journal article·2022-09Open access

Suppression of Sn whisker growth from SnAgCu solder alloy with TiO2 and ZnO reinforcement nano-particles by increasing the corrosion resistance of the composite alloy

Balázs Illés, Halim Choi, Tamás Hurtony, Karel Dušek, David Bušek, Agata Skwarek

Abstract

The main joining process of the electronic industry is still soldering with different alloys of Sn. This work studied the relationship between Sn whisker growth and corrosion resistance of 99Sn0.3Ag0.7Cu–TiO2/ZnO (0.25wt%) composite solder alloys in a corrosive environment via scanning electron microscopy and focused ion beam techniques. The corrosive environment test showed that the application of TiO2 and ZnO nano-particles almost totally suppressed the Sn whisker growth and improved the corrosion resistance of the composite solder alloys compared to the reference 99Sn0.3Ag0.7Cu alloy. The microstructural analysis of the reference 99Sn0.3Ag0.7Cu solder alloy showed that the volumetric increase of the corroded β-Sn grains resulted in local mechanical stress in the solder joints, which was released by Sn whisker development. However, in the composite solder joints, the increased grain boundary fraction and segregation of the TiO2 and ZnO nano-particles to the grain boundaries resulted in a relatively uniform and compact protective oxide layer at the β-Sn grain boundaries. This suppressed the formation of SnOx, and via this, the corrosion-induced whisker growth.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Corrosion reliability of lead-free solder systems used in electronics
2. Investigating the thermomechanical properties and intermetallic layer formation of Bi micro-alloyed low-Ag content solders10.1016/j.jallcom.2015.02.092 ↗
3. Analysis of pressure-induced whisker nucleation and growth in thin Sn films10.1007/s11664-021-09158-2 ↗
4. Review on microstructure evolution in Sn–Ag–Cu solders and its effect on mechanical integrity of solder joints10.1007/s10854-013-1240-0 ↗
5. Whisker growth from Sn solder alloys
6. Tin whisker growth from micro-alloyed SAC solders in corrosive climate10.1016/j.jallcom.2014.07.103 ↗
7. Effect of current load on corrosion induced tin whisker growth from SnAgCu solder alloys10.1016/j.corsci.2015.07.026 ↗
8. Corrosion behavior, whisker growth, and electrochemical migration of Sn–3.0Ag–0.5Cu solder doping with in and Zn in NaCl solution10.1016/j.microrel.2011.06.023 ↗
9. Electrochemical migration and rapid whisker growth of Zn and Bi dopings in Sn-3.0Ag-0.5Cu solder in 3wt.% NaCl solution
10. Sn and Bi whisker growth from SAC0307-Mn07 and SAC0307-Bi1-Mn07 ultra-thin film layers10.1016/j.vacuum.2021.110121 ↗
11. Tin whisker growth on electronic assemblies soldered with Bi-containing, Pb-free alloys10.1007/s11664-020-08544-6 ↗
12. Corrosion behavior of Pb-free Sn-1Ag-0.5Cu-XNi solder alloys in 3.5% NaCl solution10.1007/s11664-012-2452-4 ↗
13. Research advances in nano-composite solders10.1016/j.microrel.2008.10.004 ↗
14. Thermal analysis and mechanical properties of Sn–1.0 Ag–0.5 Cu solder alloy after modification with SiC nano-sized particles10.1007/s10854-013-1200-8 ↗
15. Effects of Ni and TiO2 additions in as-reflowed and annealed Sn0.7Cu solders on Cu substrates10.1016/j.jmatprotec.2016.11.031 ↗
16. SAC–xTiO2 nano-reinforced lead-free solder joint charaexrizations in ultra-fine package assembly10.1108/SSMT-04-2017-0011 ↗
17. Effect of additions of ZrO2 nano-particles on the microstructure and shear strength of Sn–Ag–Cu solder on Au/Ni metallized Cu pads10.1016/j.microrel.2011.03.042 ↗
18. Microstructure, mechanical and electrical performances of zirconia nanoparticles-doped tin-silver-copper solder alloys10.1007/s10854-016-4732-x ↗
19. Retained ratio of reinforcement in SAC305 composite solder joints: effect of reinforcement type, processing and reflow cycle10.1108/SSMT-02-2016-0004 ↗
