Abstract

Multi-wire arc additive manufacturing (MWAAM) enabled customized production with high deposition efficiency and low cost as compared to the common wire arc additive manufacturing (WAAM) technology. In this paper, two titanium alloy components were prepared using the MWAAM technique, and the microstructures, mechanical properties, and wear behaviors of Ti–6Al–4V (TC4) alloy and Ti-6.5A1-3.5Mo-1.5Zr-0.3Si (TC11) alloy were investigated. The results showed that the microstructure distribution of TC11 alloy prepared by MWAAM was more intensive and the length and width of the lamellar α-Ti phase were significantly reduced compared with that of TC4 alloy. The polar densities corresponding to the <110> texture in the two selected regions of the TC4 alloy and the TC11 alloy were 17.30 and 17.69, respectively. The proportion of the HAGBs of the TC4 sample and the TC11 sample were 99.07 % and 99.43 %, respectively. The average microhardness on the X–Y plane of TC4 and TC11 alloys were 316.17 HV and 366.14 HV, respectively, while the average microhardness on the Y-Z plane were 318.18 HV and 358.10 HV, respectively. The average compression yield strengths of TC4 and TC11 alloys were 836.61 MPa and 1088.33 MPa, respectively. The COFs of MWAAM TC4 and TC11 samples were stable at 0.479 and 0.455 under 20 N, respectively. The COFs of MWAAM TC4 and TC11 samples were stable at 0.472 and 0.432 under 60 N, respectively. The average yield strength, average ultimate strength, proportion of HAGBs, and microhardness of TC11 alloy were all higher than that of TC4 alloy. These results indicated that TC11 alloy had advantages over TC4 alloy in terms of mechanical properties and microstructure, with higher strength and deformation resistance. The properties of titanium alloy samples prepared by MWAAM were not lower than those of titanium alloy samples prepared by single wire WAAM, while MWAAM significantly better than single wire WAAM in deposition efficiency. The results obtained in this paper can help to prepare titanium alloy components with excellent mechanical properties more efficiently in MWAAM process.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. The effect of vanadium on the microstructure and mechanical properties of TiAl alloy fabricated by twin-wire directed energy deposition-arc10.1007/978-3-031-04721-3 ↗
2. Large-size ultra-high strength-plasticity aluminum alloys fabricated by wire arc additive manufacturing via added nanoparticles10.1016/j.msea.2023.144582 ↗
3. Prospects of producing aluminum parts by wire arc additive manufacturing (WAAM)10.1016/j.matpr.2022.02.137 ↗
4. High strength Ti alloy fabricated by directed energy deposition with in-situ Cu alloying10.1016/j.jmatprotec.2022.117759 ↗
5. Invited review article: strategies and processes for high quality wire arc additive manufacturing
6. Phase stability and mechanical properties of wire plus arc additively manufactured H13 tool steel at elevated temperatures10.1016/j.jmst.2020.04.085 ↗
7. Microstructure evolution and mechanical properties of the wire plus arc additive manufacturing Al-Cu alloy
8. Tailoring the surface finish, dendritic microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy by magnetic arc oscillation
9. The state of the art for Wire Arc additive manufacturing process of titanium alloys for aerospace applications10.1007/s11665-022-07128-1 ↗
10. Applications of wire arc additive manufacturing (WAAM) for aerospace component manufacturing10.1007/s00170-023-11623-7 ↗
11. A high deposition efficiency method for wire arc additive manufacturing10.1080/02670836.2023.2177805 ↗
12. Multi-wire arc additive manufacturing of Ti basic heterogeneous alloy: effect of deposition current on the microstructure, mechanical property and corrosion-resistance10.1016/j.jallcom.2022.166056 ↗
13. Grain refinement of additive manufactured Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy by the addition of La2O310.1016/j.matlet.2020.128170 ↗
14. Mechanical performance and microstructural characterisation of titanium alloy-alloy composites built by wire-arc additive manufacture10.1016/j.msea.2019.138289 ↗
