Simultaneously improved modulus, thermal expansion coefficient and wear resistance of a Mg–6Zn–1Gd–0.3Ca matrix composite by adding high volume fraction SiC particles

Wei Li, Kaibo Nie, KunKun Deng, Zhilong Liu, Quanxin Shi

Abstract

In this paper, three sizes (5, 20 and 50μm) SiC particles (SiCp) were selected, and the SiCp/Mg-6Zn-1Gd-0.3Ca (SiCp/ZG61X) composites with ∼50 vol.% were successfully prepared by squeeze casting. The effect of particle size on the properties of the composites was studied, while the wear resistance and the wear mechanism of composites were investigated. The results showed that compared with the matrix alloy, the addition of SiCp can significantly improve the properties of the composites, in which the strength increased from 175.2 to 326.5 MPa and the modulus increased from 45.0 to 159.6 GPa. At the same time, the coefficient of thermal expansion and friction were significantly reduced. In addition, the smaller the particle size, the higher the strength and modulus of the composite. However, for the coefficient of friction and thermal expansion, the larger particle size was conducive to the reduction of the two coefficients. The analysis of friction and wear behavior showed that the wear mechanism of the matrix alloy was mainly abrasive wear and adhesive wear, while the wear mechanism of the composites was abrasive wear and layered wear.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Different effects of SiC dimensions on the microstructure and mechanical properties of magnesium matrix composites10.1016/j.msea.2022.143273 ↗
2. The work hardening and softening behaviors of Mg–6Zn-1Gd-0.12Y alloy influenced by the VR/VD ratio10.1016/j.msea.2022.143970 ↗
3. Effect of hot extrusion on the microstructure and mechanical properties of SiCNWs/Mg-2Zn-0.1Y composite10.1016/j.matchar.2022.111970 ↗
4. Static recrystallization behaviour of cold rolled Mg-Zn-Y alloy and role of solute segregation in microstructure evolution10.1016/j.scriptamat.2017.04.001 ↗
5. Nucleation of recrystallized magnesium grains over quasicrystalline phase during severe plastic deformation of a Mg-Zn-Y alloy at room temperature10.1016/j.scriptamat.2017.02.039 ↗
6. Microstructure, mechanical properties and corrosion behavior of quasicrystal-reinforced Mg-Zn-Y alloy subjected to dual-frequency ultrasonic field10.1016/j.corsci.2019.108289 ↗
7. Magnesium matrix composite reinforced by nanoparticles – a review10.1016/j.jma.2020.08.018 ↗
8. Effect of Ca addition on the microstructure and tensile properties of Mg–4.0Zn–2.0Gd alloys10.1016/j.msea.2014.04.093 ↗
9. Recent developments in rare-earth free wrought magnesium alloys having high strength: a review10.1016/j.jallcom.2015.12.057 ↗
10. Microstructure and corrosion properties of Mg-4Zn-2Gd-0.5Ca alloy influenced by multidirectional forging10.1016/j.jallcom.2018.08.191 ↗
11. Microstructure and corrosion behavior of the as-extruded Mg–4Zn–2Gd–0.5Ca alloy10.1007/s40195-019-00984-2 ↗
12. Microstructure and mechanical properties of Mg-4Zn-xGd (x=0, 0.5, 1, 2) alloys10.1016/j.jma.2019.06.005 ↗
13. Effects of Zn/Y ratio on microstructure and mechanical properties of Mg-Zn-Y alloys10.1016/j.matlet.2005.06.052 ↗
14. The effect of rare earth elements on the behaviour of magnesium-based alloys: Part 1—hot deformation behaviour10.1016/j.msea.2012.12.023 ↗
15. Influence of quasicrystal I-phase on twinning of extruded Mg-Zn-Y alloys under compression10.1016/j.actamat.2018.03.060 ↗
16. Effect of solute atoms and second phases on the thermal conductivity of Mg-RE alloys: a quantitative study10.1016/j.jallcom.2018.03.070 ↗
17. Evolution of microstructure, residual stress, and tensile properties of Mg–Zn–Y–La–Zr magnesium alloy processed by extrusion10.1007/s40195-019-00901-7 ↗
