journal article·2024-03Open access

Revealing the microstructure evolution mechanism and mechanical responses of a novel Al–Zn–Mg–Cu alloy by hot deformation process

Yanmei Yang, Yefei Li, Dawei Yi, Qiaoling Zheng, Xuewei Fang, Yong Wang, Tianxing Chang, Yanan Chen, Yimin Gao, Ke Huang

Abstract

The effect of hot rolling with different rolling deformations on the microstructure evolution and improvement of mechanical properties of the novel Al–Zn–Mg–Cu alloy are investigated via optical microscope (OM), scanning electron microscope (SEM), electron backscattered diffusion (EBSD) and transmission electron microscope (TEM). The findings showed that the equiaxed grains with low dislocation density gradually elongate to become fibrous with high dislocation density as hot rolling deformation growing, and the dynamic dissolution of second-phase particles occurs at the grain boundaries of small dynamic recrystallization (DRX) grains. Dislocation entanglement is formed when a high density of dislocation is clearly visible following various rolling deformations. Dislocation cells could evolve into sub-grains, and ultimately become recrystallized grains as a result of continuous energy absorption. The percentage of low angle grain boundaries (LAGBs) with varying rolling deformation increases swiftly then declines slightly which linked to more deformed grains and sub-grains, as well as less recrystallized grains. High angle grain boundaries (HAGBs), however, show the opposite pattern. Ultimate tensile strength (UTS) and yield strength (YS) of the alloys reach peaks at deformation of 90% (UTS: 620.0 MPa, YS: 583.7 MPa). Which is predominantly attributed to the texture enhancement, grain refinement, and pinning effect of Al3(Sc, Zr, Ti) particles of L12 structure on the grain boundaries and dislocations.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Hot compressive deformation behavior and microstructural evolution of the spray formed 1420 Al–Li alloy10.1016/j.jmrt.2023.10.191 ↗
2. Wire and arc additive manufacturing of dissimilar 2319 and 5B06 aluminum alloys10.1016/j.jmst.2022.02.024 ↗
3. Achieving high strength-ductility synergy through high-density coherent precipitation in twin-roll cast Al–Zn–Mg–Cu strips
4. Effect of Cu content and Zn/Mg ratio on microstructure and mechanical properties of Al–Zn–Mg–Cu alloys10.1016/j.jmrt.2022.06.059 ↗
5. Low cycle fatigue behavior and fatigue life prediction of 2195 Al-Li alloy at warm temperatures10.1016/S1003-6326(23)66282-X ↗
6. Effects of minor Zr and Er on microstructure and mechanical properties of pure aluminum10.1016/j.msea.2013.05.035 ↗
7. Effect of combined addition of Zr, Ti and Y on microstructure and tensile properties of an Al-Zn-Mg-Cu alloy
8. Criteria for developing castable, creep-resistant aluminum-based alloys: a review10.3139/146.101249 ↗
9. Microstructure and mechanical properties of spray-deposited Al–Zn–Mg–Cu alloy processed through hot rolling and heat treatment10.1016/j.msea.2009.05.052 ↗
10. On the role of Sc or Er micro-alloying in the microstructure evolution of Al-Mg alloy sheets during annealing10.1016/j.matchar.2019.109918 ↗
11. Microstructure evolution and high-temperature performances of AA6111 alloy strengthened by Sc, Zr co-microalloying10.1016/j.msea.2023.145788 ↗
12. Effects of minor Sc on the microstructure and mechanical properties of Al-Zn-Mg-Cu-Zr based alloys10.1007/s12598-009-0020-8 ↗
13. Effects of Er and Zr additions on precipitation and recrystallization of pure aluminum10.1016/j.scriptamat.2012.09.026 ↗
14. Effect of Zr, Er and Cr additions on microstructures and properties of Al–Zn–Mg–Cu alloys10.1016/j.msea.2014.05.021 ↗
