Microstructures and properties of wire-arc additively manufactured ultra-high strength aluminum alloy under different heat treatments
Source abstract
Abstract
The microstructures, mechanical properties and corrosion behaviors of the ultra-high strength Al–Zn–Mg–Cu-Sc aluminum alloy fabricated by wire-arc additive manufacturing process using a self-prepared 7B55-Sc filler wire were systematically investigated under different heat treatments. The results showed that the microstructures of the as-deposited, T6, T73, and retrogression and re-aging (RRA) heat treatments were all composed of fine equiaxed grains with a size of about 6.0 μm. The grain boundary precipitates (GBPs) of the as-deposited sample were very coarse and continuously distributed along the grain boundaries, and the intragranular precipitates (IGPs) mainly consisted of a small amount of ηMg(Zn,Cu,Al)2 and η′ phases. After T6 heat treatment, the GBPs became much finer, but still continuously distributed along the grain boundaries. The IGPs mainly consisted of fine GP zones and η′ phases. After RRA heat treatment, the GBPs became coarser and discontinuously distributed along the grain boundaries. The IGPs were composed of η′ phases and ηMg(Zn,Cu,Al)2 phases. After T73 heat treatment, the GBPs became much coarser and sparsely distributed along the grain boundaries. The IGPs mainly consisted of coarser ηMg(Zn,Cu,Al)2 phases. The T6 heat-treated sample achieved the highest tensile strength of 618 MPa. While the strength of T73 heat-treated sample was sacrificed by up to 17% compared with the T6 heat-treated sample, but the corrosion resistance was the best of all heat-treated conditions. After RRA heat treatment, the strength was about 10% lower than the strength of the T6 condition, but the corrosion resistance was better than that of the T6 heat-treated sample.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
2. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
3. Effect of heat treatment on microstructure, hardness and corrosion resistance of 7075 Al alloys fabricated by SLM10.1016/j.jmapro.2020.10.071 ↗
4. Wire-arc additive manufacturing of a novel high-performance Al-Zn-Mg-Cu alloy: processing, characterization and feasibility demonstration
5. Wire-arc additive manufacturing of Al-Zn5.5-Mg-Cu (ML7075): shifting paradigms of additive manufacture-ability10.1016/j.matlet.2022.131841 ↗
6. Formation mechanism of Al-Zn-Mg-Cu alloy fabricated by laser-arc hybrid additive manufacturing: microstructure evaluation and mechanical properties, Addit
7. Achieving high strength-ductility of Al-Zn-Mg-Cu alloys via hot-wire arc additive manufacturing enabled by strengthening precipitates
8. Microstructure and mechanical properties of ultra-high strength Al-Zn-Mg-Cu-Sc aluminum alloy fabricated by wire + arc additive manufacturing10.1016/j.jmapro.2022.05.009 ↗
9. The effect of pre-ageing/ stretching on the ageing-hardening behavior of Al–Zn–Mg–Cu alloys correlated with Zn/Mg ratio10.1016/j.msea.2021.142331 ↗
10. Recent advances in ageing of 7xxxx series aluminum alloys: a physical metallurgy perspective10.1016/j.jallcom.2018.11.286 ↗
11. Precipitation hardening and intergranular corrosion behavior of novel Al-Mg-Zn(-Cu) alloys10.1016/j.jallcom.2020.157199 ↗
12. Ageing behavior and stress corrosion cracking resistance of a non-isothermally aged Al-Zn-Mg-Cu alloy10.1016/j.msea.2014.03.023 ↗
13. Investigation of mechanical and corrosion properties of an Al-Zn-Mg-Cu alloy under various ageing conditions and interface analysis of η' precipitate10.1016/j.matdes.2015.06.183 ↗
14. Effect of heat treatment on strength, exfoliation corrosion and electrochemical behavior of 7085 aluminum alloy10.1016/j.matdes.2011.09.033 ↗
15. Mechanical properties, corrosion behaviors and microstructures of 7075 aluminum alloy with various aging treatments10.1016/S1003-6326(08)60130-2 ↗
16. A Model for the electrical conductivity of peak-aged and overaged Al-Zn-Mg-Cu alloys10.1007/s11661-003-0221-y ↗
17. Enhanced stress corrosion cracking resistance and electrical conductivity of a T761 treated Al-Zn-Mg-Cu alloy thin plate
18. Correlation of stress corrosion cracking behaviour with electrical conductivity and open circuit potential in Al-Li-Cu-Mg-Zr alloys10.1002/maco.200603987 ↗
19. The effect of multistage ageing on microstructure and mechanical properties of 7050 alloy10.1016/j.jallcom.2016.01.266 ↗
20. Effects of severe cold rolling on tensile properties and stress corrosion cracking of 7050 aluminum alloy10.1016/j.matchemphys.2009.05.048 ↗
