laser wire deposition
23. On the influence of the heat treatment on microstructure formation and mechanical properties of near-α Ti-Fe alloys10.1016/j.msea.2018.12.071 ↗
24. Ultrafine eutectic Ti-Fe-based alloys processed by additive manufacturing – a new candidate for high temperature applications
25. Phase decomposition upon heat-treatment of a eutectoid Ti-Fe alloy processed by dual-wire-arc additive manufacturing10.1016/j.matlet.2022.132305 ↗
26. In-situ synthesis of Ti-Fe-based alloys prepared by the combination of mechanical alloying and laser melting deposition: microstructure and corrosion resistance
27. Direct fabrication of single-crystal-like structure using quasi-continuous-wave laser additive manufacturing
28. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
29. Pore elimination mechanisms during 3D printing of metals
30. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition
31. Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties10.1007/s11837-015-1297-8 ↗
32. Microstructure and mechanical properties of B modified Ti–Fe alloy manufactured by casting, forging and laser melting deposition10.1016/j.compositesb.2021.108854 ↗
33. Effect of β (110) texture intensity on α-variant selection and microstructure morphology during β→α phase transformation in near α titanium alloy10.1016/j.actamat.2016.12.069 ↗
34. Analysis of the kinetics of phase transformations10.1007/BF01105093 ↗
35. In situ characterizations of phase transformations kinetics in the Ti17 titanium alloy by electrical resistivity and high temperature synchrotron X-ray diffraction
36. Influence of cooling rate following heat treatment on microstructure and phase transformation for a two-phase alloy
37. Additive manufacturing of Ti–6Al–4V parts through laser metal deposition (LMD): process, microstructure, and mechanical properties
38. Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)
39. Effect of undercooling on microstructure evolution of Cu based alloys10.1016/j.jallcom.2022.167998 ↗
40. Effect of self-accommodation on [alpha]/[alpha] boundary populations in pure titanium10.1016/S1359-6454(03)00035-1 ↗
41. Variant selection and intervariant crystallographic planes distribution in martensite in a Ti–6Al–4V alloy
42. Dyakonov · 2019 · 123
43. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: a model for predicting their yield strength10.1016/j.scriptamat.2005.12.017 ↗
44. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition
45. A novel heterogeneous multi-wire indirect arc directed energy deposition for in-situ synthesis Al-Zn-Mg-Cu alloy: process, microstructure and mechanical properties