journal article·2022-11Open access

Strengthening mechanism of lamellar-structured Ti–Ta alloys prepared by powder metallurgy

Chufan Wang, Qi Cai, Jinxu Liu, Xifeng Yan

Abstract

Titanium-tantalum alloys with lamellar microstructure were fabricated by cold isostatic pressing under 400 MPa and pressure-free sintering at 1600 °C. By such a low-cost powder metallurgy method, the Ti–Ta alloy exhibited the tensile yield strength of 1124 MPa at room temperature, which was twice that of the cast Ti–Ta alloys. The microstructure and mechanical properties were characterized in detail to elucidate the deformation behavior and the strengthening mechanism of the Ti–Ta alloys prepared by powder metallurgy. With the increasing Ta content, the width of the α laths decreased, and that of the β laths increased, leading to the precipitation of the acicular α in the β laths. Correspondingly, the yield and ultimate strength increased, while the strain to failure decreased. Lamellar structure strengthening was determined to be the dominating mechanism for the high strength of the Ti–Ta alloys prepared by powder metallurgy. After quantitatively evaluating the contributions of laths, solute atoms, prior β grain boundaries, and dislocations, a model was established to illustrate the yield strength of the Ti–Ta alloys. The calculated values agreed well with the measured strength values of the Ti–Ta alloys, indicating that this model is effective in forecasting the strength of the dual-phase Ti alloys with lamellar structure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Cost-affordable, biomedical Ti-5Fe alloy developed using elemental powders and laser in-situ alloying additive manufacturing10.1016/j.matchar.2021.111526 ↗
2. Development of biomedical Ti-Nb-Zr-Mn alloys with enhanced mechanical properties and corrosion resistance
3. Processing and properties of topologically optimised biomedical Ti–24Nb–4Zr–8Sn scaffolds manufactured by selective laser melting10.1016/j.msea.2015.06.088 ↗
4. Relationship between microstructure, phase transformation, and mechanical behavior in Ti–40Ta alloys for biomedical applications10.1016/j.jmrt.2021.06.038 ↗
5. Tailoring bimodal structure for high strength and ductility in pure titanium manufactured via laser powder bed fusion10.1016/j.jallcom.2021.163590 ↗
6. Microstructure and corrosion characterization of a Ti-30Zr alloy with Ta additions processed by arc-melting for biomedical applications10.1016/j.matlet.2020.129041 ↗
7. A review on biomedical titanium alloys: recent progress and prospect10.1002/adem.201801215 ↗
8. Mechanical properties and microstructure of powder metallurgy Ti-xNb-yMo alloys for implant materials10.1016/j.matdes.2015.09.106 ↗
9. Supriadi · 2019
10. Microstructure and properties of a novel ternary Ti–6Zr–xFe alloy for biomedical applications10.1016/j.jallcom.2020.157119 ↗
11. Mechanical properties and electrochemical behavior of porous Ti-Nb biomaterials10.1016/j.jmbbm.2018.07.018 ↗
12. Assessment of Ti-16Nb-xZr alloys produced via PIM for implant applications10.1007/s10973-017-6808-0 ↗
13. Biomedical porous Ti-16Nb-10Zr-(0-15)Ta alloys10.3139/146.111749 ↗
14. Powder metallurgy processing of Ti-Nb based biomedical alloys10.12693/APhysPolA.134.278 ↗
15. Compositionally gradient Ti-Ta metal-metal composite with ultra-high strength10.1016/j.msea.2017.11.089 ↗
16. Preparation and characterization of Ti–Ta alloys for application in corrosive media10.1016/S0167-577X(02)01422-2 ↗
17. Laser powder bed fusion of titanium-tantalum alloys: compositions and designs for biomedical applications10.1016/j.jmbbm.2020.103775 ↗
18. Comparison of various properties between titanium-tantalum alloy and pure titanium for biomedical applications10.2320/matertrans.48.380 ↗
19. Microstructures and mechanical properties of Ti-50 mass% Ta alloy for biomedical applications10.1016/j.jallcom.2007.11.090 ↗
20. Synthesis of porous Ti–50Ta alloy by powder metallurgy10.1016/j.matchar.2018.05.033 ↗
21. Ingot metallurgy and microstructural characterization of Ti–Ta alloys10.3139/146.111010 ↗
22. Ti-25Ta alloy with the best mechanical compatibility in Ti-Ta alloys for biomedical applications10.1016/j.msec.2008.09.012 ↗
23. Characterization of fatigue properties of powder metallurgy titanium alloy10.1016/j.msea.2015.12.058 ↗
