journal article·2023-05Open access

Introducing lamellar LPSO phase to regulate room and high-temperature mechanical properties of Mg-Gd-Y-Zn-Zr alloys by altering cooling rate

Jianxin Zhou, Xiaojun Luo, Hong Yang, Bin Jiang, Wenlong Xie, Zhihua Dong, Jiangfeng Song, Junyao Xu, Guangsheng Huang, Dingfei Zhang, Fusheng Pan

Abstract

The mechanical properties of the extruded and peak-aged Mg-12.8Gd-4.7Y-2.6Zn-0.9Zr (wt.%) (GWZ1352) alloys at room and high temperatures were systematically investigated with respect to their microstructures. The microstructural features were tailored through altering the cooling rates after homogenization by water-quenching, air-cooling and furnace-cooling, respectively. As the cooling rate reduced, the number of lamellar long period stacking ordered (LPSO) phase increased substantially and its spacing decreased gradually. Additionally, solute segregation at grain boundaries occurred after furnace-cooling. After extrusion, the quenching (QE) alloy exhibited nearly full dynamic recrystallized (DRXed) grains, whereas the air-cooling (AE) and furnace-cooling (FE) alloys displayed a typical bimodal structure consisting of fine DRXed and coarse un-DRXed grains. The nucleation and development of the DRXed grains were hampered by the nano-spaced lamellar LPSO phase and the solute segregation of grain boundary. The excellent high temperature mechanical properties of the FE alloy were mostly due to the abundant lamellar LPSO phase. After aging treatment, plentiful fine β′ phase was precipitated in the quenching and aged (QEA) alloy. In contrast, the β′ phase with a larger size and lower density, accompanied with a wide precipitation-free zone (PFZ) at grain boundaries was formed in the air-cooling and aged (AEA) and furnace-cooling and aged (FEA) alloys, which severely deteriorated their mechanical properties both at room and high temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Magnesium casting technology for structural applications10.1016/j.jma.2013.02.002 ↗
2. Origin of the low precipitation hardening in magnesium alloys10.1016/j.actamat.2018.11.044 ↗
3. A combined method for producing high strength and ductility magnesium microtubes for biodegradable vascular stents application10.1016/j.jallcom.2017.06.201 ↗
4. Microstructures and tensile properties of Mg–Zn–(Gd)–Zr alloys extruded at various temperatures10.1007/s12598-017-0966-x ↗
5. Elastic properties of an Mg–Zn–Y alloy single crystal with a long-period stacking-ordered structure10.1016/j.actamat.2013.06.041 ↗
6. Dislocation structure in rapidly solidified Mg97Zn1Y2 alloy with long period stacking order phase[J]10.2320/matertrans.46.361 ↗
7. Rapidly solidified powder metallurgy Mg97Zn1Y2Alloys with excellent tensile yield strength above 600 MPa[J]10.2320/matertrans.42.1172 ↗
8. Microstructural evolution and aging behavior of Mg–4.5Y–2.5Nd–1.0Gd–0.5Zr alloys with different Zn additions10.1007/s12598-020-01510-5 ↗
9. Recent developments in high-strength Mg-RE-based alloys: focusing on Mg-Gd and Mg-Y systems10.1016/j.jma.2018.08.001 ↗
10. Cooling rate controlled basal precipitates and age hardening response of solid-soluted Mg–Gd–Er–Zn–Zr alloy10.1016/j.jma.2020.06.014 ↗
11. Precipitate evolution of as-cast Mg-9Gd-2Y-0.5Zn-0.5Zr alloy containing LPSO, β′′, β′ and γ'' phases during isothermal aging at 200°C10.1016/j.jallcom.2022.165476 ↗
12. Microstructures and mechanical properties of titanium-reinforced magnesium matrix composites: review and perspective10.1016/j.jma.2022.07.008 ↗
13. Evolution of LPSO phases and their effect on dynamic recrystallization in a Mg-Gd-Y-Zn-Zr Alloy10.1007/s11661-017-4081-2 ↗
14. Improved workability for Mg-Y-Zn alloys via increased volume fraction of block LPSO phases10.1016/j.msea.2020.139934 ↗
15. Microstructure and mechanical properties of extruded Mg-Gd-Y-Zn-Zr alloys filled with intragranular LPSO phases10.1016/j.matchar.2017.11.027 ↗
16. Tensile behavior at various temperatures of the Mg-Gd-Y-Zn-Zr alloys with different initial morphologies of LPSO phases prior to extrusion10.1016/j.msea.2022.143634 ↗
17. Effect of LPSO and SFs on microstructure evolution and mechanical properties of Mg-Gd-Y-Zn-Zr alloy
18. Ageing behavior and mechanisms of strengthening and toughening of ultrahigh-strength Mg-Gd-Y-Zn-Mn alloy10.1016/j.msea.2019.05.005 ↗
19. Effect of Sm on microstructures and mechanical properties of Mg–Gd(–Sm)–Zr alloys by hot extrusion and aging treatment10.1016/j.jmrt.2022.06.128 ↗
20. Solute segregation and precipitation in a creep-resistant Mg–Gd–Zn alloy10.1016/j.actamat.2008.08.025 ↗
