Effect of solution treatment on porosity, tensile properties and fatigue resistance of Al–Cu alloy fabricated by wire arc additive manufacturing
Source abstract
Abstract
This work studied the effect of solution heat treatment on the microstructure and properties of the Al–Cu alloy fabricated by wire arc additive manufacturing (WAAM), and focused on the influence of porosity and second phase evolution on the tensile properties and fatigue resistance of the alloy. The results show that with solution heat treatment at 530 °C for 1h, Al–Cu alloy fabricated by WAAM with low porosity (2.4 %) and high peak hardness (148.2 HV) can be obtained. Higher solution temperatures significantly increased the porosity, and extending the solution time caused the problems of increased porosity, micropore growth, microcracks as well as cavity. Influence of porosity on fatigue resistance is more significant than that on tensile properties. The results of tensile tests suggest that the effect of porosity on the strength of T6-treated alloy is limited and much smaller than that of the precipitation strengthening induced by precipitates, while the results of the fatigue crack propagation tests imply that porosity plays the dominant role in the fatigue crack propagation behaviors of the T6-treated alloy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
2. Dislocation network in additive manufactured steel breaks strength-ductility trade-off10.1016/j.mattod.2017.11.004 ↗
3. Optimization of heat treatment for an Al-Mg-Sc-Mn–Zr alloy with ultrafine grains manufactured by laser powder bed fusion10.1016/j.matchar.2022.111977 ↗
4. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
5. In-depth study of the mechanical properties for Fe3Al based iron aluminide fabricated using the wire-arc additive manufacturing process10.1016/j.msea.2016.05.047 ↗
6. Oxide accumulation effects on wire + arc layer-by-layer additive manufacture process10.1016/j.jmatprotec.2017.10.030 ↗
7. A review of wire arc additive manufacturing and advances in wire arc additive manufacturing of aluminium10.1080/02670836.2018.1455012 ↗
8. Arc-based additive manufacturing of steel components-comparison of wire- and powder-based variants10.1007/s40194-017-0527-9 ↗
9. Wire and arc additive manufacturing of aluminum components10.3390/met9050608 ↗
10. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
11. Microstructure, defects, and mechanical properties of wire + arc additively manufactured Al-Cu4.3-Mg1.5 alloy10.1016/j.matdes.2019.108357 ↗
12. Pore elimination mechanisms during 3D printing of metals10.1038/s41467-019-10973-9 ↗
13. Pore formation and evolution in wire plus arc additively manufactured 2319 Al alloy
14. Influence of surfacing modes on the formation of pore in the deposited metal produced by wire arc additive method (WAAM) using Al-Mg alloy10.4028/www.scientific.net/MSF.1037.20 ↗
15. A comparative study of additively manufactured thin wall and block structure with Al-6.3%Cu alloy using cold metal transfer process10.3390/app7030275 ↗
16. Influence of deposition strategy and heat treatment on mechanical properties and microstructure of 2319 aluminium WAAM components10.1016/j.matdes.2022.110974 ↗
17. Improving mechanical properties of wire arc additively manufactured AA2196 Al-Li alloy by controlling solidification defects
18. Relationship between precipitation behavior and loading orientations of the creep-aged Al-Cu-Li single crystal10.1016/j.jmrt.2023.03.015 ↗
19. Initial report on the oriented-precipitation of T1-phase in creep-aged Al-Cu-Li single crystal10.1007/s12540-022-01307-4 ↗
20. Fatigue responses of three AA 2000 series aluminum alloys
21. Stress aging of Al–Cu–Mg–Ag single crystal: the effect of the loading orientations10.1016/j.jallcom.2019.152635 ↗
22. Revisit the stress-orienting effect of θ' in Al-Cu single crystal during stress aging10.1016/j.matchar.2017.11.053 ↗
23. Wire-arc additive manufactured Al-Cu alloy: microstructure, mechanical properties and their anisotropy10.1080/02670836.2023.2194763 ↗
24. Effect of characteristic substrate parameters on the deposition geometry of CMT additive manufactured Al-6.3%Cu alloy
25. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy10.1016/j.msea.2015.10.101 ↗
26. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
27. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
28. On the role of Zr content into Portevin-Le Chatelier (PLC) effect of selective laser melted high strength Al-Cu-Mg-Mn alloy10.1016/j.matlet.2019.03.112 ↗
29. The Portevin-Le Chatelier (PLC) effect in an Al-Cu aluminum alloy fabricated by selective laser melting10.1016/j.matchar.2021.111198 ↗
30. Effects of notch position on the fatigue crack growth behavior of dissimilar laser welded DP980/QP980 joint10.1111/ffe.13653 ↗
31. Microstructure, mechanical properties and fatigue crack growth behavior of friction stir welded joint of 6061-T6 aluminum alloy10.1016/j.ijfatigue.2020.105556 ↗
32. Effect of hierarchical martensitic microstructure on fatigue crack growth behavior of ultra-high strength hot stamping steel10.1016/j.matchar.2021.111041 ↗
33. Effect of single tensile overload on fatigue crack growth behavior in DP780 dual phase steel10.1016/j.ijfatigue.2017.09.018 ↗
34. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
35. Microstructure, mechanical properties and fatigue crack growth behavior of an Al-Zn-Mg-Cu-Si-Zr-Er alloy fabricated by laser powder bed fusion10.1016/j.ijfatigue.2023.107636 ↗
36. Effect of ageing precipitation characteristics on fatigue fracture behavior of 2E12 aluminum alloy
37. Micro porosity and its effect on fatigue performance of 7050 aluminum thick plates10.1007/s11771-022-4961-5 ↗
38. Quantifying the influences of carbides and porosities on the fatigue crack evolution of a Ni-based single-crystal superalloy using X-ray tomography10.1007/s40195-021-01273-7 ↗