journal article·2025-05Open access

Effect of preweld conditions on the strain ageing cracking susceptibility of IN939 superalloys heat affected zone

Jilin Xie, Changhao Geng, Jiazhe Song, Yuhua Chen, Shanlin Wang, Peng He

Abstract

The evolutionary behavior of precipitated phases is a key determinant of strain aging cracking sensitivity in superalloys. In multi-component superalloys, these behaviors are influenced by pre-weld conditions and heat input. The strain aging cracking (SAC) sensitivity of the heat affected zone (HAZ) of IN-939 superalloy with various pre-weld heat treatment conditions was studied. The SAC sensitivity of the IN-939 superalloy samples was evaluated through the strain-to-fracture test (STF) by monitoring the ductility and fracture time during the test. The SAC sensitivity influencing factors including microstructure evolution, phase precipitation behavior of IN-939 superalloys were analyzed by electron probe micro analyzer (EPMA)、in-situ and exit-situ TEM test. The results showed that the SAC sensitivity of overaged IN-939 superalloys is smaller than that of the solid-solution condition showing larger ductility and longer fracture time during the STF test. The fast precipitation of γ′ phase in the IN-939 superalloy HAZ during the STF test is responsible for the large SAC sensitivity of the solid-solution condition. The SAC sensitivity temperature range is well consistent with the fast precipitation temperature of γ′ phase.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Advanced Ni-base superalloys for small gas turbines10.1179/1879139511Y.0000000010 ↗
2. Effects of pre- and post-weld heat treatment cycles on the liquation and strain-age cracking of IN939 superalloy
3. Effect of preweld heat treatment on the microstructure of HAZ (HAZ) and weldability of inconel 939 superalloy10.1007/s11665-013-0704-y ↗
4. Effects of heat treatment on mechanical properties of high-chromium nickel-base superalloy IN 93910.1179/mst.1986.2.10.1031 ↗
5. Solving recent challenges for wrought Ni-base superalloys10.1007/s11661-020-05773-6 ↗
6. IN939: metallurgy, properties and performance
7. Influence of interrupted ageing on the temporal evolution of the γ' size distribution and the co-precipitation of γ'' in alloy 718Plus10.1016/j.matchar.2023.113394 ↗
8. Evolutionary mechanisms in the plastic deformation of γ'-Ni3(Al, Ti)-strengthened additively manufactured nickel-based 939 superalloys at intermediate temperatures10.1016/j.matdes.2024.112795 ↗
9. Lippold · 2011
10. Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy10.1016/j.matchar.2011.09.006 ↗
11. The effect of heat treatment sequence on microstructure and mechanical properties of diffusion brazed IN-939 superalloy10.1016/j.jmatprotec.2018.11.020 ↗
12. The joint properties of a high-chromium Ni-based superalloy made by diffusion brazing: microstructural evolution, corrosion resistance and mechanical behavior10.1016/j.jmapro.2018.11.025 ↗
13. Microstructural investigation of IN 939 superalloy10.1016/0042-207X(92)90115-D ↗
14. Effect of pre- and post-weld heat treatment on microstructure and mechanical properties of GTD-111 superalloy welds10.1007/s12540-019-00465-2 ↗
15. Hughes, ([n.d.]).
16. Fawley, ([n.d.]).
17. Strain-Age cracking after postweld heat treatments in inconel 738 superalloy10.1515/HTMP.2010.29.1-2.61 ↗
18. Brody · 1966
19. Phase composition and phase stability of a high-chromium nickel-based superalloy, IN93910.1007/BF02645547 ↗
20. Age hardening of high temperature nickel base alloys
21. Effects of Cr content on the microstructure and stress rupture property of a directionally solidified Ni-based superalloy during long-term thermal exposure10.1016/j.msea.2018.02.005 ↗
22. Effect of casting temperature on microstructure and mechanical properties of K439B superalloy
23. Synergy of γ′ phase, MC carbide and grain boundary phase on creep behavior for nickel-based superalloy K439B
24. Dislocation climbing dominated decomposition and fracture of carbides in a Ni-based superalloy10.1016/j.actamat.2023.118669 ↗
25. Microstructure evolution and phase transformation in a nickel-based superalloy with varying Ti/Al ratios: Part 1 - microstructure evolution
26. Strain-age cracking in vacuum electron beam welded IN738LC alloy during post-weld heat treatment