Optimizing dislocation strengthening in high-strength medium-carbon steel via fast induction heating quenching & tempering
Source abstract
Abstract
This work produced high-strength quenching and tempering medium carbon steels via fast induction heating to achieve an optimal combination of strength and ductility. The achieved yield strength, tensile strength, and total elongation were 2103 MPa, 2301 MPa, and 8.26%, respectively. Compared to conventional heating, fast induction heating results in finer martensite blocks and a much higher density of dislocations. The contribution of dislocation strengthening is found to be dominant, exceeding 1000 MPa, rather than boundary strengthening as commonly considered. With a proper raising of tempering temperature, the dislocations interact and partially annihilate, leading to a fallback in strength but an increment in ductility. Thus, it can be concluded that fast induction heating is a feasible technique to balance ultrahigh strength and high ductility in medium carbon steels.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Martensite in steel: strength and structure
2. Steels for bearings10.1016/j.pmatsci.2011.06.002 ↗
3. Papaefthymiou · 2017
4. Effect of ultra-fast heat treatment on the subsequent formation of mixed martensitic/bainitic microstructure with carbides in a CrMo medium carbon steel10.3390/met9030312 ↗
5. Study of carbide dissolution and austenite formation during ultra–fast heating in medium carbon chromium molybdenum steel10.3390/met8080646 ↗
6. Control of cementite precipitation in lath martensite by rapid heating and tempering10.2355/isijinternational.44.1937 ↗
7. The effect of ultrafast heating on cold-rolled low carbon steel: formation and decomposition of austenite10.3390/met6120321 ↗
8. Effect of heating rate on the austenite formation in low-carbon high-strength steels annealed in the intercritical region10.1007/s11661-011-0753-5 ↗
9. High-efficiency fast-heating annealing of a cold-rolled dual-phase steel10.1016/j.matdes.2014.01.055 ↗
10. Effect of block size on the strength of lath martensite in low carbon steels10.1016/j.msea.2005.12.048 ↗
11. Evaluation of the block boundary and sub-block boundary strengths of ferrous lath martensite using a micro-bending test10.1016/j.msea.2010.08.026 ↗
12. Effect of prior austenite grain size on the morphology and mechanical properties of martensite in medium carbon steel10.1016/S1005-0302(12)60083-8 ↗
13. The effect of structure on the deformation of as-quenched and tempered martensite in an Fe-0.2 pct C alloy10.1007/BF02644037 ↗
14. On the yield strength of quenched low-carbon lath martensite
15. Effect of transformation substructure on the strength and toughness of Fe−Mn alloys10.1007/BF03037855 ↗
16. Refinement of cementite in high strength steel plates by rapid heating and tempering10.4028/www.scientific.net/MSF.539-543.4720 ↗
17. Martensite tempering kinetics: effects of dislocation density and heating rates10.1016/j.matchar.2020.110564 ↗
18. X-ray measurement of retained austenite
19. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
20. Comparison of dislocation densities of primary and secondary recrystallization grains of Si-Fe10.1016/0001-6160(57)90122-0 ↗
21. Microstructures and hardness of as-quenched martensites (0.1–0.5%C)10.1016/j.actamat.2011.05.061 ↗
22. Gladman · 2002 · 213
23. Modelling strength and ductility of ultrafine grained BCC and FCC alloys using irreversible thermodynamics10.1179/174328408X353750 ↗
24. The isotropic shear modulus of multicomponent Fe-base solid solutions10.1016/S1359-6454(02)00096-4 ↗
25. Structure-property relationships in high-strength microalloyed steels
26. The influence of silicon in tempered martensite: understanding the microstructure–properties relationship in 0.5–0.6wt.% C steels10.1016/j.actamat.2014.01.039 ↗
27. Carbide size refinement by controlling the heating rate during induction tempering in a low alloy steel10.1016/j.matdes.2014.05.053 ↗