Laser additive manufacturing of new α+β titanium alloy with high strength and ductility
Source abstract
Abstract
The capability to control volume fraction and morphology of α phase in α+β titanium alloys makes this group of alloys a suitable choice to develop new compositions to deal with the formidable requirement of industrial development. However, further alloying is challenged because of the difficulty of uniform mixing during the melting process and the severe segregation during solidification. Due to the intense convection within small melt pool, additive manufacturing (AM) can achieve uniform concentration distribution and thus is a perfect alloying strategy to exert the potential of more species of alloying elements. To fulfil the potential of alloying, an α+β titanium alloy with new composition was additively manufactured in this study by laser directed energy deposition (LDED). The as-deposited new α+β titanium alloy exhibited near equiaxed prior β grains and intragranular ultrafine basket-weave microstructure in which the thickness of α lath is 0.4±0.1 μm. A fibrous root morphology of primary α (αp) whose thickness is 1.4±0.2 μm formed by macroscopic diffusion in the subsequent annealing process and this special morphology is the main reason of the improvement of ductility. With the aid of this special morphology and the nucleation of fine secondary α (αs), the ultimate tensile strength (UTS) and ductility can reach 1247±3MPa and 9.2±0.2%. The achievement of high strength and good ductility indicates that the development of new titanium alloys is suitable for AM and thus could be the future direction for titanium alloys research.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Leyens · 2003
2. Matucha · 1996 · vol. 8
3. Technological aspects
4. Melting, casting and forging problems in titanium alloys10.1016/S0921-5093(97)00810-1 ↗
5. A review on high-strength titanium alloys: microstructure, strengthening, and properties10.1002/adem.201801359 ↗
6. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
7. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
8. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock
9. Davison · 2019
10. Grain refinement and improved tensile properties of Ti5Al2Sn2Zr4Mo4Cr titanium alloy fabricated by laser solid forming10.1016/j.msea.2020.140388 ↗
11. Microstructure and property of laser additive manufactured alloy Ti–6Al–2V–1.5Mo–0.5Zr–0.3Si after aged at different temperatures
12. Evolution of microstructure and intervariant boundaries of α phase in electron beam melted and heat-treated Ti–6Al–4V alloy10.1007/s12598-020-01612-0 ↗
13. Microstructure and micro-texture evolution of additively manufactured β-Ti alloys
14. Microstructures and grain refinement of additive-manufactured Ti-x W alloys
15. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
16. Synthesis of Ti-5Al, Ti-6Al-7Nb, and Ti-22Al-25Nb alloys from elemental powders using powder-bed fusion additive manufacturing10.1016/j.jallcom.2018.05.325 ↗
17. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
18. Fe nanoparticles modified pure Ti alloy on microstructure evolution and fine crystallization mechanism fabricated by additive manufacturing10.1016/j.jmrt.2023.08.221 ↗
19. The influence of iron in minimizing the microstructural anisotropy of Ti-6Al-4V produced by laser powder-bed fusion
20. Microstructural response of β-stabilized Ti–6Al–4V manufactured by direct energy deposition10.1016/j.jallcom.2019.152021 ↗
21. Influence of trace silicon addition on microstructure and properties of Ti6Al4V fabricated by wire arc additive manufacturing10.1016/j.jmrt.2023.01.065 ↗
22. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition10.1016/j.matdes.2019.108191 ↗
23. Trace carbon addition to refine microstructure and enhance properties of additive-manufactured Ti-6Al-4V
24. A high strength and low modulus metastable β Ti-12Mo-6Zr-2Fe alloy fabricated by laser powder bed fusion in-situ alloying
25. Additive manufacturing of titanium-base alloys with equiaxed microstructures using powder blends
26. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
27. Effects of β-stabilizer elements on microstructure formation and mechanical properties of titanium alloys10.1016/j.jallcom.2021.160085 ↗
28. General physical metallurgy of titanium reviewed
29. Progress on laser melting deposition processing and manufacturing of advanced aeronautical metallic structural materials and coatings
30. Progress and challenges of laser direct manufacturing of large titanium structural components10.3788/CJL20093612.3204 ↗
31. Laser-directed energy deposition: principles and applications10.1016/B978-0-12-818411-0.00003-3 ↗
32. Solidification behavior and grain morphology of laser additive manufacturing titanium alloys10.1016/j.jallcom.2018.11.055 ↗
33. Grain-refinement mechanisms in titanium alloys10.1557/JMR.2008.0002 ↗
34. The contribution of constitutional supercooling to nucleation and grain formation10.1007/s11661-015-2960-y ↗
35. Atomic structure of interphase boundary of an a precipitate plate in a β Ti-Cr alloy10.1080/09500839508242449 ↗
36. Structure and formation mechanism of α/α interface in laser melting deposited α+ β titanium alloy10.1016/j.jallcom.2015.09.236 ↗
37. The influences of anneal temperature and cooling rate on microstructure and tensile properties of laser deposited Ti–4Al–1.5 Mn titanium alloy10.1016/j.jallcom.2014.04.058 ↗
38. Texture evolution during sub-critical annealing and its effect on yield strength anisotropy of laser directed energy deposited Ti-6Al-2Zr-1Mo-1V alloy10.1016/j.msea.2022.143556 ↗
39. A review on additive manufacturing of titanium alloys for aerospace applications: directed energy deposition and beyond Ti-6Al-4V
40. Microstructure and anisotropic tensile behavior of laser additive manufactured TC21 titanium alloy10.1016/j.msea.2016.07.040 ↗
41. TC17 titanium alloy laser melting deposition repair process and properties10.1016/j.optlastec.2016.02.013 ↗
42. Microstructure evolution and mechanical properties of wire-feed electron beam additive manufactured Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy with different subtransus heat treatments10.1016/j.matdes.2020.109063 ↗
43. Additive manufacturing of high strength near β titanium alloy Ti-55511 by engineering nanoscale secondary α laths via in-situ heat treatment10.1016/j.msea.2021.141245 ↗
44. Anisotropic tensile properties and failure mechanism of laser metal deposited Ti-5Al-5Mo-5V-3Cr alloy before and after sub-transus heat-treatment10.1016/j.msea.2021.141928 ↗
45. The ageing response of direct laser deposited metastable β-Ti alloy, Ti–5Al–5Mo–5V–3Cr
46. Microstructure and mechanical properties of as-deposited and heat treated Ti-5Al-5Mo-5V-3Cr-1Zr (Ti-55531) alloy fabricated by laser melting deposition10.1016/j.jallcom.2019.151792 ↗
47. Effect of double annealing treatments on Ti-10V-2Fe-3Al alloy by directed energy deposition
48. Microstructure and mechanical properties of an ultrahigh-strength titanium alloy Ti-4.5 Al-5Mo-5V-6Cr-1Nb prepared using laser directed energy deposition and forging: a comparative study
49. Microstructure and mechanical properties of β-21S Ti alloy fabricated through laser powder bed fusion10.1007/s40964-021-00181-7 ↗