15. Effect of minor Er and Zr on microstructure and mechanical properties of Al–Mg–Mn alloy (5083) welded joints10.1016/j.msea.2012.11.002 ↗
16. Effect of Zr addition on hot deformation behavior and microstructural evolution of AA7150 aluminum allo10.1016/j.msea.2013.12.057 ↗
17. Effects of Ti addition on the microstructure and mechanical properties of Al–Zn–Mg–Cu–Zr alloy
18. Comparative study of Sc and Er addition on microstructure, mechanical properties, and electrical conductivity of Al-0.2Zr-based alloy cables10.1016/j.matchar.2018.08.037 ↗
19. Microstructure and mechanical properties of cast Al-Ce-Sc-Zr-(Er) alloys strengthened by Al11Ce3 micro-platelets and L12 Al3(Sc,Zr,Er) nano-precipitates10.1016/j.actamat.2022.118354 ↗
20. Improved strength and ductility on laser beam welded joints of 7085Al matrix nanocomposites by in-situ ZrB2 nanoparticles and Al3(Er, Zr) nanoprecipitates10.1016/j.compositesb.2023.110990 ↗
21. Study on the dynamic and static softening phenomena in Al–6Mg alloy during two-stage deformation through interrupted hot compression test10.1016/j.measurement.2015.08.033 ↗
22. Influence of roll speed difference on microstructure, texture and mechanical properties of 7075 aluminum plates produced via combined continuous casting and rolling process10.1016/S1003-6326(21)65548-6 ↗
23. Interface microstructure and bonding mechanisms of 7050 aluminum alloy thick plates produced by vacuum roll cladding
24. Texture evolution rate in continuous cast AA5052 aluminum alloy during single pass hot rolling10.1016/j.msea.2007.05.010 ↗
25. Dynamic dissolution and texture evolution of an Al–Cu–Mg–Ag alloy during hot rolling
26. Effects of rolling deformation on precipitation behavior and mechanical properties of Al–Zn–Mg–Cu alloy
27. Effect of deformation routes on the microstructures and mechanical properties of the asymmetrical rolled 7050 Aluminum alloy plates10.1016/j.msea.2018.07.060 ↗
28. Tracking the path of dislocations across ordered Al3Zr nano-precipitates in three dimensions10.1016/j.scriptamat.2013.09.014 ↗
29. Effect of T-phase on microstructure of the hot rolled Al–Cu–Mg alloy
30. Hot workability and dynamic recrystallization behavior of a spray formed 7055 aluminum alloy
31. Microstructure and mechanical properties of powder metallurgy 2024 aluminum alloy during cold rolling10.1016/j.jmrt.2021.09.120 ↗
32. Reducing the yield asymmetry in Mg-5Li-3Al-2Zn alloy by hot-extrusion and multi-pass rolling10.1016/j.jma.2020.06.015 ↗
33. Constitutive behavior and processing maps of a new wrought magnesium alloy ZE20 (Mg-2Zn-0.2Ce)10.1016/j.jma.2019.11.007 ↗
34. Effect of Mg content on the dislocation characteristics and discontinuous dynamic recrystallization during the hot deformation of Al-Mg alloy
35. Microstructures and mechanical properties of AZ91 magnesium alloy processed by multidirectional forging under decreasing temperature conditions10.1016/j.jallcom.2014.08.148 ↗
36. Hot tensile deformation behavior and a fracture damage model of the wrought Mg–Gd−Y–Zn–Zr alloy10.1016/j.jmrt.2022.12.064 ↗
37. Influence of heat treatment on the microstructure, texture and formability of 2024 aluminium alloy10.1016/j.msea.2012.04.113 ↗
38. Modelling of recrystallisation textures in aluminium alloys: II. Model performance and experimental validation10.1016/j.actamat.2006.03.019 ↗
39. Experimental analysis of deformation texture evolutions in pure Cu, Cu-37Zn, Al-6Mg, and −8Mg alloys at cold-rolling processes
40. Effect of pre-stretching deformation treatment process on microstructure and mechanical properties of Al-Cu-Mg alloy