24. Synthesis of Ti-Ta alloys with dual structure by incomplete diffusion between elemental powders10.1016/j.jmbbm.2015.07.004 ↗
25. Microstructural evolution and mechanical properties of bulk and porous low-cost Ti–Mo–Fe alloys produced by powder metallurgy10.1016/j.jallcom.2020.156768 ↗
26. Correlation between alpha phase morphology and tensile properties of a new beta titanium alloy10.1016/j.matdes.2017.02.043 ↗
27. Slip transmission behavior across alpha/beta interface and strength prediction with a modified rule of mixtures in TC21 titanium alloy10.1016/j.jallcom.2017.07.002 ↗
28. The effect of alpha platelet thickness on plastic flow during hot working of Ti-6Al-4V with a transformed microstructure10.1016/S1359-6454(01)00236-1 ↗
29. Strength and fracture toughness of TC21 alloy with multi-level lamellar microstructure10.1016/j.msea.2018.10.056 ↗
30. Tuning the number density of αs precipitates in Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-0.1Si alloys for achieving high strength10.1016/j.jallcom.2021.160732 ↗
31. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength10.1016/j.scriptamat.2018.05.040 ↗
32. Bi-lamellar microstructure in Ti–6Al–4V: microstructure evolution and mechanical properties10.1016/j.msea.2019.138077 ↗
33. Strengthening mechanism of two-phase titanium alloys with basketweave microstructure10.1016/j.jallcom.2014.03.057 ↗
34. Phase stability and stress-induced transformations in beta titanium alloys10.1007/s11837-015-1411-y ↗
35. Interdiffusion in the body cubic centered beta-phase of Ta-Ti alloys10.1016/S1359-6454(97)00272-3 ↗
36. Effects of Ta content on Young's modulus and tensile properties of binary Ti–Ta alloys for biomedical applications10.1016/j.msea.2003.12.011 ↗
37. Tailoring microstructure and properties of a superelastic Ti-Ta alloy by incorporating spark plasma sintering with thermomechanical processing10.1007/s11665-019-04061-8 ↗
38. Multi-scale nacre-inspired lamella-structured Ti-Ta composites with high strength and low modulus for load-bearing orthopedic and dental applications10.1016/j.msec.2020.111458 ↗
39. Selective laser melting of titanium alloy with 50 wt% tantalum: microstructure and mechanical properties10.1016/j.jallcom.2015.11.141 ↗
40. A review on high-strength titanium alloys: microstructure, strengthening, and properties10.1002/adem.201801359 ↗
41. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
42. Comparison of high-temperature deformation behaviors for Ti-Al-Nb-V alloy with different initial microstructures at the strain of 0.710.1016/j.msea.2020.140042 ↗
43. Deformation mechanisms and microtensile behavior of single colony Ti-6242Si10.1016/S0921-5093(01)01024-3 ↗
44. Slip transfer across phase boundaries in dual phase titanium alloys and the effect on strain rate sensitivity10.1016/j.ijplas.2018.01.011 ↗
45. Influence of alpha/beta interface phase on the tensile properties of laser cladding deposited Ti-6Al-4V titanium alloy10.1016/j.jmst.2016.09.026 ↗
46. Room temperature deformation and mechanisms of slip transmission in oriented single-colony crystals of an α/β titanium alloy10.1016/S1359-6454(98)00364-4 ↗
47. A modified Hall-Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing10.1016/j.scriptamat.2012.02.008 ↗
48. The influence of prior cold deformation on precipitation of alpha phase and variation of hardness in Ti-10Mo-8V-1Fe-3.5Al during aging treatment10.1557/JMR.2009.0051 ↗
49. Modelling strengthening mechanisms in beta-type Ti alloys10.1016/j.msea.2019.04.027 ↗
50. Solid-solution hardening of cupper crystals10.1007/BF00552938 ↗
51. Effects of Mo equivalent on the phase constituent, microstructure and compressive mechanical properties of Ti–Nb–Mo–Ta alloys prepared by powder metallurgy10.1016/j.jmrt.2021.12.054 ↗
52. Microstructure and strengthening mechanism of ultrastrong and ductile Ti-xSn alloy processed by powder metallurgy10.1016/j.jallcom.2017.03.171 ↗
53. Flow stress analysis of TWIP steel via the XRD measurement of dislocation density10.1016/j.msea.2010.01.033 ↗
54. Microstructures analysis and quantitative strengthening evaluation of powder metallurgy Ti–Fe binary extruded alloys with (α+β)-dual-phase10.1016/j.msea.2020.140708 ↗