journal article·2023-07Open access

Fracture behavior of a high pressure die casting AlSi10MnMg alloy with varied porosity levels

X.Y. Jiao, P.Y. Wang, Y.X. Liu, J. Wang, W.N. Liu, A.X. Wan, L.J. Shi, C.G. Wang, S.M. Xiong

Abstract

The fracture behavior of a high pressure die casting AlSi10MnMg alloy with varied porosity levels is investigated by synchrotron radiation X-ray computed tomography. Attention is focused on origin of crack and the evolution of porosity in the process of plastic deformation. Different from in-situ 3D tensile test, load-off specimen after plastic deformation is applied for this experiment and it is closer to the real scene. Results show that multiple defects are proposed in high pressure die casting AlSi10MnMg alloy including shrinkage, gas pore, externally solidified primary iron-rich phase (ESC-IMCI) and heterogeneous layers. In a lower-porosity sample, the surface defects like skin layer are a main crack source and a radial river pattern exhibits in crack surface. No new pores generated in the process of plastic deformation. In a higher-porosity sample, no obvious crack source and radial crack propagation path can be identified while the large crack surface fluctuation and tortuous morphology are obtained. The collapse of pre-existing small-sized pores exert a vital role in connecting large-scale pores. The micro-crack initiation and propagation originate from the expansion, consolidation and collapse of pores, especially the irregular pores.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Alloy development and process innovations for light metals casting10.1016/j.jmatprotec.2022.117606 ↗
2. Processing of light metals for enhanced performance10.1016/0924-0136(94)01707-8 ↗
3. Design and microstructural analysis of magnesium alloys for dynamical applications10.1007/s10853-011-5400-4 ↗
4. Low-cyclic fatigue behavior of peak-aged Mg–Nd-based alloy10.1007/s11661-021-06465-5 ↗
5. The effect of slow shot speed and casting pressure on the 3D microstructure of high pressure die casting AE44 magnesium alloy10.1016/j.jma.2021.09.011 ↗
6. A study of die design of semi-solid die casting according to gate shape and solid fraction10.1016/j.jmatprotec.2008.01.038 ↗
7. New HPDC Mg-RE based alloy with exceptional strength and creep resistance at elevated temperature10.1016/j.msea.2022.142921 ↗
8. Influence of wall thickness and intensification pressure on the microstructures and mechanical properties of AlSi7-SiC composites fabricated by the vacuum-assisted HPDC process10.1016/j.msea.2021.141470 ↗
9. Influence of porosity characteristics on the variability in mechanical properties of high pressure die casting (HPDC) AlSi7MgMn alloys10.1016/j.jmapro.2020.04.071 ↗
10. Kinetic analysis of pore formation in die-cast metals and influence of absolute pressure on porosity10.1016/j.vacuum.2019.108828 ↗
11. Segregation band formation in Al-Si die castings10.1007/s11661-004-0236-z ↗
12. Migration of crystals during the filling of semi-solid castings10.1007/s11661-005-0195-z ↗
13. Fluidity of alloys under high-pressure die casting conditions: flow-choking mechanisms10.1007/s11663-020-01858-0 ↗
14. Characterization of externally solidified crystals in a high-pressure die-cast AlSi10MnMg alloy and their effect on porosities and mechanical properties10.1016/j.jmatprotec.2021.117299 ↗
15. Influence of pore characteristics and eutectic particles on the tensile properties of Al–Si–Mn–Mg high pressure die casting alloy10.1016/j.msea.2020.139280 ↗
16. Skin solidification during high pressure die casting of Al–11Si–2Cu–1Fe alloy10.1016/S0921-5093(02)00747-5 ↗
17. The formation mechanism of the chill fine-grain layer with high supersaturation and its influence on the mechanical properties of die casting Al-7Si-0.5Mg alloy10.1016/j.msea.2021.142544 ↗
18. Origins of variability in the fracture-related mechanical properties of a tilt-pour-permanent-mold cast Al-alloy10.1016/j.scriptamat.2004.09.011 ↗
19. Variability in the tensile properties of squeeze-cast Al–Si–Cu–Mg alloy10.1016/j.msea.2007.11.014 ↗
20. Constitutive prediction of the defect susceptibility of tensile properties to microporosity variation in A356 aluminum alloy10.1016/j.msea.2014.01.091 ↗
21. An extended model for void growth and coalescence10.1016/S0022-5096(00)00019-3 ↗
22. Micromechanics of room and high temperature fracture in 6xxx Al alloys10.1016/j.pmatsci.2006.06.001 ↗
23. Initiation and growth of damage in a dual-phase steel observed by X-ray microtomography10.1016/j.actamat.2008.06.015 ↗
24. Characterization and micromechanical modelling of microstructural heterogeneity effects on ductile fracture of 6xxx aluminium alloys10.1016/j.actamat.2015.10.008 ↗
25. 4D imaging of void nucleation, growth, and coalescence from large and small inclusions in steel under tensile deformation10.1016/j.jmst.2022.01.024 ↗
26. Quantifying the effect of porosity on the evolution of deformation and damage in Sn-based solder joints by X-ray microtomography and microstructure-based finite element modeling10.1016/j.actamat.2012.03.048 ↗
27. The imaging of failure in structural materials by synchrotron radiation X-ray microtomography10.1016/j.engfracmech.2017.07.027 ↗
28. Shear fracture mechanism in micro-tension of an ultrafine-grained pure copper using synchrotron radiation X-ray tomography10.1016/j.scriptamat.2017.01.021 ↗
29. Defect evolution during high temperature tension-tension fatigue of SLM AISi10Mg alloy by synchrotron tomography10.1016/j.msea.2020.139809 ↗
30. A new approach to correlate the defect population with the fatigue life of selective laser melted Ti-6Al-4V alloy10.1016/j.ijfatigue.2020.105584 ↗
31. The role of defects on tensile deformation and fracture mechanisms of AM AlSi10Mg alloy at room temperature and 250 °C10.1016/j.engfracmech.2021.108215 ↗
32. 4D imaging of void nucleation, growth, and coalescence from large and small inclusions in steel under tensile deformation10.1016/j.jmst.2022.01.024 ↗
33. Brown · 1969
34. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
35. The skin effect and the yielding behavior of cold chamber high pressure die cast Mg–Al alloys10.1016/j.msea.2012.02.029 ↗
36. On the tensile failure induced by defect band in high pressure die casting of AM60B magnesium alloy10.1016/j.msea.2016.08.039 ↗