21. Formation of enclosed precipitates structure in a novel Mg-RE alloy to enhance high-temperature mechanical properties, Mater
22. Evolution of the hardening precipitates with an enclosed structure in pre-deformed Mg-Sm-Nd-Zn-Zr alloy10.1016/j.matlet.2019.03.060 ↗
23. Tuning texture and precipitation using Y/Gd atomic ratio in iso-concentration Mg–Y–Gd–Ag–Zr extruded alloys10.1016/j.matchar.2020.110473 ↗
24. Thermodynamics-based selection and design of creep-resistant cast Mg alloys10.1007/s11661-015-3128-5 ↗
25. The relationship between (Mg,Zn)3RE phase and 14H-LPSO phase in Mg–Gd–Y–Zn–Zr alloys solidified at different cooling rates10.1016/j.jallcom.2010.12.136 ↗
26. Clarifying the deformation modes and strengthening mechanisms of Mg-11Gd-5Y-2Zn-0.7Zr with outstanding high-temperature mechanical properties10.1016/j.msea.2023.144638 ↗
27. Materials advances through aberration-corrected electron microscopy10.1557/mrs2006.4 ↗
28. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
29. Precipitation in a Mg–10Gd–3Y–0.4Zr (wt.%) alloy during isothermal ageing at 250°C10.1016/j.jallcom.2005.11.046 ↗
30. Characterisation of strengthening precipitate phases in a Mg–Y–Nd alloy[J]10.1016/S1359-6454(00)00013-6 ↗
31. A detailed HAADF-STEM study of precipitate evolution in Mg–Gd alloy10.1016/j.jallcom.2018.10.193 ↗
32. Effect of Zn additions on the age-hardening of Mg–2.0Gd–1.2Y–0.2Zr alloys10.1016/j.actamat.2007.02.036 ↗
33. Characterization of planar features in Mg–Y–Zn alloys10.1016/j.actamat.2009.09.025 ↗
34. Polytypes of long-period stacking structures synchronized with chemical order in a dilute Mg–Zn–Y alloy10.1080/09500839.2011.609149 ↗
35. Growth and transformation mechanisms of 18R and 14H in Mg–Y–Zn alloys10.1016/j.actamat.2012.08.022 ↗
36. The evolution of internal strain in Mg–Y–Zn alloys with a long period stacking ordered structure10.1016/j.scriptamat.2011.07.017 ↗
37. Influence of alloying element segregation at grain boundary on the microstructure and mechanical properties of Mg-Zn alloy10.1016/j.matdes.2022.111322 ↗
38. Strengthening and toughening mechanisms in Mg–Zn–Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
39. Strengthening mechanisms acting in extruded Mg-based long-period stacking ordered (LPSO)-phase alloys10.1016/j.actamat.2018.10.016 ↗
40. Atomic-scale segregations at the deformation-induced symmetrical boundary in an Mg-Zn-Y alloy10.1016/j.actamat.2016.07.054 ↗
41. Evolution of long-period stacking ordered phases and their effect on recrystallization in extruded Mg-Gd-Y-Zn-Zr alloy during annealing10.1016/j.matchar.2020.110515 ↗
42. Development of extruded Mg-6Er-3Y-1.5Zn-0.4Mn (wt.%) alloy with high strength at elevated temperature10.1016/j.jmst.2019.05.053 ↗
43. Effect of the interspacing of intragranular lamellar LPSO phase on dynamic recrystallization behaviors of Mg-Gd-Y-Zn-Zr alloys10.1016/j.matchar.2022.112326 ↗
44. Analysis of abnormal texture formation and strengthening mechanism in an extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.jmst.2019.11.021 ↗
45. Formation mechanism of the abnormal texture during extrusion in Mg-Y-Sm-Zn-Zr alloy10.1016/j.jallcom.2019.153477 ↗
46. Phase transformations in metals and alloys[M]
47. Effect of heat treatment variables on the formation of precipitate free zones (PFZs) in Mg-8Al-0.5Zn alloy10.1016/j.matchar.2017.12.018 ↗
48. High tensile ductility and strength in bulk nanostructured nickel10.1002/adma.200800214 ↗
49. Microstructure evolution and mechanical behavior of a binary Al–7Mg alloy processed by equal-channel angular pressing10.1016/j.actamat.2014.10.025 ↗
50. Synergic effects of Gd and Y contents on the age-hardening response and elevated-temperature mechanical properties of extruded Mg–Gd(-Y)-Zn-Mn alloys10.1016/j.msea.2021.141019 ↗
51. Effect of grain size on slip activity in pure magnesium polycrystals10.1016/j.actamat.2014.10.001 ↗
52. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
53. Weak strengthening effect of the precipitated lamellar phase in the homogenized Mg-8Gd-4Y-1.6Zn-0.5Zr (wt%) alloy followed by furnace cooling10.1016/j.msea.2018.08.056 ↗
54. Modeling the temperature dependent effect of twinning on the behavior of magnesium alloy AZ31B sheet10.1016/j.msea.2006.03.160 ↗
55. Role of Yb in enhancing the heat resistance of cast Mg-Sm-Zn alloy10.1016/j.msea.2022.143009 ↗
56. Effect of Gd content on high temperature mechanical properties of Mg–Gd–Y–Zr alloy10.1016/j.msea.2015.11.047 ↗
57. In-situ analysis of the tensile deformation modes and anisotropy of extruded Mg-10Gd-3Y-0.5Zr (wt.%) at elevated temperatures10.1016/j.ijplas.2016.06.001 ↗
58. Formation of denuded zones in crept Mg–2.5Gd–0.1Zr alloy10.1016/j.actamat.2014.10.046 ↗