journal article·2021-11Open access

Effect of TiC/TiC–TiB2 on microstructure and mechanical properties of spray formed 7055 aluminum alloy TIG welded joints

Yun Cheng, Junhua Xu, Lihua Yu, Yunxuan Hu, Ting Huang, Hao Zhang

Abstract

Owing to the notorious hot-crack susceptibility and severe softening fusion-weld joints of Al–Zn–Mg–Cu alloys, they are generally considered unweldable. In this study, TiC/7xxx (TC) and TiC–TiB2/7xxx (BC) aluminum matrix composites, fabricated by in-situ mixed-salt reaction, were used as filler rods of spray formed 7055 alloys to modify the microstructure and mechanical properties of TIG weld joints. Compared with 7055-weld metal (WM), the grain sizes of TC-WM and BC-WM were refined from 100 μm to 24 μm and 26 μm, respectively. The precipitation of eutectic phases in WM was reduced by ceramic particles, which decreased the hot-crack susceptibility of joints. In the as-welded state, the ultimate tensile strength of TC and BC joints increased from 240 ± 5 MPa to 274 ± 5 MPa and 300 ± 5 MPa, respectively. The addition of ceramic particles also improved the impact toughness and hardness of weld joints. Grain refinement, load-bearing strengthening, coefficients of thermal expansion mismatch strengthening, and Zener pinning strengthening are the dominant strengthening mechanisms of weld joints with ceramic particles.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Effect of contact solid solution treatment on peak aging of Al-Zn-Mg-Cu alloys10.1016/j.jmrt.2020.02.074 ↗
2. Microstructure evolution during homogenization and hot workability of 7055 aluminum alloy produced by twin-roll casting10.1016/j.jmrt.2021.05.114 ↗
3. Mechanical properties of solution heat treated Al-Zn-Mg-Cu (7075) alloy under different cooling conditions: analysis with full field measurement and finite element modeling10.1016/j.jallcom.2020.158180 ↗
4. Microstructure and mechanical properties of heat affected zone in multi-pass GMA welded Al–Zn–Mg–Cu alloy10.1016/S1003-6326(19)65133-2 ↗
5. Solidification cracking susceptibility of quaternary aluminium alloys10.1080/13621718.2021.1893007 ↗
6. Improve the quality of 1060Al/Q235 explosive composite plate by friction stir processing10.1016/j.jmrt.2019.10.027 ↗
7. Investigation on friction stir welding of hybrid composites fabricated on Al–Zn–Mg–Cu alloy through friction stir processing10.1016/j.jmrt.2019.06.033 ↗
8. Effects of multi-pass friction stir processing on microstructures and mechanical properties of the 1060Al/Q235 Composite Plate10.3390/met10030298 ↗
9. Influences of pulsed current welding and post weld aging treatment on fatigue crack growth behaviour of AA7075 aluminium alloy joints10.1016/j.ijfatigue.2007.04.012 ↗
10. Effectiveness of cold metal transfer process for welding 7075 aluminium alloys10.1179/1362171815Y.0000000017 ↗
11. Numerical Simulation and experimental investigation on electron beam welding of Spray-Formed 7055 aluminum alloy10.3390/met10101392 ↗
12. Tensile fracture behavior in CO2 laser beam welds of 7075-T6 Aluminum Alloy10.1016/j.matdes.2004.02.017 ↗
13. Development of new high strength Al – Sc filler wires for fusion welding 7000 series aluminium aerospace alloys10.1179/136217103225010989 ↗
14. Effect of pulsed current and post weld aging treatment on tensile properties of argon arc welded high strength aluminium alloy10.1016/j.msea.2006.12.125 ↗
15. The influence of nanoparticles on dendritic grain growth in Mg alloys10.1016/j.actamat.2018.04.023 ↗
16. Nanoparticle-induced superior hot tearing resistance of A206 alloy10.1007/s11661-012-1531-8 ↗