20. Effects of TiO2 nanoparticles addition on microstructure, microhardness and tensile properties of Sn–3.0Ag–0.5Cu–xTiO2 composite solder10.1016/j.matdes.2013.10.033 ↗
21. Effect of TiO2 additions on Sn-0.7Cu-0.05Ni lead-free composite solder10.1016/j.microrel.2016.08.011 ↗
22. Effect of nanoparticles addition on the microstructure and properties of lead-free solders: a review10.3390/app9102044 ↗
23. Influence of nanoparticle addition on the formation and growth of intermetallic compounds (IMCs) in Cu/Sn–Ag–Cu/Cu solder joint during different thermal conditions
24. Effects of Nano-TiO2 additions on thermal analysis, microstructure and tensile properties of Sn3.5Ag0.25Cu solder10.1016/j.matdes.2009.08.008 ↗
25. An investigation of nanoparticles addition on solidification kinetics and microstructure development of tin–lead solder10.1016/S0921-5093(03)00466-0 ↗
26. Effect of adding 0.5 wt% ZnO nanoparticles, temperature and strain rate on tensile properties of Sn–5.0 wt% Sb–0.5 wt% Cu (SSC505) lead free solder alloy10.1016/j.msea.2016.01.081 ↗
27. Application of ZnO nanoparticles in Sn99Ag0.3Cu0.7 based composite solder alloys10.3390/nano11061545 ↗
28. Structural characterization and creep resistance of nano-silicon carbide reinforced Sn–1.0Ag–0.5Cu lead-free solder alloy10.1016/j.matdes.2013.10.043 ↗
29. Creep property of composite solders reinforced by nano-sized particles10.1007/s10854-007-9327-0 ↗
30. Solderability of Sn-0.7Cu/Si3N4 lead-free composite solder on Cu-substrate10.1016/j.phpro.2011.11.047 ↗
31. Tensile creep characteristics of Sn–3.5Ag–0.5Cu (SAC355) solder reinforced with nano-metric ZnO particles10.1016/j.msea.2014.02.061 ↗
32. Automatic characterisation method for statistical evaluation of tin whisker growth10.1016/j.microrel.2017.04.007 ↗
33. Effect of TiO2 sol on the microstructure and tribological properties of Cu-Sn coating10.1016/S1875-5372(18)30010-9 ↗
34. Oxidation study of pure tin and its alloys via electrochemical reduction analysis10.1007/s11664-005-0077-6 ↗
35. Study on corrosion behavior of β-Sn and intermetallic compounds phases in SAC305 alloy by in-situ EC-AFM and first-principles calculation10.1016/j.corsci.2021.109244 ↗
36. Corrosion properties of tin-copper alloy coatings in aspect of tin whisker growth10.1016/j.jallcom.2013.06.092 ↗
37. A critical review of thermodynamic data for inorganic tin species10.1016/S0016-7037(01)00645-7 ↗
38. Effect of micromorphology on corrosion and mechanical properties of SAC305 lead-free solders10.1016/j.microrel.2020.113634 ↗
39. Low-temperature Sn electrodeposition: texture evolution, grain boundary constitution and corrosion behavior10.1016/j.surfcoat.2021.127709 ↗
40. Roll of grain-boundary free energy & surface free energy for tin whisker growth
41. Temperature driven texture and grain boundary engineering of electrodeposited β-Sn coatings and its effect on the coating corrosion behaviour: five-parameter grain boundary character distribution analysis study10.1016/j.scriptamat.2021.113763 ↗
42. Electrodeposition current density induced texture and grain boundary engineering in Sn coatings for enhanced corrosion resistance10.1016/j.corsci.2021.109945 ↗
43. Evolution of texture and strain in Sn coating with Cr addition and its effect on the coating corrosion behavior10.1016/j.mtla.2020.100944 ↗
44. Metallurgical, physical, mechanical and oxidation behavior of lead-free chromium dissolved Sn–Cu–Bi solders10.1016/j.jmrt.2021.05.055 ↗
45. On the corrosion, stress corrosion and cytocompatibility performances of ALD TiO2 and ZrO2 coated magnesium alloys10.1016/j.jmbbm.2021.104945 ↗
46. TiO2 Sol strengthened Cu-Sn-PTFE composite coatings with high homogeneity and superior resistance to wear10.1016/j.wear.2019.01.031 ↗