Directed energy deposition of Invar 36 alloy using cold wire pulsed gas tungsten arc welding: Effect of heat input on the microstructure and functional behaviour
Source abstract
Abstract
Invar alloys exhibit low thermal expansion and are useful in applications requiring dimensional stability when subject to temperature changes. Conventional production of Invar faces certain challenges that can be offset by exploiting additive manufacturing processes. This study employed pulsed gas tungsten arc welding (GTAW) to deposit Invar 36 alloy blocks at five heat inputs (HI) ranging from 200–550 J mm-1. The results show that the microstructure comprised of columnar grains and remained in the austenitic phase regardless of the HI. Ductility dip cracking was found to prevail in all the blocks except the block deposited at the lowest HI. The decreased susceptibility to cracking with a reduction in the HI was due to the preservation of the grain boundary area, consequently leading to an improved partitioning of strain among the grain boundaries. On lowering the HI from 550 to 200 J mm-1 the average yield strength, tensile strength and elongation improved by 16%, 23% and 38%, respectively. The HI had a negligible effect on the mean linear coefficient of thermal expansion (CTE) in different temperature ranges as the CTE values were nearly identical between the blocks deposited at 200 and 550 J mm-1. In general, the CTE in the building direction was slightly higher than the travel direction, with a maximum difference between the CTE of the two directions being 15%. In summary, this work demonstrates the application of the cold wire GTAW process as an alternative to conventional/laser based methods for realizing the functional properties of Invar.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. The invar problem10.1109/TMAG.1976.1059049 ↗
2. Lnvar alloys10.1016/S1359-0286(96)80023-4 ↗
3. Relation between anomalous magnetovolume behavior and magnetic frustration in Invar alloys10.1103/PhysRevB.54.12225 ↗
4. Davis · 1998
5. 1990 · 2
6. Thyssenkrupp · Stainless Steel · 2017 · 316L · 11
7. S. Yamamo. World's first invar alloy LNG piping under the seabed. The 14th International Conference & Exhibition on Liquefied Natural Gas. Poster Session. PO-13.
8. Weldability of Invar and its large-diameter pipe
9. Welding of invar Fe-36Ni alloy for tooling of composite materials10.1080/09507119809448543 ↗
10. The selection of process parameters in additive manufacturing for aerospace alloys10.1007/s00170-017-0280-7 ↗
11. Yakout · 2018 · 405
12. Allen · 2006
13. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
14. Additive manufacturing and its societal impact: a literature review10.1007/s00170-012-4558-5 ↗
15. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
16. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
17. Current status and perspectives on wire and arc additive manufacturing (WAAM)10.3390/ma12071121 ↗
18. Wire-feed additive manufacturing of metal components: technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
19. Selective laser melting of Invar 36: microstructure and properties10.1016/j.actamat.2015.10.020 ↗
20. Thermal expansion coefficients in invar processed by selective10.1007/s10853-017-1169-4 ↗
21. On thermal expansion behavior of invar alloy fabricated by modulated laser powder bed fusion10.1016/j.matdes.2018.10.025 ↗
22. Investigations on density and surface roughness characteristics during selective laser sintering of Invar-36 alloy
23. Microstructures and unique low thermal expansion of Invar 36 alloy fabricated by selective laser melting10.1016/j.matchar.2020.110409 ↗
24. Laser additive manufacturing processing of a mixture of iron and nickel powders
25. Investigation on microstructure and properties of laser solid formed low expansion Invar 36 alloy10.1016/j.jmrt.2020.03.108 ↗
26. Effect of the heat input on wire-arc additive manufacturing of invar 36 alloy: microstructure and mechanical properties10.1007/s40194-022-01295-4 ↗
27. Thermal expansion behaviour of Invar 36 alloy parts fabricated by wire-arc additive manufacturing10.1016/j.jmrt.2022.06.114 ↗
28. Wire-arc additive manufacturing: invar deposition characterization
29. Interfacial microstructure and mechanical properties of Fe-36Ni invar alloy GTAW joint10.1016/j.msea.2016.11.055 ↗
30. Grain coarsening and boundary migration during welding of invar Fe-36Ni alloy10.1016/S1044-5803(98)00020-5 ↗
31. Weldability of Fe-36% Ni alloy (report I): hot cracking with cross-bead test (materials, metallurgy, weldability)
32. Recent gas metal arc welding (GMAW) process developments: the implications related to international fabrication standards10.1007/s40194-017-0463-8 ↗
33. Kou · 2021 · 37
34. Mittal
35. ISO 6892-1:2019(en) Metallic materials — Tensile testing — Part 1: Method of test at room temperature · 2019 · 11
36. 2014
37. Kou · 2021 · 209
38. Wire and arc additive manufacturing: opportunities and challenges to control the quality and accuracy of manufactured parts10.1016/j.matdes.2021.109471 ↗
39. Review on effect of heat input for wire arc additive manufacturing process10.1016/j.jmrt.2021.02.002 ↗
40. Influence of thermal properties on residual stresses in SLM of aerospace alloys10.1108/RPJ-03-2019-0065 ↗
41. Vernyhora · 2012 · 2012
42. The crystal structure of iron-nickel alloys10.1103/PhysRev.21.402 ↗
43. Kurz · 1984
44. Preferred growth direction of metals
45. Deformation microstructural evolution and strain hardening of differently oriented grains in twinning-induced plasticity beta titanium alloy10.1016/j.msea.2016.01.105 ↗
46. Cracking mechanism and susceptibility of laser melting deposited Inconel 738 superalloy10.1016/j.matdes.2019.108105 ↗
47. Welding metallurgy and weldability
48. Kou · 2020 · 379
49. Lippold · 2011 · 47
50. Weldability of Fe-36% Ni alloy (report VI): further investigation on mechanism of reheat hot cracking in weld metal (materials, metallurgy & weldability)
51. An investigation of ductility dip cracking in nickel-based weld metals-Part II: fracture behavior and fracture surface morphology are related to microstructure, composition, and temperature
52. Weldadility of Fe-36% Ni alloy (report V): behaviors of grain-boundary sliding and cavity formation preceding reheat hot cracking in weld metal (materials, metallurgy & weldability)
53. Weldability of Fe-36% Ni alloy (report III): dynamic observation of reheat hot crack and evaluation of hot ductility of reheated weld metal (materials, metallurgy & weldability)
54. Weldability of Fe-36% Ni alloy (report II) : effect of chemical composition on reheated hot cracking in weld metal(materials, metallurgy & weldability)
55. Cullity · 2011
56. Honda · 1978
57. On residual stress development, prevention, and compensation in metal additive manufacturing10.3390/ma13020255 ↗
58. Influence of thermal properties on residual stresses in SLM of aerospace alloys10.1108/RPJ-03-2019-0065 ↗