Microstructure and mechanical properties of Mg–Zn–Y–Mn magnesium alloys with different Zn/Y atomic ratio

Jianqiang Hao, Jinshan Zhang, Hongxia Wang, Weili Cheng, Yang Bai

Abstract

The effects of Zn/Y atomic ratio on the microstructure and mechanical properties of Mg–Zn–Y–Mn alloys were studied and analyzed using optical microscopy (OM), scanning electron microscopy (SEM), x-ray diffraction (XRD), differential scanning calorimetry (DSC), microhardness testing, high-temperature creep testing and an electronic universal testing machine. The results indicated that when Zn/Y ratio is 3:1, the alloy is mainly composed of α-Mg, I phase and W phase; when Zn/Y ratio is 1.5:1, the alloy is mainly composed of α-Mg and W phase; the alloys are all composed of α-Mg, W phase and LPSO phase when the Zn/Y ratio decreases to 1:1 or 0.8:1. With the decrease of Zn/Y ratio, the yield strength and tensile strength of alloy first increase and then decrease; the high-temperature creep resistance increases first and then decreases, and the elongation shows the trend of decreasing, increasing and then decreasing again. In total, the Mg94Zn2.5Y2.5Mn1 alloy exhibits the best mechanical properties and the best creep resistance, which is mainly related to the type and amount of the second phase.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Effects of Ti addition on the formation of LPSO phase and yield asymmetry of Mg-Zn-Y-Mn alloy10.1016/j.msea.2018.08.042 ↗
2. Strengthening Effect of extruded Mg-8Sn-2Zn-2Al Alloy: influence of micro and mano-size Mg2Sn precipitates10.3390/ma10070822 ↗
3. Effects of 14H LPSO phase on the dynamic recrystallization and work hardening behaviors of an extruded Mg-Zn-Y-Mn alloy10.1016/j.msea.2020.140727 ↗
4. Hot deformation behavior and workfability of the homogenized Mg-5.8Zn-1.2Y-1Mn alloy containing I and W phases10.1016/j.jmrt.2021.09.031 ↗
5. Effects of spheroidizing treatment on the dynamic recrystallization behavior and yield asymmetry of an extruded Mg94Zn2.5Y2.5Mn1 alloy10.1016/j.msea.2018.11.089 ↗
6. Effects of Ca on the formation of LPSO phase and mechanical properties of Mg-Zn-Y-Mn alloy10.1016/j.msea.2015.09.046 ↗
7. Effect of microalloying with boron on the microstructure and mechanical properties of Mg-Zn-Y-Mn alloy10.1016/j.msea.2016.05.095 ↗
8. A high strength and good ductility Mg-Zn-Ni-Ti alloy with long-period stacking ordered structure by hot rolling and aging treatment10.1016/j.msea.2015.09.057 ↗
9. Cottrell atmospheres along dislocations in long-period stacking ordered phases in a Mg-Zn-Y alloy10.1016/j.scriptamat.2016.02.030 ↗
10. Enhancement of strength and ductility of SiCp/AZ91 composites by RD-ECAP processing10.1016/j.msea.2019.138579 ↗
11. Influence of micro-alloying Cd on growth pattern, mechanical properties and microstruture of as-cast Mg94Y2.5Zn2.5Mn1 alloy containing LPSO structure10.1016/j.msea.2019.01.098 ↗
12. Microstructures of Mg-Zn-Zr-RE alloys with high RE and low Zn contents10.1016/0925-8388(94)91113-4 ↗
13. Rapidly solidified powder metallurgy Mg97Zn1Y2 alloys with excellent tensile yield strength above 600 MPa10.2320/matertrans.42.1172 ↗
14. The 18R and 14H long-period stacking ordered structures in Mg-Y-Zn alloys10.1016/j.actamat.2010.01.022 ↗
15. Optimum parameters and kinetic analysis for hot working of a solution-treated Mg-Zn-Y-Mn magnesium alloy10.1016/j.jallcom.2018.04.292 ↗
16. Effects of Zn/Y ratio on microstructure and mechanical properties of Mg-Zn-Y alloys10.1016/j.matlet.2005.06.052 ↗
17. Effect of mole ratio of Y to Zn on phase constituent of Mg-Zn-Zr-Y alloys10.1016/S1003-6326(11)60783-8 ↗
18. Effect of Y addition on microstructure and mechanical properties of Mg-Zn-Mn alloy10.1016/S1003-6326(14)63199-X ↗
19. The influence of element Y on the mechanical properties of the as-extruded Mg-Zn-Y-Zr alloys10.1016/j.jallcom.2006.02.035 ↗
20. Effects of phase composition and content on the microstructures and mechanical properties of high strength Mg-Y-Zn-Zr alloys10.1016/j.matdes.2015.09.087 ↗
21. Thermal diffusivity and thermal conductivity of Mg-Zn-rare earth element alloys with long-period stacking ordered phase10.1016/j.scriptamat.2008.10.022 ↗
22. Effects of Mn addition and X-phase on the microstructure and mechanical properties of high-strength Mg-Zn-Y-Mn alloys10.1016/j.msea.2013.11.043 ↗
23. Significance of stable and metastable phases in high temperature creep resistant magnesium-rare earth base alloys10.1016/j.jallcom.2003.10.099 ↗
24. Influence of Mn content on mechanical properties and fatigue behavior of extruded Mg alloys10.1016/j.msea.2006.01.091 ↗
25. Effects of Mn on the microstructure and mechanical properties of long period stacking ordered Mg95Zn2.5Y2.5 alloy10.1016/j.matlet.2013.06.112 ↗
26. Effect of rare-earth Y on microstructure and mechanical properties of as-cast Mg-2.0Zn-0.3Zr alloy
27. Effects of yttrium on microstructure and mechanical properties of hot-extruded Mg-Zn-Y-Zr alloys10.1016/j.msea.2004.02.007 ↗
28. Hot deformation and processing map of an extruded Mg-Zn-Mn-Y alloy containing I and W phases10.1016/j.matdes.2015.08.023 ↗
29. Effect of microstructure and texture on the mechanical properties of the as-extruded Mg-Zn-Y-Zr alloys10.1016/j.msea.2006.08.037 ↗
30. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy10.1016/j.actamat.2010.07.050 ↗