15. Mechanism of corrosion protection in reinforced Ti-6Al-4 V alloy by wire arc additive manufacturing using magnetic arc oscillation10.1016/j.matchar.2023.112844 ↗
16. Laser additive manufacture of titanium alloys
17. Research progress and prospects of CMT-based Wire Arc additive manufacturing technology for titanium alloys
18. A review on wire and arc additive manufacturing of titanium alloy10.1016/j.jmapro.2021.08.018 ↗
19. Selective laser melting-wire arc additive manufacturing hybrid fabrication of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.msea.2016.12.065 ↗
20. Wire arc additive manufacturing (WAAM): a new process to shape engineering materials10.1016/j.matpr.2020.08.030 ↗
21. Effect of deposition rate on microstructure and mechanical properties of wire arc additive manufacturing of Ti-6Al-4V components10.1007/s11771-021-4683-0 ↗
22. Experimental investigation of the influence of Wire Arc additive manufacturing on the machinability of titanium parts10.3390/met10010024 ↗
23. Hybrid manufacturing of components from Ti-6Al-4V by metal forming and wire-arc additive manufacturing10.1016/j.jmatprotec.2020.116689 ↗
24. Microstructural characterisation and mechanical properties of Ti-5Al-5V-5Mo-3Cr built by wire and arc additive manufacture10.1080/14786435.2022.2113470 ↗
25. Enhanced crack buffering of additively manufactured Ti–6Al–4V alloy using calcium fluoride particles10.1016/j.jmrt.2023.02.155 ↗
26. Improving mechanical properties of Wire Arc additively manufactured Ti-6Al-4V alloy by ultrasonic needle peening treatment10.3740/MRSK.2021.31.5.245 ↗
27. Dynamic mechanical properties of TC11 titanium alloys fabricated by Wire Arc additive manufacturing10.3390/ma15113917 ↗
28. Multi-wire arc additive manufacturing of TC4-Nb-NiTi bionic layered heterogeneous alloy: microstructure evolution and mechanical properties10.1016/j.matchar.2023.113001 ↗
29. Multi-wire arc additive manufacturing of TC4/Nb bionic layered heterogeneous alloy: microstructure evolution and mechanical properties10.1016/j.msea.2023.145076 ↗
30. Revealing microstructural evolutions, mechanical properties and wear performance of wire arc additive manufacturing homogeneous and heterogeneous NiTi alloy10.1016/j.jmrt.2023.10.055 ↗
31. Analysis of microstructure, mechanical properties, and wear performance of NiTi alloy fabricated by cold metal transfer based wire arc additive manufacturing10.1016/j.jmrt.2022.07.068 ↗
32. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
33. Microstructural tailoring and mechanical properties of a multi-alloyed near β titanium alloy Ti-5321 with various heat treatment10.1016/j.msea.2017.11.029 ↗
34. Effect of molybdenum content on microstructure and mechanical properties of Ti-Mo-Fe alloys by powder metallurgy
35. Dynamic response of Ti-6.5Al-1Mo-1V-2Zr-0.1B alloy fabricated by wire arc additive manufacturing10.1016/j.msea.2020.140310 ↗
36. Microstructure and mechanical properties of TC4/NiTi bionic gradient heterogeneous alloy prepared by multi-wire arc additive manufacturing10.1016/j.msea.2023.144678 ↗
37. Microstructure and mechanical properties of a graded structural material10.1016/j.msea.2014.06.016 ↗
38. Multi-material wire arc additive manufacturing of a bio-inspired heterogeneous layered NiTi/Nb/Ti6Al4V structure: Microstructural evolutions and mechanical properties10.1016/j.msea.2023.145896 ↗
39. Compression behavior of wire + arc additive manufactured structures10.3390/met11060877 ↗
40. Microstructure evolution in compositionally graded Ti(4–12 wt% Mo) prepared by laser directed energy deposition10.1016/j.jmrt.2023.01.215 ↗
41. Analysis of microstructure, mechanical properties, wear characteristics and corrosion behavior of SLM-NiTi under different process parameters10.1016/j.jmapro.2022.01.010 ↗
42. Friction of stable gradient nano-grained metals10.1016/j.scriptamat.2020.04.041 ↗
43. Enhancing hardness and wear performance of laser additive manufactured Ti6Al4V alloy through achieving ultrafine microstructure10.3390/ma13051210 ↗