Effect of different heat input on the microstructure and mechanical properties of laser cladding repaired 300M steel
Source abstract
Abstract
Laser cladding repair technology is valued for its ability to repair of damaged parts with high performance. However, there are so many parameters affect the repair quality that it takes a lot of work to determine the optimal parameters. In this article, a variety of parameters were combined as dimensionless heat input (Q∗), and the effect of Q∗ on the microstructure and mechanical properties of 300M steel repaired samples were studied. Results showed that with the increase of Q∗, microstructure of heat affected zone transformed from tempered martensite to tempered martensite and low bainite. The microstructure of the repaired zone transformed from untempered martensite to untempered martensite and a small amount of retained austenite. With increasing of Q∗, residence time above the austenitizing temperature was extended, and more uniform microstructure were obtained in the repaired zone. What's more, at Q∗ = 5.1, the repair efficiency increases twice than Q∗ = 1. The tensile strength of the repaired samples reached 1017.6 MPa and the elongation reached 6.9%, which were far lower than that of forged samples. The heat treatment was carried out on the repaired parts, which eliminated the microstructure difference due to different Q∗. Compared with the repaired samples without heat treatment, the tensile strength increased by 75% to 1783.8 MPa and the elongation increased by 86% to 10.4%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Effect of clad orientation on the mechanical properties of laser-clad repaired ultra-high strength 300M steel
2. Additive metal technologies for aerospace sustainment10.1016/B978-0-08-100540-8.00015-7 ↗
3. Effect of solution temperature on the microstructure and mechanical properties of Hastelloy X superalloy fabricated by laser directed energy deposition
4. Effect of tempering temperature on microstructure and mechanical properties of laser solid formed 300 steel10.1016/j.jallcom.2016.07.276 ↗
5. Intensive laser repair through additive manufacturing of high-strength martensitic stainless steel powders (I) — powder preparation, laser cladding and microstructures and properties of laser-cladded metals10.1016/j.jmrt.2021.10.109 ↗
6. Multi-index co-evaluation of metal laser direct deposition: an investigation of energy input effect on energy efficiency and mechanical properties of 316L parts10.1016/j.jmapro.2022.02.016 ↗
7. Plastic strain localization induced by microstructure gradient in laser cladding repaired structures10.1016/j.tafmec.2020.102520 ↗
8. Effect of laser clad repair on the fatigue behavior of ultra-high strength AISI 4340 steel10.1016/j.msea.2014.03.077 ↗
9. Analysis of the stress raising action of flaws in laser clad deposits10.1016/j.matdes.2012.10.010 ↗
10. To study the laser cladding of ultra high strength AerMet-100 alloy powder on AISI-4340 steel for repair and refurbishment10.1016/j.matpr.2020.09.154 ↗
11. Effect of Ti on T15M composite coating fabricated by laser cladding technology10.1016/j.surfcoat.2017.07.008 ↗
12. Additive manufacturing of metallic components-Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
13. High strength and ductility of 34CrNiMo6 steel produced by laser solid forming10.1016/j.jmst.2018.09.062 ↗
14. Defect formation and prevention in directed energy deposition of high-manganese steels and the effect mechanical properties10.1016/j.msea.2019.138688 ↗
15. Cracking mechanism of Hastelloy X superalloy during directed energy deposition additive manufacturing
16. Elimination of Start/Stop defects in laser cladding10.1016/j.surfcoat.2011.10.040 ↗
17. The influence of stellite 6 particle size on the inter-track porosity in multi-track cladding10.1016/j.surfcoat.2006.01.008 ↗
18. Density analysis of direct metal laser re-melted 316L stainless steel cubic primitives10.1023/B:JMSC.0000013875.62536.fa ↗
19. Effect of laser power on microstructure and interfacial bonding strength of laser cladding 17-4PH stainless steel coatings10.1016/j.matchemphys.2021.125236 ↗
20. Effect of laser power and powder feed rete on interfacial crack and mechanical/microstructural characterizations in repairing of 630 stainless steel using direction energy deposition
21. The effect of cladding speed on phase constitution and properties of AISI 431 stainless steel laser deposited coatings10.1016/j.surfcoat.2011.05.035 ↗
22. Effect of the scanning speed on the microstructure evolution and wear behaviors of laser cladding NiCrBSi composite coatings10.1016/j.optlastec.2015.03.015 ↗
23. Effect of laser scanning speed on the microstructure and wear properties of T15M cladding coating fabricated by laser cladding technology10.1016/j.optlaseng.2018.05.024 ↗
24. Effect of dimensionless heat input during laser solid forming of high-strength steel10.1016/j.jmst.2021.05.038 ↗
25. Effect of microstructure on the fatigue crack growth behavior of laser solid formed 300M steel10.1016/j.msea.2017.04.001 ↗
26. Effect of microstructure on the Charpy impact properties of directed energy deposition 300M steel
27. Influence of molten pool mode on microstructure and mechanical properties of heterogeneously tempered 300M steel by selective laser melting
28. Effects of heat treatment on microstructure and tensile properties of laser melting deposited AISI 431 martensitic stainless steel10.1016/j.msea.2016.04.014 ↗
29. Microstructure evolution and mechanical properties of 308L stainless steel coatings fabricated by laser hot wire cladding
30. Microstructural of additively manufactured metallic materials10.1146/annurev-matsci-070115-031816 ↗
31. Microstructure and mechanical properties of laser solid formed 300 steel10.1016/j.jallcom.2014.09.111 ↗