18. Microstructure and mechanical properties of M40/AZ91 composites fabricated by pressure infiltration method
19. Microstructure, mechanical properties and wear resistance of SiCp/AZ91 composite prepared by vacuum pressure infiltration10.1016/S1003-6326(21)65781-3 ↗
20. Microstructures and fabricating proces s of SiCp/az91d composites by vacuum pressure infiltration
21. Fabrication of SiC particles-reinforced magnesium matrix composite by ultrasonic vibration10.1007/s10853-011-5780-5 ↗
22. Effect of particle size on microstructure and mechanical properties of SiCp/AZ91 magnesium matrix composite10.1016/j.msea.2012.02.064 ↗
23. Effects of bimodal size SiC particles on the microstructure evolution and fracture mechanism of AZ91 matrix at room temperature10.1016/j.msea.2012.05.094 ↗
24. Characterization and strengthening mechanism of SiC nanoparticles reinforced magnesium matrix composite fabricated by ultrasonic vibration assisted squeeze casting10.1557/jmr.2017.202 ↗
25. Effects of SiCp parameters on microstructures, interface structure and mechanical property of Mg bulk composites produced by ultrasonic vibration processing10.1007/s12666-017-1268-6 ↗
26. High strength SiCp/AZ91 composite assisted by dynamic precipitated Mg17Al12 phase10.1016/j.jallcom.2017.10.164 ↗
27. Experimental and numerical studies of the effect of particle size on the deformation behavior of the metal matrix composites10.1016/j.msea.2006.10.158 ↗
28. The thermal expansion and mechanical properties of high reinforcement content SiCp/Al composites fabricated by squeeze casting technology10.1016/S1359-835X(03)00253-7 ↗
29. Microstructure, mechanical properties and mechanism of ultrasound-assisted rapid transient liquid phase bonding of magnesium alloy in air10.1016/j.matdes.2015.11.071 ↗
30. High-strength and high-modulus Al18B4O33W/GWZ1031K magnesium matrix composite prepared by squeeze casting10.1016/j.msea.2021.141393 ↗
31. Fabrication, microstructure and mechanical properties of Mg matrix composites reinforced by high volume fraction of sphere TC4 particles10.1016/j.jma.2016.10.003 ↗
32. Effect of extrusion parameters on microstructure and mechanical properties of SiC particle reinforced Mg-3.6Zn-0.6Y-0.2Ca matrix composites
33. Optimisation of the spark plasma sintering process for high volume fraction SiCp/Al composites by orthogonal experimental design10.1016/j.ceramint.2020.09.240 ↗
34. Reinforcement of thermally-conductive SiC/Al composite with 3D-interpenetrated network structure by various SiC foam ceramic skeletons10.1016/j.ceramint.2021.07.269 ↗
35. Anisotropic thermal expansion behavior of an interpenetrating metal/ceramic composite10.1016/j.tca.2019.178488 ↗
36. Microstructures and properties of Al–50%SiC composites for electronic packaging applications10.1016/S1003-6326(16)64358-3 ↗
37. Dry sliding wear behavior of (GNPs + TiB2)-reinforced AZ91 magnesium matrix hybrid composites produced by pressure infiltration casting method10.1007/s40962-020-00552-w ↗
38. Mechanical and wear properties of high rate NiAl particle-reinforced Al composites produced by pressure infiltration method10.1007/s40962-020-00564-6 ↗
39. Preparation and characterization of binder less Mg/Mg alloy infiltrated SiCp reinforced composites10.1007/s11665-007-9073-8 ↗
40. Effects of particle size and surface modification of SiC on the wear behavior of high volume fraction Al/SiCp composites10.1016/j.jallcom.2020.154647 ↗
41. Synergy effect of reinforcement particle, fiber and matrix on wear resistance of hybrid metal matrix composite fabricated by low pressure infiltration process10.1016/j.matdes.2014.06.025 ↗