Effect of annealing process on interface microstructure and mechanical property of the Cu/Al corrugated clad sheet
Source abstract
Abstract
In this research, annealing treatment was performed on the Cu/Al corrugated clad sheets fabricated by the corrugated cold roll bonding (CCRB) process. Interface microstructure evolution, interface phase development, intermetallic compound (IMC) growth kinetics, interface bonding strength, and electrical resistivity at various positions of the Cu/Al corrugated clad sheet were investigated under different annealing conditions. The IMC layers (CuAl2, Cu9Al4 and CuAl) with uneven thickness were formed at the Cu/Al corrugated interface during the annealing process. Interface defects caused by shear deformation can effectively reduce the growth activation energies of IMC sub-layer at positions I (back waist), III (front waist), and IV (trough). On the contrary, the interface brittle layers and overlayer can slightly increase the activation energy at position II (peak). The sequence of growth activation energies for IMC sub-layer was QCuAl<QCu9Al4<QCuAl2. When Cu/Al corrugated clad sheet was annealed at 350 °C for 30 min, the recrystallization degree of Al plate at position III (front waist) was higher than the position II (peak), which was mainly due to the severe plastic deformation at the front waist position. Meanwhile, the transformation from low angle grain boundaries (LAGBs) to high angle grain boundaries (HAGBs) of the Al plate was more likely to occur at position III (front waist). Interface shear strength presented wavy distribution along the interface when the Cu/Al corrugated clad sheet was annealed at 350 °C for different times. With the increase of annealing time, the average shear strength first increased and then decreased rapidly. When the annealing time was 60 min, the average shear strength reached the maximum value of 45.61 MPa, and the average electrical resistivity reduced to the minimum value of 11.56 × 10−8 Ω m. Considering the double influence of annealing process on bonding strength and electrical resistivity, it was recommended that the Cu/Al corrugated clad sheet be annealed at 350 °C for 60 min.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Effect of heat treatment on the bending behavior of tri-layered Cu/Al/Cu composite plates10.1016/j.matdes.2012.12.070 ↗
2. Effects of annealing temperature on interface microstructure and element diffusion of ultra-thin Cu/Al composite sheets10.1016/j.matlet.2022.132491 ↗
3. Microstructure and mechanical behaviors of Al/Cu laminated composites fabricated by accumulative roll bonding and intermediate annealing10.1016/j.msea.2021.142510 ↗
4. Effect of annealing and cold rolling on interface microstructure and properties of Ti/Al/Cu clad sheet fabricated by horizontal twin-roll casting
5. Effects of annealing temperature on the interfacial microstructure and bonding strength of Cu/Al clad sheets produced by twin-roll casting and rolling10.1016/j.jmatprotec.2020.116804 ↗
6. Effects of asymmetry and annealing on interfacial microstructure and mechanical properties of Cu/Al laminated composite fabricated by asymmetrical roll bonding10.1016/j.jallcom.2019.152453 ↗
7. Texture development in the interfacial zone of Al/Cu bimetal cold roll-bonded for E-mobility10.1016/j.matlet.2018.10.079 ↗
8. Interfacial bonding mechanism of Cu/Al composite plate produced by corrugated cold roll bonding10.1007/s12598-020-01660-6 ↗
9. Effect of heat treatment on bonding mechanism and mechanical properties of high strength Cu/Al/Cu clad composite10.1016/j.jallcom.2019.06.132 ↗
10. Effect of annealing temperature on microstructure and bond strength of cast-rolling Cu-Al clad plates10.1088/2053-1591/ab1d3a ↗
11. Experimental and numerical analysis of Cu/Al8011/Al1060 trilayered composite: a comprehensive study
12. Formation and growth of Cu-Al IMCs and their effect on electrical property of electroplated Cu/Al laminar composites10.1016/S1003-6326(16)64462-X ↗
13. Effect of annealing on the microstructures and mechanical properties of Al/Mg/Al laminates10.1016/j.msea.2018.06.065 ↗
14. Growth kinetics of TiAl 3 phase in annealed Al/Ti/Al explosively welded clads10.1016/j.matlet.2017.04.025 ↗
15. Influence of annealing on the microstructure and mechanical properties of Ti/steel clad plates fabricated via cold spray additive manufacturing and hot-rolling10.1016/j.msea.2020.138968 ↗
16. Influence of heat treatment on interface of Cu/Al bimetal composite fabricated by cold rolling10.1016/j.compositesb.2011.04.045 ↗
17. Interfacial microstructure and mechanical properties of Cu/Al clad sheet fabricated by asymmetrical roll bonding and annealing10.1016/j.msea.2011.09.087 ↗
18. Interface strengthening of a roll-bonded two-ply Al/Cu sheet by short annealing10.1016/j.matchar.2021.111021 ↗
19. Effects of intermetallic compound on the electrical and mechanical properties of friction welded Cu/Al bimetallic joints during annealing10.1016/j.jallcom.2004.07.057 ↗
20. Intermetallic fprmation in the aluminum copper system10.1142/S0218625X03005396 ↗
21. Brittleness study of intermetallic (Cu, Al) layers in copper-clad aluminium thin wires10.1016/j.msea.2011.05.077 ↗
22. Influence of interfacial structure development on the fracture mechanism and bond strength of aluminum/copper bimetal plate10.2320/matertrans.47.1232 ↗
23. Microstructures and mechanical properties of Cu/Al compound materials during thermal cycle
24. Behavior of aluminum oxide, intermetallics and voids in Cu-Al wire bonds10.1016/j.actamat.2011.05.041 ↗
25. Effect of annealing on the interfacial structure of aluminum-copper joints10.2320/matertrans.MER2006371 ↗
26. Interfacial reactions on annealing Cu/Al multilayer thin films10.1063/1.355183 ↗
27. Interface-position-dependent structure evolution and mechanical behavior of corrugated cold rolled Cu/Al clad plate: experiment and simulation
28. Bulk mechanical alloying of Cu-Ag and Cu/Zr two-phase microstructures by accumulative roll-bonding process10.1016/j.actamat.2006.12.027 ↗
29. On the evolution of microstructure, texture and corrosion behavior of a hot-rolled and annealed AZ31 alloy10.1016/j.matchemphys.2021.124598 ↗
30. Friction stir butt-welding of roll cladded aluminum thin sheets: effect of microstructural and texture changes on mechanical properties10.1016/j.msea.2021.142490 ↗
31. Thermal stability of an Mg-Nd alloy processed by high-pressure torsion10.1002/adem.201900801 ↗
32. Ab initiostudy of the effect of solute atoms on the stacking fault energy in aluminum10.1103/PhysRevB.75.224105 ↗
33. Investigation on bonding strength of steel/aluminum clad sheet processed by horizontal twin-roll casting, annealing and cold rolling10.1016/j.matdes.2016.09.061 ↗
34. Effect of solution treatment and artificial aging on microstructure and mechanical properties of Al-Cu alloy10.1016/S1003-6326(13)62509-1 ↗