21. Development of microstructures and texture during cold rolling in AA 7055 aluminum alloy10.1016/j.msea.2008.10.055 ↗
22. Effect of minor Sc and Zr addition on microstructure and properties of ultra-high strength aluminum alloy10.1016/S1003-6326(14)63544-5 ↗
23. Structure and properties of an ultra-high strength 7xxxx aluminum alloy contained Sc and Zr10.1016/S1005-8850(08)60052-3 ↗
24. The physical meanings of 5 basic parameters for an X-ray diffraction peak and their application, China10.1007/BF02831544 ↗
25. Microstructure and mechanical properties of 600 MPa grade ultra-high strength aluminum alloy fabricated by wire-arc additive manufacturing10.1016/j.jmst.2022.12.007 ↗
26. Improved solution treatment for an as-rolled Al–Zn–Mg–Cu alloy. Part I. Characterization of constituent particles and overheating10.1016/j.msea.2011.11.065 ↗
27. Effect of aging treatment on microstructure, mechanical and corrosion properties of 7055 aluminum alloy prepared using powder by-product10.1016/j.msea.2021.141606 ↗
28. Multiscale analysis of grain boundary microstructure in high strength 7xxxx Al alloys10.1016/j.actamat.2020.10.021 ↗
29. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
30. Effects of multi-stage aging treatments on the precipitation behavior and properties of 7136 aluminum alloy10.1016/j.jallcom.2019.152256 ↗
31. Size effect in the Al3Sc dispersoid-mediated precipitation and mechanical/electrical properties of Al-Mg-Si-Sc alloys10.1016/j.jmst.2020.03.056 ↗
32. Precipitation of Al3(Sc,Zr) particles in an Al-Zn-Mg-Cu-Sc-Zr alloy during conventional solution heat treatment and its effect on tensile properties10.1016/j.actamat.2008.04.005 ↗
33. Mechanical properties and microstructure of aluminum alloy 2618 with Al3(Sc, Zr) phases10.1016/j.msea.2003.09.092 ↗
34. Corrosion behavior and mechanical properties of Al-Zn-Mg aluminum alloy weld10.1016/j.corsci.2017.05.007 ↗
35. The characterization and corrosion resistance of cerium chemical conversion coatings for 304 stainless steel10.1016/S0010-938X(03)00135-5 ↗
36. Effects of solution heat treatment on corrosion resistance of 5083F Al alloy10.1016/S1003-6326(08)60371-4 ↗
37. Hall–Petch relation and boundary strengthening, Scripta
38. Microstructure analysis of 7050 aluminum alloy processed by multistage aging treatments10.1016/j.jallcom.2022.164400 ↗
39. Heat treatment of 7xxxx series aluminum alloys—some recent developments10.1016/S1003-6326(14)63306-9 ↗
40. Effect of grain boundary characteristic on intergranular corrosion and mechanical properties of severely sheared Al-Zn-Mg-Cu alloy10.1016/j.msea.2018.06.097 ↗
41. Influence of heat treatment on the strength and fracture toughness of 7N01 aluminum alloy10.1016/j.jallcom.2016.03.228 ↗
42. The effect of pre-ageing temperature and retrogression heating rate on the strength and corrosion behavior of AA715010.1016/j.corsci.2011.08.042 ↗
43. A TEM study of microstructural changes during retrogression and reaging in 7075 aluminum10.1007/BF02645554 ↗
44. Recent advances in ageing of 7xxxx series aluminum alloys: a physical metallurgy perspective10.1016/j.jallcom.2018.11.286 ↗
45. Precipitation formation on ∑5 and ∑7 grain boundaries in 316L stainless steel and their roles on intergranular corrosion10.1016/j.actamat.2021.116822 ↗
46. Effect of grain boundary precipitation on corrosion of heating-aging treated Al-4.47Zn-2.13Mg-1.20Cu alloy10.1016/j.jmrt.2020.03.106 ↗
47. Environmental factors affecting localized corrosion of 7075-T7351 aluminum alloy plate10.1007/BF02642428 ↗
48. Stress corrosion cracking behaviour of 7xxxx aluminum alloys: a literature review10.1016/S1003-6326(16)64220-6 ↗
49. Effects of retrogression and re-aging treatment on precipitation behavior, mechanical and corrosion properties of a Zr + Er modified Al-Zn-Mg-Cu alloy10.1016/j.matchar.2021.111617 ↗
50. Effect of recrystallization on plasticity, fracture toughness and stress corrosion cracking of a high-alloying Al-Zn-Mg-Cu alloy10.1016/j.matlet.2020.128074 ↗
51. Effect of Zr, Er and Cr additions on microstructures and properties of Al–Zn–Mg–Cu alloys10.1016/j.msea.2014.05.021 ↗
52. Stress corrosion cracking and hydrogen embrittlement of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2004.06.023 ↗
53. Study of the potential electrochemical noise during corrosion process of aluminum alloys 2024, 7075 and pure aluminum10.1002/maco.200390132 ↗
54. Retrogression and re-aging treatment on short transverse tensile properties of 7010 aluminum alloy extrusions