Formation, evolution and remove behavior of manganese-containing inclusions in medium/high manganese steels

Jianhua Chu, Yi Nian, Liqiang Zhang, Yanping Bao, Naqash Ali, Chaojie Zhang, Hongwei Zhou

Abstract

The effect of manganese content, aluminium content, top slag and stirring on manganese-containing inclusions characteristics was investigated by laboratory thermal experiments and precipitation thermodynamics calculation. The results indicated that the types of manganese-containing inclusions in manganese steel were mainly single MnS, MnS–Al2O3, MnS–TiN and MnS–Al2O3–TiN complex inclusions. The morphology of manganese-containing inclusions was transformed from spherical and ellipsoidal to polyhedral as result of manganese content increased, which is attributed to large solidus-liquidus phase difference of high manganese steel, promoting the formation of type III MnS. It is also found that the manganese-containing inclusions shows irregular morphology with clear angularities after addition of aluminium, which was determined by both formation of flaky AlN and type III MnS with polygonal caused by increased of activity coefficient of S and the surface tension of molten steel. Furthermore, the manganese-containing inclusions in manganese steel is considered MnS–MnO type with top salg, in which patchy or multipoint shape MnS is embedded on the surface of oxide. The force field analysis in induction stirring demonstrated that the inclusion particles are removed by top slag and refractory adsorption under the action of strong electromagnetic force and buoyancy. This work provides an improved understanding for the controlling and removing of manganese-containing inclusions in high quality medium/high manganese steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Introduction and mechanical evaluation of a novel 3rd-generation medium manganese AHSS with 86 GPa% of PSE10.1016/j.msea.2022.143104 ↗
2. Effect of annealing time on the microstructure and mechanical properties of aluminum added low-density medium manganese steel10.1016/j.matlet.2022.132211 ↗
3. Ce addition enabling superior strength and ductility combination of a low-carbon low-manganese transformation-induced plasticity steel10.1016/j.msea.2022.143474 ↗
4. Potential significance of low tempering treatment in improving the mechanical properties of a cold-rolled and intercritical annealed medium Mn steel10.1002/srin.202100814 ↗
5. Influences of manganese content and heat treatment on mechanical properties of precipitation-strengthened steels10.1016/j.msea.2022.142724 ↗
6. Revealing the cryogenic-temperature toughness and deformation mechanisms in high manganese austenitic steels10.1016/j.matchar.2022.112024 ↗
7. Effects of cerium addition on the microstructure, mechanical properties and strain hardening behavior of TWIP steel Fe-18Mn-0.6C10.1016/j.matchar.2021.111626 ↗
8. Argon–oxygen decarburization of high-manganese steels: effect of alloy composition10.1002/srin.202000480 ↗
9. Study on the relationship between vacuum denitrification and manganese evaporation behaviours of manganese steel melts10.1016/j.vacuum.2021.110420 ↗
10. Kinetic study of Mn vacuum evaporation from Mn steel melts10.1016/j.seppur.2020.117698 ↗
11. Characterization of oxidation behavior of Mn fumes generated in the vacuum treatment of melting Mn steels10.1002/srin.202170011 ↗
12. Reaction of Al-killed manganese steel with ladle slag10.1002/srin.201800480 ↗
13. A reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: Part I. Composition evolution in molten mold flux10.1007/s11663-012-9770-z ↗
14. Steel/refractory/slag interfacial reaction and its effect on inclusions in high-Mn high-Al steel10.1016/j.ceramint.2021.09.194 ↗
15. Inclusion engineering in medium Mn steels: effect of hot-rolling process on the deformation behaviors of oxide and sulfide inclusions10.1007/s11663-021-02363-8 ↗
16. In-situ observation of peritectic solidification of Fe-Mn-Al-C steel with medium manganese10.1016/j.jallcom.2022.164750 ↗
17. Non-metallic inclusions in high manganese austenitic alloys
18. Non-metallic inclusions in high-manganese-alloy steels10.1002/srin.200506069 ↗
19. Characterization of nonmetallic inclusions in high-manganese and aluminum-alloyed austenitic steels10.1007/s11661-012-1088-6 ↗
20. Effect of aluminium content on the formation of inclusions in Fe–5Mn–xAl steels, Ironmak10.1080/03019233.2020.1791549 ↗
21. Effect of Al content on non-metallic inclusions in Fe–23Mn–xAl–0.7C lightweight steels, Ironmak10.1080/03019233.2021.1909993 ↗
22. Evolution mechanism of inclusions in medium-manganese steel by Mg treatment with different aluminum contents10.1007/s11663-019-01514-2 ↗
23. Effects of Al addition on the reaction between high-manganese steel and CaO–SiO2–Al2O3–MgO slag10.1002/srin.202000143 ↗
24. Effect of Al content on the reaction between Fe-10Mn-xAl (x = 0.035wt%, 0.5wt%, 1wt%, and 2wt%) steel and CaO-SiO2-Al2O3-MgO slag10.1007/s12613-021-2298-y ↗
25. The effect of cooling conditions on the evolution of non-metallic inclusions in high manganese TWIP steels10.1007/s11663-015-0568-7 ↗
26. Extraction, thermodynamic analysis, and precipitation mechanism of MnS-TiN complex inclusions in low-sulfur steels10.1007/s11661-016-3463-1 ↗
27. MnS precipitation behavior in MnO–SiO2 inclusion in Fe–Mn–Si–O–S alloy system at solid-liquid coexistence temperature10.2355/isijinternational.ISIJINT-2019-777 ↗
28. Nucleation catalysis10.1021/ie50510a031 ↗
29. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
30. Characterization transformation of inclusions using rare earth Ce treatment on Al-killed titanium alloyed interstitial free steel10.1002/srin.201970101 ↗
31. The effect of aluminum on the divorced eutectic transformation of MnS inclusions10.1007/s11663-021-02085-x ↗
32. Interfacial Reaction between CaO-SiO2-MgO-Al2O3 Flux and Fe-xMn-yAl (x= 10 and 20 mass pct, y= 1, 3, and 6 mass pct) Steel at 1873 K (1600 C)10.1007/s11663-012-9667-x ↗
33. MnS precipitation in association with manganese silicate inclusions in Si/Mn deoxidized steel10.1007/s11661-001-0239-y ↗
34. Electromagnetic separation of coarse Al–Si melts: the migration behavior of iron-rich phase and continuous growth of primary silicon10.1016/j.jallcom.2019.153006 ↗
35. Removal of SiC particles from solar grade silicon melts by imposition of high frequency magnetic field10.1016/S1003-6326(11)61537-9 ↗
36. Separation of SiC from Si by addition of Al with electromagnetic induction melting, J. Alloy10.1016/j.jallcom.2020.155310 ↗
37. Application of electromagnetic (EM) separation technology to metal refining processes: a review10.1007/s11663-014-0123-y ↗