17. Nanoparticle-induced unusual melting and solidification behaviours of metals10.1038/ncomms14178 ↗
18. Nanoparticle-enabled phase control for arc welding of unweldable aluminum alloy 707510.1038/s41467-018-07989-y ↗
19. Tensile properties and strengthening effects of Al 3003 alloy weldment reinforced with TiO2 nanoparticles10.1016/j.compositesb.2019.107159 ↗
20. Microstructure and mechanical properties of Al/ZrC/TiC hybrid nanocomposite filler metals of tungsten inert gas welding fabricated by accumulative roll bonding10.1016/j.jmapro.2017.02.012 ↗
21. Optimization of GTAW Al 3003 weld using fabricated nanocomposite filler metal
22. Applying the ultrasonic vibration during TIG welding as a promising approach for the development of nanoparticle dispersion strengthened aluminum weldments10.1016/j.jmatprotec.2020.116672 ↗
23. Study on aluminum alloy joints welded with nano-treated Al-Mg-Mn filler wire10.1016/j.matlet.2020.128739 ↗
24. Nano-carbide strengthened as-welded joint for precipitation-hardened austenitic Fe–Mn–Al–C lightweight alloys10.1016/j.jmrt.2021.06.062 ↗
25. Wetting of TiC by molten Al at 1123–1323 K10.1016/j.actamat.2010.11.055 ↗
26. Al-TiB2 micro/nanocomposites: particle capture investigations, strengthening mechanisms and mathematical modelling of mechanical properties10.1016/j.msea.2016.11.034 ↗
27. Investigate on the phase interfaces and performance evaluation of TiB2p/Al–Si–Cu–Zn (T6) composites10.1016/j.jmrt.2021.03.018 ↗
28. Microstructural characterization and mechanical properties of in situ cast nanocomposites Al/TiC type10.1016/j.jmrt.2020.09.012 ↗
29. Microstructure and mechanical properties of 7055 Al alloy prepared under different sintering conditions using powder by-products10.1016/j.msea.2020.140562 ↗
30. Effect of pretreatment on microstructural stability and mechanical property in a spray formed Al-Zn-Mg-Cu alloy10.1016/j.matdes.2021.109618 ↗
31. Design, microstructure and high temperature properties of in-situ Al3Ti and nano-Al2O3 reinforced 2024Al matrix composites from Al-TiO2 system10.1016/j.jallcom.2018.09.376 ↗
32. On the microstructural and mechanical characterization of hybrid laser-welded Al-Zn-Mg-Cu alloys10.1007/s11665-015-1408-2 ↗
33. Effect of solution-treating temperature on the intergranular corrosion of a peak-aged Al-Zn-Mg-Cu alloy10.1016/j.jmrt.2020.04.035 ↗
34. Strengthening mechanism of TiC/Al composites using Al-Ti-C/CNTs with doping alloying elements (Mg, Zn and Cu)10.1016/j.jmrt.2020.04.033 ↗
35. Effect of d alumina fibers on the aging characteristics of 2024-based metal-matrix composites10.1007/BF02670599 ↗
36. Microstructural development in an aluminum alloy-SiC whisker composite10.1016/0001-6160(88)90236-2 ↗
37. 6061 aluminum alloy-SiC particulate composite: a comparison between aging behavior in T4 and T6 treatment10.1016/0921-5093(91)90575-8 ↗
38. Microstructure and mechanical behaviour of in situ fabricated AA6061–TiC metal matrix composites10.1016/j.acme.2016.12.006 ↗
39. Evolution of microstructure and mechanical properties of A1-5 wt% Ti composite fabricated by P/M and hot extrusion: effect of heat treatment10.1016/j.msea.2017.02.049 ↗
40. Formation mechanism of in situ Al3Ti in Al matrix during hot pressing and subsequent friction stir processing10.1016/j.matchemphys.2011.08.042 ↗
41. Effects of ultrasound assisted solidificaiton on the microstructure and mechanical properties of nano-sized TiB2/Al-4.5Cu composites10.1016/j.mtla.2021.101024 ↗
42. Hierarchical grain refinement during the laser additive manufacturing of Ti-6Al-4V alloys by the addition of micron-sized refractory particles