Effect of grain size on high-temperature corrosion performance of laser cladding inconel 625 coating
Source abstract
Abstract
As the calorific value of waste-to-energy incineration continues to rise, the corrosion damage to boilers becomes increasingly severe. The impact of the grain size on the high-temperature corrosion resistance of Inconel 625 coating was investigated. The results indicated that the corrosion performance of the coating in 1:1 NaCl–KCl salts at 700 °C for 120 h was highly dependent on the grain size of the coating. The coating fabricated with a laser power of 1800 W and an overlapping distance of 1.5 mm had an average grain size of 13.7 μm and highest hardness, exhibiting the best corrosion performance, with a corrosion weight loss of 1.4 mg/cm 2 . Coatings processed under different conditions all formed a three-layered structure, with a NiO outermost layer, a Cr 2 O 3 intermediate layer, and an innermost Cr-depletion zone. Coatings with finer grains formed a continuous and dense protective oxide layer of NiO and Cr 2 O 3 due to the rapid diffusion of alloy elements, effectively preventing the invasion of corrosive media and protecting the substrate from corrosion.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Nuclear Materials and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. An overview of characteristics of municipal solid waste fuel in China: physical, chemical composition and heating value10.1016/j.rser.2014.04.024 ↗
2. Preferential policies promote municipal solid waste (MSW) to energy in China: current status and prospects10.1016/j.rser.2014.04.049 ↗
3. Application of coatings to alleviate fireside corrosion on heat transfer tubes during the combustion of low-grade solid fuels: a review10.1021/acs.energyfuels.0c02145 ↗
4. Corrosion of heat exchanger materials in co-combustion thermal power plants10.1016/j.rser.2022.112328 ↗
5. The environmental comparison of landfilling vs. incineration of MSW accounting for waste diversion10.1016/j.wasman.2011.10.023 ↗
6. Status and perspectives of municipal solid waste incineration in China: a comparison with developed regions10.1016/j.wasman.2017.04.014 ↗
7. Mineralization behavior and strengthening technology of high calcium MSWI fly ash in sintering co-treatment process10.1016/j.jmrt.2022.07.118 ↗
8. Municipal solid waste (MSW) incineration fly ash as an important source of heavy metal pollution in China10.1016/j.envpol.2019.04.082 ↗
9. The evolution of waste-to-energy incineration: a review10.1016/j.rser.2018.04.088 ↗
10. A review of technologies and performances of thermal treatment systems for energy recovery from waste10.1016/j.wasman.2014.11.010 ↗
11. A literature review of the latest trends and perspectives regarding alkali-activated materials in terms of sustainable development10.1016/j.jmrt.2023.07.038 ↗
12. High-temperature corrosion behavior of superalloys in molten salts – a review10.1080/10408436.2016.1243090 ↗
13. Review on fate of chlorine during thermal processing of solid wastes10.1016/j.jes.2018.09.003 ↗
14. Corrosion problems in incinerators and biomass-fuel-fired boilers10.1155/2014/505306 ↗
15. High-temperature corrosion in waste-to-energy boilers10.1007/s11666-006-9005-4 ↗
16. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
17. Long-term hot corrosion behavior of boiler tube alloys in waste-to-energy plants10.1007/s11085-016-9627-y ↗
18. Thermally sprayed coatings resistant to erosion and corrosion for power plant boilers - a review10.1016/j.surfcoat.2014.10.046 ↗
19. Advances in corrosion-resistant thermal spray coatings for renewable energy power plants: Part II—effect of environment and outlook10.1007/s11666-019-00939-0 ↗
20. A comprehensive review of corrosion resistance of thermally-sprayed and thermally-diffused protective coatings on steel structures10.1007/s11666-019-00855-3 ↗
21. Application of high temperature corrosion-resistant materials and coatings under severe corrosive environment in waste-to-energy boilers10.1007/s11666-006-9012-5 ↗
22. Advances in corrosion-resistant thermal spray coatings for renewable energy power plants. Part I: effect of composition and microstructure10.1007/s11666-019-00938-1 ↗
23. Recent research and development status of laser cladding: a review10.1016/j.optlastec.2021.106915 ↗
24. High-temperature corrosion behavior of the FeCrAl laser cladding coatings in waste-to-energy superheaters: influence of Al content10.1016/j.surfcoat.2024.130650 ↗
25. Corrosion of Ni-based alloy coatings prepared by laser cladding in high-temperature chloride environment10.1016/j.surfcoat.2024.130823 ↗
26. Chlorine-induced high-temperature corrosion characteristics of Ni-Cr alloy cladding layer and Ni-Cr-Mo alloy cladding layer10.1016/j.corsci.2023.111102 ↗
27. Corrosion characteristics of Inconel 625 cladding layer and NiCrMoAl cladding layer in molten NaCl-KCl and NaCl-KCl-Na2SO410.1016/j.corsci.2023.111308 ↗
28. FEM-based thermogram correction for Inconel 625 joint hardness clustering10.3390/ma15031113 ↗
29. Temperature-based prediction of joint hardness in TIG welding of Inconel 600, 625 and 718 nickel superalloys10.3390/ma14020442 ↗
30. Reed · 2006
31. A comparison of the high-temperature oxidation behaviour of conventional wrought and laser beam melted Inconel 62510.1016/j.corsci.2019.108347 ↗
32. Microstructure characteristics of Inconel 625 superalloy manufactured by selective laser melting10.1016/j.jmst.2014.09.020 ↗
33. High-temperature oxidation behavior and mechanism of Inconel 625 super-alloy fabricated by selective laser melting10.1016/j.optlastec.2020.106509 ↗
34. Reduction of micro-cracking in nickel superalloys processed by Selective Laser Melting: a fundamental alloy design approach10.1016/j.actamat.2015.04.035 ↗
35. Grain size evolution under different cooling rate in laser additive manufacturing of superalloy10.1016/j.optlastec.2019.105662 ↗
36. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
37. The structure and properties of laser-cladded Inconel 625/TiC composite coatings10.3390/ma16031265 ↗
38. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
39. Grain boundary depletion and migration during selective oxidation of Cr in a Ni–5Cr binary alloy exposed to high-temperature hydrogenated water10.1016/j.scriptamat.2014.06.022 ↗
40. Corrosion behaviour of various model alloys with NaCl–KCl coating10.1016/j.matchemphys.2005.03.015 ↗
41. Hot corrosion behavior of Inconel 625 superalloy in eutectic molten nitrate salts10.1007/s11085-017-9830-5 ↗
42. Electrochemical study on the hot corrosion behavior of Ni16Cr13Co4Mo alloy in molten NaCl-KCl and NaCl-KCl-Na2SO410.1016/j.corsci.2022.110247 ↗
43. Electrochemical study on the corrosion behaviors of 316 SS in HITEC molten salt at different temperatures10.1016/j.solmat.2018.06.044 ↗
44. The fate of chlorine during MSW incineration: vaporization, transformation, deposition, corrosion and remedies10.1016/j.pecs.2019.100789 ↗
45. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
46. The corrosion behavior of Fe–10Cr nanocrystalline coating10.1016/j.electacta.2005.12.015 ↗
47. Nanocrystalline steel processed by severe rolling of lath martensite10.1016/j.msea.2006.06.047 ↗
48. Electrochemical corrosion behavior of nanocrystalline materials—a review10.1016/S1005-0302(10)60001-1 ↗