Effect of SiC addition on microstructure and properties of Al–Mg alloy fabricated by powder and wire cold metal transfer process
Source abstract
Abstract
Adding heterogeneous nucleation refiners is an effective route to obtain fine grained microstructure. To investigate effect of silicon carbide (SiC) particles on mechanical properties of Al–Mg alloy, metallic matrix composites (MMCs) were fabricated by an innovative powder and wire cold metal transfer (CMT) process with enhanced mechanical properties. Microstructure evolution, grain orientation and mechanical properties of CMT processed MMCs reinforced by SiC particles at different concentrations were discussed. The mechanical properties of Al–Mg alloy reached the highest tensile strength of 325.6 ± 16 MPa by addition of SiC particles with a volume fraction of 8% and an average grain diameter of 49.1 μm. This research provided a novel, time-saving, low-cost approach to fabricate Al–Mg composites and expands application of Al–Mg alloy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Selective laser melting to manufacture “in situ” metal matrix composites: a review10.1002/adem.201801244 ↗
2. Additive manufacturing (3D printing): a review of materials, methods, applications and challenges10.1016/j.compositesb.2018.02.012 ↗
3. Investigation of cutting forces, surface integrity, and tool wear when high-speed milling of high-volume fraction SiCp/Al6063 composites in PCD tooling10.1007/s00170-018-2294-1 ↗
4. Weld properties and residual stresses of VPPA Al welds at varying welding positions10.1016/j.jmrt.2020.01.040 ↗
5. Improved mechanical properties of AlSi7Mg/nano-SiCp composites fabricated by selective laser melting10.1016/j.jallcom.2019.151926 ↗
6. Al/SiCNP and Al/SiCNP/X nanocomposites fabrication and properties: a review
7. Alumina/silicon carbide composites fabricated via in situ synthesis of nano-sized SiC particles10.1016/j.ceramint.2008.05.013 ↗
8. Microstructure and tensile behavior of hybrid nano-micro SiC reinforced iron matrix composites produced by selective laser melting10.1016/j.jallcom.2013.06.087 ↗
9. Influence of mechanical alloying on the microstructure and mechanical properties of powder metallurgy Ti 2 AlNb-based alloy10.1016/j.powtec.2017.03.034 ↗
10. Rejuvenation of inside surface of intergranular corrosion-damaged type 304 stainless steel tube through laser surface melting10.1007/s11665-020-04681-5 ↗
11. Characteristic behaviour of aluminium metal matrix composites: a review10.1016/j.matpr.2017.12.180 ↗
12. Selective laser melting of in-situ Al4SiC4 + SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
13. A review of wire arc additive manufacturing and advances in wire arc additive manufacturing of aluminium10.1080/02670836.2018.1455012 ↗
14. In-situ wire-feed additive manufacturing of Cu-Al alloy by addition of silicon10.1016/j.apsusc.2019.05.068 ↗
15. A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement10.1016/j.jmapro.2018.08.001 ↗
16. Correlation between arc mode, microstructure, and mechanical properties during wire arc additive manufacturing of 316L stainless steel10.1016/j.msea.2019.02.078 ↗
17. Effects of heat distribution during cold metal transfer arc welding on galvanized steel using volumetric heat source model10.1016/j.jmrt.2020.07.004 ↗
18. Sun · 2011
19. Porosity in wire arc additive manufacturing of aluminium alloys
20. Optimisation of interpass temperature and heat input for wire and arc additive manufacturing 5A06 aluminium alloy10.1080/13621718.2016.1259031 ↗
21. The effects of forced interpass cooling on the material properties of wire arc additively manufactured Ti6Al4V alloy10.1016/j.jmatprotec.2018.03.024 ↗
22. Faridmehr · 2001 · 3
23. Microstructure and wear studies of laser clad Al-Si/SiC(p) composite coatings10.1016/j.surfcoat.2007.04.003 ↗
24. Effect of Ce on the microstructure and mechanical properties of 5356 aluminum alloy
25. Effect of heat input on microstructure and mechanical properties of Al-Mg alloys fabricated by WAAM10.1016/j.apsusc.2019.04.255 ↗
26. Rapid fabrication of Al-based bulk-form nanocomposites with novel reinforcement and enhanced performance by selective laser melting10.1016/j.scriptamat.2014.10.011 ↗
27. Effect of titanium powder on microstructure and mechanical properties of wire + arc additively manufactured Al-Mg alloy10.1016/j.matlet.2019.01.117 ↗
28. Hierarchical microstructure and strengthening mechanisms of a CoCrFeNiMn high entropy alloy additively manufactured by selective laser melting10.1016/j.scriptamat.2018.05.015 ↗
29. Effect of scan pattern on the microstructure and mechanical properties of Powder Bed Fusion additive manufactured 17-4 stainless steel10.1016/j.matdes.2017.07.047 ↗
30. Fabrication of Fe-based bulk amorphous alloys using hot metal and commercial ferro-alloys10.2320/matertrans.46.2237 ↗
31. Location dependence of microstructure and mechanical properties of Cu–Al alloy fabricated by dual wire CMT10.1088/2053-1591/ab583e ↗
32. Microstructural evolution and mechanical properties of deep cryogenic treated Cu–Al–Si alloy fabricated by Cold Metal Transfer (CMT) process10.1016/j.matchar.2019.110011 ↗
33. Microstructural characterization and properties of selective laser melted maraging steel with different build directions10.1080/14686996.2018.1527645 ↗
34. In-situ strengthening of a high strength low alloy steel during Wire and Arc Additive Manufacturing (WAAM)
35. Enhanced strength and ductility in a friction stir processing engineered dual phase high entropy alloy10.1038/s41598-017-16509-9 ↗
36. Formation mechanism of typical onion ring structures and void defects in friction stir lap welded dissimilar aluminum alloys10.1016/j.matdes.2015.11.014 ↗
37. Enhancing the tribo-mechanical properties of aerospace AL7075-T6 by magnetron-sputtered Ti/TiN, Cr/CrN & TiCr/TiCrN thin film ceramic coatings10.1016/j.ceramint.2014.07.067 ↗
38. Reactions in the matrix and interface of the Fe–SiC metal matrix composite system10.1016/S0921-5093(99)00158-6 ↗
39. Comparison between current models for the strength of particulate-reinforced metal matrix nanocomposites with emphasis on consideration of Hall–Petch effect10.1016/j.msea.2011.10.043 ↗
40. Zener pinning pressure in tempered martensite lath structure10.4028/www.scientific.net/MSF.715-716.745 ↗
41. Strengthening mechanisms in particulate metal matrix composites10.1016/0956-716X(91)90349-6 ↗
42. Effect of particle orientation anisotropy on the tensile behavior of metal matrix composites: experiments and microstructure-based simulation10.1016/j.msea.2004.09.017 ↗